Mar 08, 2024 Leave a message

Differences between CRGO and CRNGO silicon steel

Silicon steel, also named electrical steel, is soft magnetic alloy with extremely low content of carbon. The participation of silicon not only increases the resistivity and maximum permeability of iron, but also reduces iron loss, coercivity and aging of magnetism. That's why silicon steel is generally applied into electric machine and transformer core manufacturing. With multiple advantages, electrical steel plays a fundamental role in Electricity, Electronics and Military industries.

 

The differences between grain oriented and non grain oriented silicon steel

(1) As for grain oriented silicon steel, the grains basically face one direction, so the silicon content is higher. Grain oriented silicon steel is mainly used in manufacturing transformers.

As for non-oriented silicon steel, the distribution of grains is disordered, therefore the silicon content is lower. So non grain oriented silicon steel is mainly used in motor manufacturing.

(2) Bounded by 3% of silicon content, cold-rolled silicon steel is divided into cold-rolled non grain oriented (CRNGO) silicon steel and cold-rolled grain oriented (CRGO) silicon steel.

Cold-rolled non grain oriented silicon steel has relatively low production process requirements, and the mass fraction of silicon is between 0.5% and 3.0%. The thickness of finished product after cold rolling is generally 0.35mm or 0.5mm. Its Bs is higher than that of grain-oriented silicon steel. with uniform thickness, high dimensional accuracy, smooth and flat surface, which improves the filling factor and the magnetic properties of the material.

The silicon mass fraction of cold rolled oriented silicon steel is above 3.0%, and the carbon mass fraction is 0.03%-0.05%. There's a low amount of oxide of steel and inhibitors are required. Compared with cold-rolled non-oriented silicon steel, grain-oriented silicon steel has stronger magnetic directionality, and higher magnetic permeability and lower iron loss. Cold rolled grain oriented silicon steel, also known as cold-rolled transformer electrical steel, is commonly used in transformer manufacturing.

(3) Cold-rolled grain-oriented silicon steel can also be divided into two types: common grain-oriented silicon steel (CGO) and high magnetic induction grain-oriented silicon steel (Hi-B). High magnetic induction cold-rolled grain-oriented silicon steel is single-oriented steel strip, which is mainly used to manufacture various electromagnetic components such as choke coils, transformers in electronic instruments, etc.

Cold Rolled Grain Oriented (CRGO) Silicon Steel

GO Electrical Steel

Silicon steel application

(1) Cold-rolled non grain oriented silicon steel

① Large electromechanical: water industry, fire industry, nuclear power units or wind turbine units...

 

② Home appliance:High efficiency frequency conversion air conditioning or refrigerator compressor...

 

③ Small and medium-sized electromechanical: Y1, Y2, Y3 series and derivative series products. High efficiency, super efficiency series...

 

④ New energy vehicles: drive motor; New energy vehicle micromotor...

 

(2) Cold-rolled grain oriented silicon steel

① Transformer: High-end transformer [for 750kV/ 1000kV]

② Medium and low end transformer [for 220-500kV,110-200kV]

③ Energy-saving transformer: 0.18-0.30mm thickness