Oct 23, 2025 Leave a message

ASTM B163 UNS N08825 Heat Retaining Alloy Seamless Pipe

 
ASTM B163 UNS N08825 Heat Retaining Alloy Seamless Pipe
 

ASTM B163 UNS N08825 seamless tubing is an Incoloy 825 nickel-iron-chromium alloy known for its excellent corrosion resistance in a variety of corrosive environments. While it performs well at high temperatures, its primary attribute is corrosion resistance, not as a "heat-insulating" alloy. It is most commonly used in condensers and heat exchangers.

ASTM B163 UNS N08825 Heat Retaining Alloy Seamless Pipe

Is Inconel 825 alloy magnetic?

 

Inconel 825 Alloy

Inconel 825 is generally nonmagnetic. The alloy is composed of a blend of nickel, iron, and chromium, with added molybdenum, copper, and titanium. These elements enhance its overall corrosion resistance and maintain its nonmagnetic properties.

ASME B163 covers nickel and nickel alloy seamless tubing for condensers and heat exchangers. This standard covers outside diameter and average wall thickness, or outside diameter and minimum wall thickness. Tubing shall be of the alloys and conditions specified in this specification. The material shall conform to the specified compositional limits for nickel, copper, molybdenum, iron, manganese, carbon, silicon, chromium, aluminum, titanium, phosphorus, cerium, zirconium, yttrium, boron, cobalt, niobium, tungsten, and nitrogen. The material's tensile strength, yield strength, elongation, and Rockwell hardness shall conform to the mechanical property requirements of this specification. Test methods include chemical analysis, tensile strength, rounding procedure, Rockwell hardness, grain size, and hardness conversion.

 

SB163, SB423, and N08825 nickel alloy seamless tubing are nickel-iron-chromium alloys with additions of molybdenum and copper. The chemical composition of this nickel-steel alloy is designed to provide excellent resistance to a wide range of corrosive environments. It is similar to Alloy 800 but exhibits improved resistance to aqueous corrosion. It offers excellent resistance to reducing and oxidizing acids, stress corrosion cracking, and localized corrosion such as pitting and crevice corrosion. 825 Alloy Incoloy 825 is particularly resistant to sulfuric and phosphoric acid corrosion. This nickel steel alloy is used in chemical processing, pollution control equipment, oil and gas well piping, nuclear fuel reprocessing, acid production, and pickling equipment.

 

ASTM B163 UNS N08825 Heat Retaining Seamless Pipe Chemical Composion:

Element %
Nickel 38.0-46.0
Chromium 19.5-23.5
Molybdenum 2.5-3.5
Copper 1.5-3.0
Titanium 0.6-1.2
Iron 22.0 min (~33%)
Carbon 0.05 max
Manganese 1.0 max
Sulphur 0.03 max
Silicon 0.5 max
Aluminium 0.2 max


UNS N08825 Heat Retaining Seamless Pipe Physical Properties:

Density / Specific Gravity 8.1 kg/m³ 0.30 lb/in³
Melting point 1370-1400℃


UNS N08825 Heat Retaining Pipe Mechanical Properties:

Alloy state Tensile strength Yield strength Elongation Brinell hardness
Rm N/mm² R P0. 2N/mm² A 5 % HRB Max
N08825 517 172 30 200
Hot Finished
N08825 586 241 30 200
Cold Finished

 

Common Applications
UNS N08825 pipe's corrosion resistance and high-temperature resistance make it an ideal choice for a variety of industrial applications:
Condensers and heat exchangers: This is its primary intended use according to ASTM B163, and its seamless construction enables efficient and reliable heat transfer.
Chemical Processing: This alloy is resistant to a variety of acids and corrosive media, making it suitable for chemical processing vessels and piping.
Oil and Gas Industry: It is used for oil and gas well piping and equipment, particularly in sour service environments.
Nuclear Industry: Applications include nuclear fuel reprocessing and radioactive waste disposal.
Pollution Control: It is also used in equipment specifically designed for pollution control.

 

Gnee Steel

 

About Gnee Steel

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.

Send Inquiry

whatsapp

Phone

E-mail

Inquiry