Comparison between Nickel Alloy 200 and Nickel 600
Nickel Alloy 200 and Nickel 600 are different materials. Nickel Alloy 200 is commercially pure nickel, widely used due to its excellent corrosion resistance in strong alkalis and high electrical conductivity. In contrast, Nickel 600 is a nickel-chromium-iron alloy with higher mechanical strength and greater heat resistance, designed specifically for high-temperature and corrosive environments, such as in the chemical, aerospace, and electronics industries.
Will Nickel 200 rust?
Corrosion Resistance: Nickel 200/201 exhibits excellent corrosion resistance in reducing, neutral, and oxidizing atmospheres, provided that a passivating oxide film can form in the oxidizing atmosphere. This oxide film endows the alloy with excellent corrosion resistance in corrosive environments.

What is nickel alloy 600?
Nickel Alloy 600, also marketed under the brand name Inconel 600, is a unique nickel-chromium alloy renowned for its oxidation resistance at high temperatures. It has a wide range of applications, from low-temperature applications to high-temperature applications up to 2000°F (1093°C).
What is Nickel 200 alloy?
Nickel 200 (UNS N02200/W.Nr. 2.4060 and 2.4066) is commercially available forged nickel with a purity of 99.6%. It possesses good mechanical properties and excellent corrosion resistance.
Chemical Composition Comparison: Nickel 200 vs Nickel 600
| Element | Nickel 200 (UNS N02200) | Nickel 600 (UNS N06600) |
|---|---|---|
| Nickel (Ni) | ≥ 99.6 % | ≥ 72.0 % |
| Chromium (Cr) | – | 14.00 – 17.00 % |
| Iron (Fe) | ≤ 0.20 % | 6.00 – 10.00 % |
| Manganese (Mn) | ≤ 0.35 % | ≤ 1.00 % |
| Silicon (Si) | ≤ 0.15 % | ≤ 0.50 % |
| Carbon (C) | ≤ 0.15 % | ≤ 0.15 % |
| Sulfur (S) | ≤ 0.01 % | ≤ 0.015 % |
| Copper (Cu) | ≤ 0.25 % | ≤ 0.50 % |
| Aluminum (Al) | – | ≤ 0.30 % |
| Titanium (Ti) | – | ≤ 0.30 % |
| Cobalt (Co) | ≤ 0.25 % | – |
| Magnesium (Mg) | ≤ 0.15 % | – |
| Phosphorus (P) | – | – |
| Boron (B) | – | – |
| Other Elements | ≤ 0.05 % | ≤ 0.30 % |
Mechanical Properties Comparison: Nickel 200 vs Nickel 600
| Property | Nickel 200 (UNS N02200) | Nickel 600 (UNS N06600) |
|---|---|---|
| Tensile Strength | 380 – 550 MPa | 550 – 690 MPa |
| Yield Strength (0.2% Offset) | 150 – 250 MPa | 240 – 350 MPa |
| Elongation | 40 – 55 % | ≥ 30 % |
| Hardness (Annealed) | 45 – 70 HRB | 65 – 90 HRB |
| Modulus of Elasticity | 200 GPa | 207 GPa |
| Fatigue Strength (Rotating Beam) | 180 – 220 MPa | 270 – 310 MPa |
| Impact Toughness (Charpy V-Notch) | > 100 J (at 20°C) | > 100 J (at 20°C) |
| High-Temperature Tensile Strength (at 600°C) | ≈ 120 MPa | ≈ 350 MPa |
| High-Temperature Yield Strength (at 600°C) | ≈ 80 MPa | ≈ 180 MPa |
| Creep Rupture Strength (700°C, 1000h) | Not typically used at this temperature | ≈ 60 MPa |
| Thermal Expansion Coefficient (20–100°C) | 13.3 μm/m·°C | 13.3 μm/m·°C |
| Thermal Conductivity (100°C) | 82 W/m·K | 14.8 W/m·K |
| Maximum Recommended Service Temperature (Continuous) | ≈ 315°C | ≈ 1095°C |
| Density | 8.89 g/cm³ | 8.47 g/cm³ |
| Electrical Resistivity (at 20°C) | 0.086 μΩ·m | 1.03 μΩ·m |
| Magnetic Permeability (Annealed) | 1.0 μ (non-magnetic) | 1.01 – 1.10 μ (slightly magnetic) |
| Feature | Nickel Alloy 200 | Nickel Alloy 600 (Inconel 600) |
|---|---|---|
| Composition | Commercially pure nickel (99.6%) | Nickel-chromium-iron alloy |
| Key Property | High corrosion resistance in neutral and alkaline environments | High strength and excellent oxidation resistance at high temperatures |
| Maximum Service Temperature | Generally limited to below 315°C (600°F) to avoid graphite formation | Up to 2000°F (1093°C) |
| Tensile Strength (UTS) | 420 – 540 MPa | 650 – 990 MPa |
| Electrical Conductivity | High (18% IACS) | Low (1.7% IACS) |
| Corrosion Resistance | Excellent in reducing/neutral media and caustic environments | Excellent in both oxidizing and reducing conditions at high temperatures |
| Applications | Chemical processing, food processing, marine applications | Aerospace, nuclear reactors, chemical processing at high temperatures |
Why Choose Gnee as Your Nickel-Based Alloy Supplier
✅ Over 18 years of export experience, products sold to more than 80 countries
✅ Certified by ISO, SGS, and BV
✅ Global inventory of Inconel, Hastelloy, Incoloy, and Monel alloy tubing, plates, and bars
✅ Custom processing services available – including cutting, polishing, CNC machining, and packaging
✅ Fast delivery within 7-15 days, supported by global logistics partners
📦 Packaging and Shipping
All stainless steel products are packaged using the following methods:
Wooden pallets or crates
Moisture-proof packaging
Labels with furnace number, standard, and size labels
Shipped worldwide by sea, air, or express
Gnee Steel also supplies custom Inconel 600 products in various sizes and specifications. Please send us your drawings for a quote!