GH4169 Alloy High Temperature Performance Guide

For designers of aero-engine discs, high-pressure fasteners, and nuclear reactor springs, the biggest challenge lies in the gap in material validation. When components are subjected to high-frequency vibrations and temperatures exceeding 650°C, relying on nominal data can lead to:

 

Unexpected fatigue failure: Non-metallic inclusions in low-mass alloys induce microcracks.

Thermal creep sagging: Dimensional tolerances of components gradually decrease over time.

Stress relaxation: Fastener clamping forces decrease, leading to the failure of the entire assembly.

 

Our high-performance GH4169 material is designed to address these risks, providing the industrial-grade durability and data stability required for mission-critical simulations.

Click to get a GH4169 product quote

 
GH4169 Alloy High Temperature Performance Guide
 
GH4169 Alloy High Temperature Performance Guide

GH4169 Alloy High Temperature Performance Guide

GH4169 (equivalent to UNS N07718) is a precipitation-hardening nickel-based superalloy designed to provide superior performance in high-temperature environments (typically operating at temperatures up to 650°C). Due to its excellent strength, fatigue resistance, and structural stability, it is widely used in aerospace applications, such as gas turbine disks and rocket engines.

What is GH4169 equivalent to?

 

Inconel 718

GH4169 (equivalent to the American brand Inconel 718) is a precipitation-hardening nickel-based superalloy widely used in the aerospace industry due to its excellent mechanical properties (Lu et al., 2014).

GH4169 Equivalent

1. Chemical composition of GH4169 alloy (wt%)

Element Content (%) Function
Nickel (Ni) 50.0 – 55.0 Matrix element; high-temperature stability
Chromium (Cr) 17.0 – 21.0 Oxidation and corrosion resistance
Iron (Fe) Balance (~18-20) Fe-Ni-Cr base alloy
Niobium (Nb) 4.75 – 5.50 Core strengthening element – forms γ″ phase (Ni₃Nb)
Molybdenum (Mo) 2.80 – 3.30 Solid-solution strengthening; creep resistance
Titanium (Ti) 0.65 – 1.15 Forms γ′ strengthening phase (Ni₃(Al,Ti))
Aluminum (Al) 0.20 – 0.80 Forms γ′ strengthening phase; improves oxidation resistance
Carbon (C) ≤ 0.08 Low carbon for toughness
Manganese (Mn) ≤ 0.35 Deoxidizer
Silicon (Si) ≤ 0.35 Deoxidizer
Phosphorus (P) ≤ 0.015 Ensures toughness
Sulfur (S) ≤ 0.015 Ensures hot workability
Boron (B) 0.002 – 0.006 Grain boundary strengthener
Cobalt (Co) ≤ 1.00 Residual element
Copper (Cu) ≤ 0.30 Residual element

 

2. Typical mechanical data for GH4169

Temperature (℃/°F) Yield Strength (0.2% MPa) Tensile Strength (MPa) Elongation (δ5 %) Industrial Significance
20°C (Room Temp) ≥ 1030 MPa ≥ 1240 MPa ≥ 12% Precision Machining & Fit
540°C (1000°F) ≥ 950 MPa ≥ 1150 MPa ≥ 13% High-Pressure Stability
650°C (1200°F) ≥ 850 MPa ≥ 1000 MPa ≥ 15% Elite Structural Load
700°C (1292°F) ≥ 750 MPa ≥ 880 MPa ≥ 18% Thermal Burst Capacity

Click to download the GH4169 alloy PDF file now

 

3. Table of Stress Fracture and Creep Resistance Properties of GH4169 Alloy

Applied Stress (MPa) Test Temp (℃) Rupture Life (h) Elongation at Rupture
690 MPa 650°C ≥ 100 Hours ≥ 12%
450 MPa 700°C ≥ 100 Hours ≥ 15%
200 MPa 760°C ≥ 25 Hours ≥ 20%

 

4. Key High-Temperature Properties of GH4169

Operating Temperature Range: This alloy maintains excellent yield strength and can withstand significant stresses at temperatures up to 650°C.

