GH4169 and GH3536 (Hastelloy X) are both high-performance nickel-based superalloys commonly used in the aerospace field, but they have different applications: GH4169 is a precipitation-hardening alloy with excellent strength below 650°C (e.g., turbine disks), while GH3536 is a solid solution alloy with better oxidation resistance and ductility at higher temperatures (>800°C) (e.g., combustion chambers).

02.

What is GH4169 equivalent to?

Inconel 718

GH4169 (equivalent to the American brand Inconel 718) is a precipitation-hardening nickel-based superalloy widely used in the aerospace industry due to its excellent mechanical properties (Lu et al., 2014).

GH4169 Equivalent

1. Comparison of chemical composition of GH4169 and GH3536 (wt%)

Element GH4169 (Inconel 718) GH3536 (Hastelloy X) Key Difference
Nickel (Ni) 50.0 – 55.0 Balance (~≥65) GH3536 has higher Ni
Chromium (Cr) 17.0 – 21.0 20.5 – 23.0 GH3536 higher Cr
Iron (Fe) Balance (~18-20) 17.0 – 20.0 GH4169 slightly higher Fe
Molybdenum (Mo) 2.80 – 3.30 8.0 – 10.0 GH3536 has ~3x more Mo
Cobalt (Co) ≤ 1.00 0.5 – 2.5 GH3536 contains Co
Tungsten (W) – 0.2 – 1.0 GH3536 contains W
Niobium (Nb) 4.75 – 5.50 – GH4169 unique – γ″ former
Titanium (Ti) 0.65 – 1.15 – GH4169 unique
Aluminum (Al) 0.20 – 0.80 – GH4169 unique
Carbon (C) ≤ 0.08 0.05 – 0.15 GH3536 higher C
Manganese (Mn) ≤ 0.35 ≤ 1.00 GH3536 higher
Silicon (Si) ≤ 0.35 ≤ 1.00 GH3536 higher
Phosphorus (P) ≤ 0.015 ≤ 0.040 –
Sulfur (S) ≤ 0.015 ≤ 0.030 –
Boron (B) 0.002 – 0.006 ≤ 0.010 –

 

2. Comparison of mechanical and environmental properties of GH4169 and GH3536

Feature GH4169 (Alloy 718) GH3536 (Hastelloy X) Industrial Verdict
Strengthening Method Precipitation Hardening (γ′′) Solid Solution (Mo, W) GH4169 carries more weight.
Max Service Temp (Load) 700°C (1292°F) 850°C - 950°C GH4169 for Structural Load.
Oxidation Limit (Static) 980°C 1200°C (2200°F) GH3536 wins in the Fire.
Thermal Fatigue Life Moderate Elite (Resists Cracking) GH3536 for thermal cycling.
Fabricability Challenging (Hardens fast) Superior (Excellent Weld) GH3536 reduces labor costs.
Nickel Content (Ni) ~ 53% ~ 47% GH4169 has higher Nb content.

Click to download the GH4169 alloy PDF file now

Performance Applications of GH4169 and GH3536
GH3536 Alloy
03

GH3536 Alloy

GH3536 is the industry standard for components exposed to fluctuating open flame environments.

Superior Cyclic Oxidation Performance: Its high chromium and iron content forms a tightly adhering protective layer that does not peel off even during rapid cooling cycles.

Superior Machining Performance: GH3536 is renowned for its excellent weldability, enabling crack-free assembly of complex thin-walled combustion chamber and afterburner linings.

Cost-Effective Solution: For static fire zone components, GH3536 offers the best material lifecycle cost-effectiveness.

04

GH4169 Alloy

GH4169 is the "King of Tensile Loads," suitable for applications where components must maintain their shape under extreme pressure.

Superior Yield Strength: Maintains a yield strength of ≥ 1030 MPa at room temperature. It is the material of choice for rotating rings and turbine shafts.

High Cycle Fatigue (HCF): Specifically designed to resist failure caused by high-frequency mechanical vibrations in the "cooler" parts of the engine (below 700°C).

GH4169 Alloy
 
 

5. Common Applications of GH4169 and GH3536

GH4169 (Inconel 718): Turbine discs, fasteners, and high-strength hot-end components operating below 650°C.

GH3536 (Hastelloy X): Combustion chamber housings, transition components, and exhaust components.

Turbine disc
Turbine disc
Fasteners
Fasteners

Combustion chamber housing

Combustion chamber housing
Exhaust components
Exhaust components

 

Why Choose Gnee as Your Nickel-Based Alloy Supplier

✅️VIM + VAR Melting: Mandatory double-vacuum melting for GH4169 ensures zero internal inclusions, maximizing its fatigue resistance.

✅️Precision Flatness: Our aerospace sheets undergo advanced leveling, essential for automated laser cutting of cooling holes.

✅️MTC 3.1 Traceability: Full EN 10204 3.1 Mill Test Certificates detailing elevated temperature tensile and creep data.

✅️Wholesale Inventory: We maintain a massive stock of both grades in Seamless Pipe, Round Bar, and Sheet forms ready for Fast Global Shipping.

Gnee Alloy GH4169(inconel 718) Certificate

Gnee Alloy GH4169(inconel 718) Certificate

 

📦 Packaging and Shipping

All Nickel Based Alloy products are packaged using the following methods:

Wooden pallets or crates

Moisture-proof packaging

Labels with furnace number, standard, and size labels

Shipped worldwide by sea, air, or express

 Gnee Steel GH3030 Product Packing

 Gnee Alloy GH4169 Product Packing

Contact us for the latest export price quote for GH4169 Alloy

 

FAQ

Q1: Can I weld GH4169 and GH3536 together in a transition liner?
A: Yes. They have excellent metallurgical compatibility. We recommend using ERNiCr-3 or specialized filler metals to ensure the joint remains stable across the different thermal expansion zones.

 

Q2: Why is GH3536 better for combustion liners than 310S?
A: While 310S is a basic heat-resistant steel, GH3536 is a nickel-based superalloy with Molybdenum. It offers much higher creep strength and far better resistance to thermal fatigue cracking than 310S.

 

Q3: Which alloy is more expensive?
A: Generally, GH4169 is more expensive per kg due to its high Niobium (Nb) content and the complex multi-stage aging heat treatments (16+ hours) required to reach its performance specs.

 

Q4: Do you offer cut-to-size services for turbine discs and liners?
A: Absolutely. We offer Custom Fabrication, including precision laser and waterjet cutting, to deliver blanks ready for your stamping or forming line.