Nov 09, 2025 Leave a message

Datasheet-For-Inconel-600-1-7-(1)-1-6.pdf

ASTM B166 UNS N06600 Nickel Alloy Bright Annealed Bar

 
 
 
ASTM B166 UNS N06600 Nickel Alloy Bright Annealed Bar
ASTM B166 UNS N06600 Nickel Alloy Bright Annealed Bar
01.

ASTM B166 UNS N06600 Nickel Alloy Bright Annealed Bar

ASTM B166 UNS N06600 is a high-strength nickel-chromium alloy bar with good oxidation resistance and excellent resistance to chloride stress corrosion cracking, suitable for high-temperature and corrosive environments such as chemical plants and nuclear power plants. A bright annealed surface refers to a bright, polished surface obtained through a bright annealing process, which improves surface finish and reduces absolute roughness.

02.

What is the maximum operating temperature of Inconel 600?

2000°F

Inconel 600 (AMS 5540) is a nickel-chromium alloy designed for low-temperature and high-temperature environments up to 2000°F (1093°C).

Inconel 600

Inconel 600 round bars are a nickel-based alloy with good carburizing properties and excellent high-temperature corrosion resistance. Inconel 600 round bars effectively resist dry chlorine and many other gases at moderately high temperatures. Alloy 600 bars are a nickel-chromium alloy with good high-temperature oxidation resistance and resistance to decomposition cracking under chloride pressure, corrosion from high-cleanliness water, and acid oxidation. Inconel 600 flat bars are also a nickel-chromium-iron alloy with good high-temperature corrosion resistance and resistance to rapid corrosion under chloride ion pressure, corrosion from high-cleanliness water, and combustion corrosion.

 

The chemical composition of this nickel-based steel alloy is carefully designed to provide excellent resistance to a variety of corrosive environments. Inconel 600 is a standard engineering material with excellent heat and corrosion resistance. Inconel 601 also features high strength, good machinability, excellent metallurgical stability, and high resistance to carburizing. Inconel 600 is hardened and strengthened through cold working processes.

 

ASTM B166 UNS N06600 Chemical Composition:

Alloy C Mn Si S Cu Fe Ni Cr Al Ti
600 0.15 max 1.00 max 0.5 max 0.015 max 0.5 max 6.0-10.0 72.0 min 14.0-17.0 - -

 

ASTM B166 UNS N06600 Mechanical Properties:

Nickel Alloy Tensile Stress Yield Stress (0.2%Offset) Elongation
600 Psi - 120,000 , MPa - 825 Psi - 90,000 , MPa - 620 7-12%

 

Common Applications

Chemical Processing: Equipment used to process various acids (e.g., fatty acids) and other corrosive compounds.

Nuclear Industry: Commonly used in nuclear power plants and reactors due to its high temperature and corrosion resistance.

Heat Treatment: Used in high-temperature furnace applications.

Aerospace and Gas Turbines: Components used in jet engines and gas turbines.

Electronics: Can be used in electronic components.

 

Ordering and Specifications

Sizes: Diameters range from 3 mm to 600 mm, and lengths up to 6000 mm; custom sizes are also generally available.

Shapes: Available in a variety of shapes, including round, hexagonal, and square bars.

Standardization: Materials conform to ASTM B166 and ASME SB-166 standards.

Processing: Bars can be produced through hot rolling, cold drawing, or forging processes.

 

Why Choose Gnee Nickel Alloy (Supplier Example)?

✅ Large stock of Inconel series alloy tubes/bars/plates/fittings available for fast shipping.

✅ Factory direct sales, highly competitive prices, excellent value for money.

✅ Comprehensive quality assurance: Material Testing Certificate (MTC), chemical composition certificate, and mechanical property certificate.

✅ Value-added services: slitting, cutting, polishing, surface treatment.

✅ Worldwide shipping, secure and reliable packaging, and provision of export-required documents.

 

About Gnee Steel

Gnee Steel is a supplier of Inconel 600 and Inconel 725, offering a wide range of products including: seamless pipe (sizes: 4-219 mm; thickness: 0.5-20 mm); welded pipe (sizes: 5.0-1219.2 mm; thickness: 0.5-20 mm); plates (thickness 0.1 to 100 mm; width 10-2500 mm); strips; alloy round bars (diameter 3-800 mm); flat bars (thickness 2-100 mm; width 10-500 mm); hexagonal bars (size 2-100 mm); wire rods; and extruded profiles. We collaborate with steel mills to provide customers with 600/725 alloys, whose products meet or exceed numerous leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN, and BS standards.


Gnee Steel stocks and sells Inconel 600 and Inconel 725, pipes, tubes, plates, strips, round bars, flat bars, forged billets, hexagonal steel, wire rods, and extruded profiles. Please feel free to contact us at ss@gneesteel.com for a quote.

Gnee Steel
ASTM B166 UNS N06600 Nickel Alloy Bright Annealed Bar
ASTM B166 UNS N06600 Nickel Alloy Bright Annealed Bar
ASTM B166 UNS N06600 Nickel Alloy Bar
ASTM B166 UNS N06600 Nickel Alloy Bar

Send Inquiry

whatsapp

Phone

E-mail

Inquiry