Tensile Strength and Yield Strength: At 650°C, this alloy retains high strength and is one of the alloys with the best deformation resistance below this temperature.

Creep and Stress Fracture: GH4169 exhibits excellent fatigue resistance and low-cycle fatigue life, but prolonged exposure (e.g., 1000 hours) to 650°C leads to a significant decrease in stress fracture life.

Oxidation and Corrosion Resistance: This alloy exhibits good oxidation resistance at temperatures up to 650°C, but if the temperature rises to 850°C, the oxide film may become porous and easily peel off.

 

5. GH4169 - UNS N07718 High Temperature Alloy Applications

GH4169 - UNS N07718 High Temperature Alloy Applications

1. Aerospace Industry

Turbine Blades and Guide Vanes: The alloy maintains its strength and resists creep at high temperatures, making it an ideal material for jet engine turbine blades and guide vanes.

Rocket Engines and Engine Components: Its high strength and resistance to thermal and mechanical fatigue make it suitable for critical components of rocket engines.

High-Temperature Fasteners: Due to its excellent mechanical properties and oxidation resistance, it is used in aircraft manufacturing.

 

2. Power Generation Industry

Gas Turbine Components: GH4169 alloy, due to its high-temperature resistance, oxidation resistance, and corrosion resistance, is used in various components of gas turbines, including discs, shafts, and housings.

Nuclear Reactors: Its resistance to radiation damage and high-temperature performance makes it suitable for nuclear reactors, especially for control rods and other components exposed to high temperatures and radiation.

 

3. Oil and Gas Industry

Downhole Tools: Due to its resistance to sulfide stress cracking and corrosion in harsh environments, it is used in oil and gas exploration and production equipment, such as downhole tools.

Underwater Equipment: GH4169's corrosion resistance and high strength make it an ideal material for underwater valves, connectors, and fasteners.

 

4. Marine Applications

Propulsion Systems: Used in marine propulsion systems requiring extremely high corrosion resistance and mechanical strength.

Submarine Components: Its excellent seawater corrosion resistance and high strength make it an ideal material for critical submarine components.

 

Why Choose Gnee as Your Nickel-Based Alloy Supplier

✅️Wholesale Pricing: Benefit from Direct Factory Pricing on bulk tonnage and long-term MRO contracts.

✅️Industrial Durability: Our materials are optimized for the long-haul, reducing the Total Cost of Ownership (TCO) for your equipment.

✅️Certified Quality: Fully compliant with AMS 5662, AMS 5596, and ASTM B637 standards.

✅️Fast Global Shipping: Optimized logistics for rapid delivery to aerospace and energy hubs worldwide.

gh4169-uns-n07718-high-temperature-alloy

Gnee Alloy GH4169(inconel 718) Certificate

 

📦 Packaging and Shipping

All Nickel Based Alloy products are packaged using the following methods:

Wooden pallets or crates

Moisture-proof packaging

Labels with furnace number, standard, and size labels

Shipped worldwide by sea, air, or express

 Gnee Steel GH3030 Product Packing

 Gnee Alloy GH4169 Product Packing

Contact us for the latest export price quote for GH4169 Alloy

 

FAQ

 

Q1: How do you predict the fatigue life of GH4169 under cyclic pressure?
A: Fatigue life is highly dependent on the grain size and surface integrity. We provide Precision Ground (h8-h11) rods that eliminate surface stress initiators, ensuring your part reaches its maximum theoretical cycle limit.

 

Q2: Is GH4169 interchangeable with Inconel 718 in high-vibration engine zones?
A: Yes. GH4169 is the technical equivalent designation. Provided it is produced via VIM+VAR, it offers the exact same fatigue and stress-rupture profile required by international aviation blueprints.

 

Q3: Does the aging process affect the creep resistance?
A: Absolutely. Creep strength is maximized through the Double-Aging cycle (718°C + 621°C). We can supply the material in the Fully Aged state to save you the risk and cost of in-house heat treatment.

 

Q4: Do you offer trial samples for laboratory fatigue testing?
A: Yes. We support innovation by offering Flexible MOQs for certified specimens and test coupons.

Send Inquiry