Sep 28, 2026 Leave a message

ASTM B168 Inconel 600 Alloy sheet / plate:Properties and Typical Applications

Inconel 600 Alloy sheet /plate, designated UNS N06600, is a nickel-chromium-iron solid-solution strengthened alloy plate product produced to multiple ASTM standards. It retains stable mechanical properties across cryogenic to 1095°C, delivers resistance to oxidation and chloride-ion stress corrosion cracking. It maintains performance in both oxidizing and mild reducing environments.

 

GNEE supplies cut-to-size plates with MTC test certificates for high-temperature and corrosive industrial service.

 

INCONEL® Alloy 600

   

Inconel 600 UNS N06600 Alloy sheet:Executive Standards & Grade Overview

 

Inconel 600 alloy sheets and plates follow unified international industrial standards to ensure interchangeability and engineering reliability. The core applicable standard is ASTM B168, which specially regulates size, tolerance, performance and inspection requirements for alloy flat products.

 

Other recognized equivalent standards include AMS 5540 and German standard W.Nr 2.4816. All GNEE supplied Inconel 600 sheets and plates strictly comply with above specifications, supporting global industrial project acceptance.

 

Inconel 600 Alloy sheet Chemical Composition (ASTM B168 Standard)

 

The stable performance of Inconel 600 is derived from its strict chemical composition control. High nickel content is the core of its excellent corrosion and high-temperature resistance. The standard component range is shown in the table below.

 

Element

Weight Percentage (%)

Ni+Co

≥72.0

Cr

14.0 – 17.0

Fe

6.0 – 10.0

C

≤0.15

Mn

≤1.00

Si

≤0.50

 

Inconel 600 Alloy sheet Mechanical Properties (Annealed State)

 

Inconel 600 sheets and plates maintain balanced mechanical strength and ductility at room temperature and medium-high temperature. The annealed state is the most commonly used delivery state, suitable for subsequent bending, welding and forming processing.

 

Performance Item

Standard Value

Tensile Strength

≥550 MPa

Yield Strength (0.2% Offset)

≥240 MPa

Elongation

≥30%

Hardness

≤195 HB

 

The alloy retains stable structural toughness under thermal cycling conditions. It will not produce obvious brittle deformation or performance attenuation, meeting the long-term service requirements of industrial equipment.

 

Inconel 600 Nickel Alloy:Core Performance Characteristics

 

Inconel 600 UNS N06600 sheet and plate have irreplaceable advantages compared with ordinary stainless steel and other nickel alloys, adapting to complex harsh working conditions.

 

1.High-Temperature Oxidation & Carburization Resistance

Inconel 600 (UNS N06600) relies on 14.0–17.0% chromium alloying elements to form a dense, adherent Cr₂O₃ passivation film on the material surface. This stable oxide layer suppresses oxygen diffusion and metal matrix oxidation at high temperatures. The alloy maintains structural stability in continuous and cyclic high-temperature thermal environments, avoiding scaling, peeling and matrix ablation that commonly occur in 304 and 316 stainless steel.

 

Service Atmosphere

Max Continuous Service Temperature

Max Cyclic Service Temperature

Core Performance Index

Dry Air / Oxidizing Environment

1177°C

1093°C

No oxide peeling, stable passivation film

High-temperature Steam

870°C

760°C

Resists steam oxidation and internal diffusion corrosion

Carburizing Furnace Atmosphere

950°C

850°C

Suppresses carbon penetration and matrix brittleness

 

2.Chloride Stress Corrosion Cracking Resistance

Stress corrosion cracking (SCC) is the dominant failure mode of ordinary austenitic stainless steel in chloride-containing high-temperature water and brine environments. Inconel 600 contains more than 72% nickel base, which effectively inhibits the dislocation slip and crack propagation mechanism induced by chloride ions. The high-nickel microstructure eliminates the SCC sensitivity of 304/316 stainless steel under tensile stress + chloride coupling conditions.

 

Material Grade

Nickel Content

Chloride SCC Resistance

Applicable Working Condition

Inconel 600

≥72.0%

No cracking after long-term cyclic chloride exposure

High-temperature brine, seawater circulation, chloride chemical medium

304 Stainless Steel

8.0%–10.5%

Prone to transgranular SCC above 60°C

Unable to adapt to high-temperature chloride working conditions

316L Stainless Steel

10.0%–14.0%

SCC failure occurs in concentrated chloride environment

Limited service life in high-salinity industrial systems

 

3.Medium Corrosion Resistance in Alkaline & Weak Acid Environments

Inconel 600 alloy matrix maintains stable chemical inertness in high-concentration alkaline solutions, halogen compounds and low-ph corrosive media. Unlike stainless steel which is prone to pitting corrosion and intergranular corrosion in alkaline aging environments, Inconel 600 does not produce corrosion product accumulation or surface pitting after long-term contact with NaOH, KOH and other alkaline media.

