Oct 29, 2024 Leave a message

Classification of strengthening methods of nickel-based high-temperature alloys

Nickel-based high-temperature alloys can be divided into solid solution strengthened alloys and precipitation strengthened alloys according to different strengthening methods.
Solid solution strengthened alloys have certain high temperature strength and good oxidation resistance. In addition, they also have good hot corrosion resistance, hot and cold fatigue resistance, weldability and plasticity.
This alloy is suitable for manufacturing parts with high working temperature and low stress, such as the combustion chamber of a gas turbine.
Precipitation strengthened alloys adopt three strengthening methods: solid solution strengthening, precipitation strengthening and grain boundary strengthening. They have good oxidation resistance, fatigue resistance, hot corrosion resistance and high temperature creep strength. This alloy is suitable for manufacturing parts with high stress at high temperature, such as turbine blades and turbine disks of gas turbines.
1. Solid solution strengthening: By adding W, Mo, Cr, Ta, Nb and other elements to the matrix alloy, these elements are inconsistent with the lattice constant of the matrix, resulting in matrix lattice distortion, reducing stacking fault energy, producing short-range order and atomic segregation, thereby hindering dislocation movement and improving the thermal strength of the alloy. The solid solution strengthening effect is mainly reflected in two aspects: when the temperature is lower than 0.6Tm, the lattice distortion increases the slip resistance and makes the slip deformation difficult; when the temperature is higher than 0.6Tm, the interatomic bonding force increases, the element diffusion capacity decreases, the recrystallization temperature increases, and the diffusion deformation is hindered.
‌2. Precipitation strengthening: by adding elements such as Al, Ti, Nb, Re, Ta to the alloy to form a stable γ′ phase, or adding elements such as C and B to form various types of carbides. These second phases precipitate in the matrix in a coherent form, forming a strong elastic stress field, hindering the movement of dislocations, and thus strengthening the matrix. The γ′ phase is coherent with the matrix, and has the same crystal lattice. It can be cut by the moving dislocations to form antiphase domain boundaries and superlattice dislocations, further strengthening the matrix.
‌3. Grain boundary strengthening: by adding elements such as B, C, and Zr to fill atomic vacancies, improve the alloying degree of grain boundaries, and purify grain boundaries. This method improves the overall performance of the alloy by increasing the strength and stability of the grain boundaries.

Nickel-based high-temperature alloys Nickel-based high-temperature alloys