Detailed explanation of Inconel 601 round bars

Detailed explanation of Inconel 601 round bars
Inconel 601 round bar is a nickel-chromium-iron alloy known for its excellent resistance to high-temperature oxidation and corrosion. This material is widely used as a general-purpose engineering material for various demanding environments, particularly in applications where heat resistance is crucial.
What are the differences between Inconel 625 and 601?
Inconel 601 has a melting point of 2467°F (1350°C), while Inconel 625 has a melting point of 2375°F (1310°C). In terms of tensile strength at room temperature, Inconel 601 ranges from 590-930 MPa, while 625 has a slightly higher strength of 690-895 MPa.

What are the differences between Inconel 600 and Inconel 601 round bars?
Inconel 600 and 601 round bars share many similarities; both offer strong corrosion and oxidation resistance. They are also used in a variety of applications, from nuclear reactors to petrochemical plants. However, the two alloys differ in their chromium content; Inconel 600 has a chromium content between 16-25%, while Inconel 601 has almost double that amount, up to 50%. This makes Inconel 601 more corrosion and heat resistant than its counterpart, making it the preferred material for demanding end uses. For example, Inconel 601 can withstand temperatures up to 2200°F, while Inconel 600 can only withstand temperatures up to 1600°F. Therefore, Inconel 600 is typically used in household applications, while Inconel 601 is better suited for industrial applications.
What is special about Inconel 601 round bars?
Inconel 601 round bars are known for their exceptional strength and corrosion resistance at high temperatures. With its excellent strength and chemical resistance, 601 Inconel round bars are an ideal choice for demanding environments requiring high-temperature service. Due to its resistance to oxidation and carburization at temperatures up to 2200°F (1000°C), it is used in aerospace applications. Furthermore, it exhibits good oxidation resistance when exposed to corrosive gases such as chlorine or sulfur dioxide and can be used in a variety of hydrocarbon applications. Compared to similar products, Inconel 601 round bars also possess superior mechanical properties, making them ideal for many industrial operations requiring complex physical and chemical requirements.
Inconel 601 Round Bar Specifications
| Standards | ASTM B166 / ASTM SB166 |
| Size | 3.17 MM TO 350 MM DIA & AS PER CUSTOMER'S REQUIREMENT |
| Dimeter | 25mm to 152mm & AS PER CUSTOMER'S REQUIREMENT. |
| Length | 2000mm, 2440mm, 3000mm, 5800mm, 6000mm & AS PER CUSTOMER'S REQUIREMENT. |
| Condition | Cold Drawn, Polished Cold Drawn Centreless Ground & Polished, Annealed round bar & AS PER CUSTOMER'S REQUIREMENT. |
| Finish | Bright, Polish, Bright, Rough Turned, Grinding, Centreless Ground & Black. |
| Tolerence | h8, h9(DIN 671), h10, h11, ASTM A484, DIN 1013. |
| Form | Round, Rod, Precision Ground Bar, Square, Round Rod, Hollow, Hex (A/F), Triangle, Rectangle, Threaded, T-Bar, Half Round Bar, Flat Bar, Rings, Blocks, Billet, Ingot, I/H Bar, Angle Bar, Channel Bar, Profiles, Forging Etc. |
Inconel Bar 601 Price List
| Alloy 601 Round Bar Price Per Kg | FOB Price:US $4702-5601 / Ton |
| Inconel Alloy 601 Hex Bar Price | FOB Price:US $6010-2502 / Ton |
| Inconel Alloy 601 Flat Bar Price | FOB Price:US $2902-3402 / Ton |
| 601 Inconel Round Bar Price | FOB Price:US $6602-7102 / Ton |
| Inconel Rod 601 Price | FOB Price:US $3702-4601 / Piece |
| Inconel Alloy 601 Round Bar Price | FOB Price:US $6602-7102 / Ton |
| Alloy 601 Rods Price | FOB Price:US $1360.00-$2696.00 / Ton |
| Inconel Alloy 601 Round Bar Price | FOB Price:US $650.00-$1650.00 / Ton |
| Inconel Rod 601 Price Per Kg | FOB Price:US $3000.00-$5000.00 / Ton |
| Nickel Alloy Rod 601 Price Per Kg | FOB Price:US $1100.00-$2684.00 / Ton |
| 601 Alloy Square Bar Price | FOB Price:US $5422-5922 / Ton |
Inconel 601 Round Bar Equivalent Standards
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
|---|---|---|---|---|---|---|---|
| Inconel 601 | 2.4851 | N06601 | NCF 601 | NA 49 | XH60BT | NC23FeA | NiCr23Fe |
Inconel 601 Round Bar Chemical Composition
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr |
|---|---|---|---|---|---|---|---|---|
| Inconel 601 | 0.10 max | 1.00 max | 0.50 max | 0.015 max | 1.00 max | Balance | 58.0 – 63.0 | 21.0 – 25.0 |
601 Inconel Round Bar Stock Available
| » Inconel 601 Bar Stockist | » 601 Inconel Flat Bar Supplier |
| » Alloy 601 Round Bar Weight Calculator | » 2.4851 Inconel Bar |
| » Inconel 601 Round Rod | » Inconel Alloy 601 Bar Manufacturers |
| » 601 Inconel Bright Bar | » 601 Inconel Alloy Forged Bar |
| » Inconel Alloy 601 Hex Bar | » Inconel 601 Square Bar |
| » Nickel Alloy 601 Round Bar HSN Code | » 601 Inconel Flat Bar |
| » Inconel Alloy 601 Cold Rolled Bar | » Inconel Alloy 601 Hex Bar |
| » Alloy 601 Rectangular Bar | » Inconel 601 Hexagon Bar |
| » UNS N06601 Round Bar | » 601 Inconel Round Bars |
| » 601 Inconel Black Bar | » 601 Inconel Alloy Hollow Bar |
| » ASME SB166 601 Inconel Bar | » 8mm Square Inconel 601 Bar |
| » 601 Alloy Round Bar | » Alloy 601 Round Bar Supplier |
| » Inconel Alloy 601 Flat Bar | » Inconel 601 Polished Bars |
| » Inconel 601 Rod | » ASTM B166 Inconel Alloy 601 Bars |
| » 601 Inconel Bar | » Inconel Alloy 601 Round Bar Suppliers |
Why Choose Gnee as Your Nickel-Based Alloy Supplier
✅ Over 18 years of export experience, products sold to more than 80 countries
✅ Certified by ISO, SGS, and BV
✅ Global inventory of Inconel, Hastelloy, Incoloy, and Monel alloy tubing, plates, and bars
✅ Custom processing services available – including cutting, polishing, CNC machining, and packaging
✅ Fast delivery within 7-15 days, supported by global logistics partners
📦 Packaging and Shipping
All stainless steel products are packaged using the following methods:
Wooden pallets or crates
Moisture-proof packaging
Labels with furnace number, standard, and size labels
Shipped worldwide by sea, air, or express

About Gnee Steel
Gnee Steel is a professional manufacturer of nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy 800, Incoloy 800H/HT, Incoloy 825, Monel 400, Monel K500, and other high-temperature alloy materials. We specialize in the production and sales of alloy materials. Gnee Steel's products are widely used in aerospace, chemical, power generation, automotive, nuclear energy, and other fields, and we can provide customized alloy material solutions according to customer needs. For inquiries about alloy material prices or customized alloy material solutions, please feel free to contact us via email at ss@gneemetal.com for a quote.
Square Meters Built
Enterprise Employees
Years Experience
Partner countries