Mar 11, 2024 Leave a message

CRNGO&CRGO

Cold-rolled-non-grain-oriented steel (CRNGO)

There is no particular pressing used to adjust the crystal orientation of this silicon steel product (this is the overall texture of the material). An isotropic material is produced from this jumble of unoriented grain (where magnetic properties are omnidirectional). This is the more cost-effective choice, and it is used in circumstances in which cost is prioritized above efficiency and in which the magnetic flux does not need to be kept constant. CRNGO is often found in electric motors and generators that have moving components.

Non-oriented silicon steels don't require a secondary recrystallization process for their property development, nor is a high-temperature anneal necessary. Hence, the lower limit on silicon is not essential. Non-oriented silicon steels contain between 0.5 and 3.25% Si plus up to 0.5% Al. This addition increases resistivity and lowers the temperature of primary recrystallization.

Non-oriented silicon steels find usage in large rotating equipment, including motors, power generators, and AC alternators. These steels can come in two conditions: fully-processed or semi-processed.

Cold-rolled-grain-oriented steel (CRGO)

The magnetic flux in this silicon steel is steady and directed to the processing. The rolling procedure gave it a highly ordered crystal structure, which can be seen in its appearance. Cold-rolled strips with a thickness of less than 2mm are made from CRGO, which is provided in coil form. First, the coil is rolled out, and then it is cut into the desired shape. This process is repeated for both grain-oriented and non-grain-oriented laminated sheets. This is the motivation for the need of its workability.

The manufacturing of oriented silicon steel requires a more controlled composition and more sophisticated processing. The final texture development process includes a series of careful working and annealing operations, ensuring that the material stays essentially single-phase, particularly during the final anneal. This is because phase transformation destroys the texture.

The silicon content in today's commercial steel is about 3.25%. Although having more silicon might be favorable due to increased resistivity and lower magnetostriction, this leads to complications in cold rolling.

Cold rolled non grain oriented electrical steel

Non grain oriented electrical steel