 

Corrosive Medium

Working Temperature

Annual Corrosion Rate

Service Performance

50% NaOH Alkaline Solution

≤150°C

≤0.02 mm/y

No pitting or intergranular corrosion

Dilute Sulfuric Acid & Weak Acid Mixed Medium

≤80°C

≤0.015 mm/y

Stable surface passivation state

Halogen-containing Industrial Wastewater

60–120°C

≤0.025 mm/y

Resists local selective corrosion

 

4.Cold & Hot Working and Welding Adaptability

Inconel 600 is supplied in fully annealed state, with uniform internal grain structure and low work hardening rate. Compared with high-strength nickel alloys, it has lower processing resistance and forming residual stress. The alloy supports conventional cold working processes such as precision cutting, plane bending, roller rolling and stamping forming, and can achieve complex structural sizing without preheating treatment.

 

Processing Type

Process Parameters

Processing Performance Index

Cold Bending Forming

Room temperature processing, conventional bending radius

No cracking, flatness tolerance ≤±0.5mm/m

Hot Rolling & Shaping

Processing temperature 950–1150°C

Uniform grain, no local thinning defect

Welding Process

GTAW/GMAW conventional welding

Weld seam compact, no hot crack or porosity defect

 

5.Thermal Cycle Structural Stability

Industrial high-temperature furnace equipment often works in repeated heating and cooling cycle conditions. Ordinary alloy materials are prone to brittle phase precipitation, grain growth and thermal fatigue failure after long-term thermal cycling. Inconel 600 nickel-chromium solid solution structure maintains stable single-phase austenite state in the temperature range of room temperature to 1093°C, without harmful carbide precipitation and phase transformation.

 

Thermal Cycle Condition

Cyclic Times

Post-cycle Performance Change

200°C ↔ 900°C rapid temperature change

500 cycles

No phase transformation, stable mechanical properties

200°C ↔ 900°C rapid temperature change

1000 cycles

Dimensional variation ≤0.1%, no thermal fatigue crack

Long-term constant temperature 900°C aging

1000h aging

No brittle phase precipitation, stable hardness value

 

Inconel 600 Alloy Plate Heat Treatment and Production Process

The performance stability of Inconel 600 plate depends on standardized hot rolling precision control and strict post-process heat treatment system. GNEE adopts integrated production procedures from raw material inspection, hot rolling forming, solution annealing to finished product finishing, eliminating internal stress and structural defects to ensure consistent batch performance.

 

astm b166/b168 inconel 600 bar plate standards

Solution Treatment & Aging Heat‑Treatment Furnace Actual Shot

1.Raw Material Inspection & Preparation

Before production, each batch of Inconel 600 raw steel ingots undergoes PMI spectral detection to verify Ni, Cr, Fe and trace element components, ensuring compliance with UNS N06600 and ASTM B168 standards. Raw materials are pretreated by surface grinding and oxide layer removal to avoid impurity inclusion and surface defects in subsequent rolling.

 

2.High-temperature Hot Rolling Forming

The ingot is heated uniformly in a heating furnace at 1050–1180°C to ensure uniform internal temperature and eliminate component segregation. Controlled multi-pass hot rolling is adopted to gradually shape the plate, precisely controlling rolling speed and pressing reduction. This process ensures uniform thickness tolerance and compact internal structure, avoiding layered defects and loose grains.

 

3.Core Solution Annealing Treatment

Solution annealing is the key heat treatment process for Inconel 600 plate performance. After hot rolling, the plate is heated to 1010–1050°C for sufficient heat preservation, then rapidly water-cooled. This process dissolves intergranular carbides into the matrix to obtain uniform single-phase austenite structure.

 

Standard solution treatment eliminates processing residual stress, improves material ductility and processing performance, and fundamentally enhances intergranular corrosion resistance and thermal cycle stability. All GNEE finished plates are delivered in fully annealed state to meet subsequent bending, welding and high-temperature service requirements.

 

4.Surface Finishing & Flatness Correction

After heat treatment, the alloy plate is leveled by precision straightening equipment to eliminate local bending and wave deformation. The surface is polished and pickled to remove high-temperature oxide scale and rolling traces, achieving uniform surface roughness and flatness index. Non-standard size plates support customized cutting and edge finishing.

