GNEE Steel is an acknowledged exporter , supplier , distributor of ASTM A240 TP422 Plate.We are ISO 9001:2008 certified manufacturer manufacturer of ASTM A240 Grade 422 plate & now we became Distributor of UNS S42200 Sheet & DIN 1.4935 Stainless Steel Plate. We maintain over 1000 ton SS 422 Plates in various shape,sizes & coating which makes us one of the largest stockholder 422 SS Plate in China.We are largest stockist and exporter of ASTM A240 TP422 Stainless steel Plate in China.We offer 422 stainless steel plate in various sizes at best price.We are well known trader of Stainless Steel 422 Plates in China .We producing supplier of stainless steel 422 plate & SS 422 Sheet.


ASTM A240 SS 422 Plate Specifications
| Description | ASTM A240 / ASME SA240 Stainless Steel Plates, ASTM A240 Hot Rolled Stainless Steel Plates |
| Standard | ASTM, ASME, BS, DIN, EN |
| Material | 310S, 310, 309, 309S, 316, 316L, 316Ti, 317, 317L, 321, 321H, 347, 347H, 304, 304L, |
| 302, 301, 201, 202, 403, 405, 409, 409L, 410, 410S, 420, 430, 631, 904L, Duplex, etc | |
| Specification | Cold rolled: 1219mm * 2438mm (4′ x 8′), 1219mm * 3048mm (4′ x 10′), 1220mm * 2440mm, 1250mm * 2500mm or as your requirement.
Hot rolled: 1500mm * 2000mm, 1000mm * 3000mm, 1500mm * 4000mm, 1500m * 6000mm or as your requiremnt. |
| Technique | Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) |
| Form | Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Etc. |
| Surface | 2B, 2D, BA, NO. 1, NO. 4, NO.8, 8K, Mirror, Checkered, Embossed, Hair Line, Sand Blast, Brush, Etching |
| Thickness | 0.25-200mm, 0.3mm to 120mm |
| Width | 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm |
| Length | 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, 12000mm |
| Package | Standard Export Seaworthy Package, or as required. |
| Value Added Services | Cladding,Heat Treatment,Annealed, Pickling, Polish,Rolling,Cutting,Bending,Forging,Minor Fabrication Etc. |
| MTC | Mill Test Certificate, Available as per EN 10204 3.1 |
ASTM A240 Stainless Steel 422 Sheet Chemical Composition
| Element | Content (%) |
|---|---|
| Iron, Fe | ~ 82 |
| Chromium, Cr | 11.0-13.0 |
| Manganese, Mn | 1.00 |
| Nickel, Ni | 0.5-1.0 |
| Molybdenum, Mo | 0.75-1.25 |
| Tungsten, W | 0.75-1.25 |
| Silicon, Si | 0.75 |
| Carbon, C | 0.20-0.25 |
| Vanadium, V | 0.15-0.3 |
| Phosphorous, P | 0.025 |
| Sulfur, S | 0.025 |
ASTM A240 TP422 Stainless Steel Plate Physical Properties
| Density (lb / cu. in.) | 0.287 |
| Specific Gravity | 7.94 |
| Specific Heat (Btu/lb/Deg F – [32-212 Deg F]) | 0.12 |
| Electrical Resistivity (microhm-cm (at 68 Deg F)) | 432 |
| Melting Point (Deg F) | 2590 |
| Modulus of Elasticity Tension | 28 |
ASTM A240 SS 422 Mechanical Properties
| Properties | Metric | Imperial |
|---|---|---|
| Elastic modulus | 190-210 GPa | 27557–30458 ksi |
| Poisson's ratio | 0.27-0.30 | 0.27-0.30 |
422 Stainless Metal Plates In Stock list
| ASTM A240 TP422 Stainless Steel 2B Finish Plate | ASTM A240 TP422 Stainless Steel Cold Rolled Plates |
| ASTM A240 TP422 Stainless Steel 4 Finish Plate | ASTM A240 TP422 Stainless Steel 2D Finish Plate |
| ASTM A240 TP422 Stainless Steel CR Plates | ASTM A240 TP422 Stainless Steel 8 Finish Plate |
| ASTM A240 TP422 Stainless Steel Hot Rolled Plates | Stainless Steel ASTM A240 TP422 HR Plates |
| ASTM A240 TP422 Stainless Steel Plates | ASTM A240 TP422 Stainless Steel Chequered Plate |