Dec 01, 2025 Leave a message

Datasheet-For-Inconel-600-1-7-(1)-1-6.pdf

Comparison of Inconel 600 and 625 pipes

 
Comparison of Inconel 600 and 625 pipes
Comparison of Inconel 600 and 625 pipes
01

Comparison of Inconel 600 and 625 pipes

Due to its higher molybdenum content, Inconel 625 tubing offers superior strength and corrosion resistance, making it ideal for harsh environments such as marine and petrochemical plants. Inconel 600 tubing, on the other hand, is better suited for high-temperature applications with lower corrosion requirements, such as chemical processing and heat treatment. Alloy 625 tubing offers superior mechanical properties (higher strength, but lower hardness) and corrosion resistance, while Alloy 600 tubing is more economical and performs well at high temperatures without chloride corrosion issues.

02

What are the advantages of Inconel 625?

Inconel 625 alloy is an ideal choice for seawater applications because it possesses the following characteristics: it is not prone to localized corrosion (pitting and crevice corrosion), has high corrosion fatigue strength, high tensile strength, and is resistant to chloride stress corrosion cracking.

Inconel 625
 

Due to its higher molybdenum content, Inconel 625 tubing offers superior strength and corrosion resistance, making it ideal for harsh environments such as marine and petrochemical plants. Inconel 600 tubing, on the other hand, is better suited for high-temperature applications with lower corrosion requirements, such as chemical processing and heat treatment. Alloy 625 tubing offers superior mechanical properties (higher strength, but lower hardness) and corrosion resistance, while Alloy 600 tubing is more economical and performs well at high temperatures without chloride corrosion issues.

 

Standard Specification For Inconel 600 / 625 Pipes & Tubes

Specifications : ASTM B167, B163, B516, B517, B704, B705 / ASME SB167, SB163, SB516, SB517, SB704, SB705

Dimensions : ASTM, ASME and API

Size Range : 15"NB – 150"NB

Outer Diameter : 6.35 mm OD upto 254 mm OD in 0.6 TO 20 mm thickness.

Schedule : SCH 10, SCH20, SCH30, SCH40, STD, SCH60, XS, SCH80, SCH120, SCH140, SCH160, XXS

Type : Seamless / ERW / Welded / Fabricated / LSAW Pipes

Length : Single Random, Double Random & Cut Length

Form : Round Pipes/Tubes, Square Pipes/Tubes, Pipe/Tubes, Coiled Tubes, "U" Shape, Pan Cake Coils, Hydraulic Tube

Grade : 600, 625

 

Inconel 600 / 625 Pipe and Tube Equivalent Grades

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
Inconel 600 2.4668 N06600 NCF 600 NA 13 МНЖМц 28-2,5-1,5 NC15FE11M NiCr15Fe
Inconel 625 2.4856 N06625 NCF 625 NA 21 ХН75МБТЮ NC22DNB4M NiCr22Mo9Nb

 

Chemical Composition of Inconel 600 / 625 Pipe Tube

Grade C Mn Si S Cu Fe Ni Cr
Alloy 600 0.15 max 1.00 max 0.50 max 0.015max 0.50 max 6.00 – 10.00 72.00 min 14.00 – 17.00
Alloy 625 0.10 max 0.50 max 0.50 max 0.015 max - 5.0 max 58.0 min 20.0 - 23.0
 

Mechanical Properties of Inconel 600 / 625 Pipe Tube

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Alloy 600 8.47 g/cm3 1413 °C (2580 °F) Psi – 95,000 , MPa – 655 Psi – 45,000 , MPa – 310 40 %
Alloy 625 8.4 g/cm3 1350 °C (2460 °F) Psi – 1,35,000 , MPa – 930 Psi – 75,000 , MPa – 517 42.5 %

 

Why Choose Gnee as Your Nickel-Based Alloy Supplier

✅ Over 18 years of export experience, products sold to more than 80 countries

✅ Certified by ISO, SGS, and BV

✅ Global inventory of Inconel, Hastelloy, Incoloy, and Monel alloy tubing, plates, and bars

✅ Custom processing services available – including cutting, polishing, CNC machining, and packaging

✅ Fast delivery within 7-15 days, supported by global logistics partners

📦 Packaging and Shipping

All stainless steel products are packaged using the following methods:

Wooden pallets or crates

Moisture-proof packaging

Labels with furnace number, standard, and size labels

Shipped worldwide by sea, air, or express

 

About Gnee Steel

Gnee Steel is a supplier of Inconel 600 alloy, offering a wide range of products including: seamless pipe (sizes: 4-219 mm; thickness: 0.5-20 mm); welded pipe (sizes: 5.0-1219.2 mm; thickness: 0.5-20 mm); plates (thickness: 0.1 to 100 mm; width: 10-2500 mm); strips; alloy round bars (diameter: 3-800 mm); flat bars (thickness: 2-100 mm; width: 10-500 mm); hexagonal bars (size: 2-100 mm); wire rods; and extruded profiles. We collaborate with steel mills to provide our customers with Inconel 600 alloy products that meet or exceed numerous leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN, and BS standards.


Gnee Steel stocks and sells Inconel 600, pipes, plates, strips, round bars, flat bars, forged billets, hexagonal steel, wire rods, and extruded profiles. Please feel free to contact us at ss@gneesteel.com for a quote.

Gnee Steel

Send Inquiry

whatsapp

Phone

E-mail