 

5.Full-item Finished Product Inspection

Finished Inconel 600 plates undergo dimensional tolerance detection, surface defect inspection, hardness testing and mechanical tensile testing. For thick plates used in pressure equipment, ultrasonic NDT inspection is implemented to eliminate internal cracks and inclusions. All batches are equipped with complete 3.1 test reports to meet international engineering acceptance standards.

 

 

Difference Between Inconel 600 Sheet and Plate

 

Although made of the same UNS N06600 material, sheets and plates differ in processing technology, thickness range and application scenarios, which are selected according to actual engineering needs.

 

Inconel 600 Sheet

It is processed by cold rolling with thin thickness, smooth and flat surface and high dimensional accuracy. It is mostly used for equipment lining, thermal insulation shielding plates, thin-wall protective structures and decorative anti-corrosion layers.

 

Inconel 600 Plate

It is produced by hot rolling with thicker specification and stronger bearing capacity. It is mainly used for pressure-bearing structural parts, equipment cylinder plates, flange substrates and high-load anti-corrosion components.

 

Inconel 600 Sheet and Plate Typical Industrial Applications

 

Relying on comprehensive high-temperature and anti-corrosion performance, Inconel 600 sheets and plates are widely used in high-end industrial fields with strict working condition requirements.

 

Heat Treatment & Industrial Furnace Industry

Used for furnace liners, heat treatment baskets, furnace shielding plates and high-temperature circulating structural parts. It resists high-temperature oxidation and prolongs the service life of furnace body components.

01

Chemical & Petrochemical Industry

Suitable for reaction kettle lining, heat exchanger plates, corrosion-resistant container components in chloride and alkaline medium environments. It avoids stress corrosion cracking failure.

02

Nuclear Power & Energy Generation Industry

Applied to nuclear power auxiliary equipment, high-temperature pure water system components and power plant high-temperature protective plates. It features stable performance and high safety coefficient.

03

Aerospace & Precision Machinery

Used for high-temperature heat insulation baffles, sealing structural parts and anti-corrosion protective components of aerospace equipment, adapting to variable temperature and harsh service environments.

04

Pulp & Paper Industrial Equipment

It serves anti-corrosion structural plates in pulp bleaching and corrosive liquid treatment systems, effectively resisting medium erosion and improving equipment stability.

05

 

Processing, Fabrication & Quality Control

 

GNEE provides one-stop customized processing services for Inconel 600 UNS N06600 sheets and plates. According to customer drawings and engineering requirements, we support precision cutting, bending, polishing, rolling and non-standard sizing processing.

 

In terms of quality control, we implement full-process inspection. Raw materials pass strict PMI positive material identification to ensure accurate alloy composition. Finished products undergo dimensional calibration, surface defect detection and hardness testing.

 

For thick plates used in pressure-bearing equipment, we support ultrasonic NDT non-destructive testing to eliminate internal inclusions and cracks. All products can be equipped with complete 3.1 material test certificates to meet international project acceptance standards.

 

Inconel 600 Tech Data
PMI‑Spectral Analysis
Inconel 600 - Introduction, Applications And Data Sheet
UT‑Ultrasonic Testing
Inconel 600 Plate and ASTM B168 UNS N06600 Sheet
Hardness Testing

 

Contact now

 

📦 Packaging and Shipping:

 

  • Our nickel-based alloy products adopt industrial anti-corrosion packaging for overseas shipment:
  • Heat-treated wooden pallets or solid export crates
  • Multi-layer moisture-proof & rust-resistant wrapping
  • Marked labels with heat number, material grade, standard and dimensions
  • Global delivery options: sea freight, air freight and courier express

 

INCONEL Alloy 600

  

 

FAQ:

What are the key differences between Inconel 600 and Inconel 750?

Inconel 600 is a solid-solution strengthened nickel alloy, while Inconel X-750 is a precipitation-hardenable alloy enhanced with aluminum and titanium for much higher strength.

 

What are the key differences between Inconel 600 and Inconel 718?

Inconel 600 is designed for extreme high-temperature oxidation resistance up to 2000°F (1095°C), while Inconel 718 is a precipitation-hardened alloy built for superior mechanical strength and load-bearing performance up to 1200°F (650°C).

 

What are the key differences between Inconel 600 and 625?

Inconel 600 is a nickel-chromium-iron alloy built for high-heat oxidation resistance, while Inconel 625 adds molybdenum and niobium for superior mechanical strength and exceptional resistance to severe marine and acid corrosion.

 

Send Inquiry

whatsapp

Phone

E-mail

Inquiry