Dec 27, 2023 Leave a message

Analysis of performance parameters of Nickel270 pure nickel alloy

Analysis of performance parameters of Nickel270 pure nickel alloy

 

 

Overview of superalloys;

High temperature alloy is a special alloy material with excellent high temperature performance and corrosion resistance. It is mainly composed of nickel, chromium, molybdenum, tungsten and other elements. It is also called a "super alloy." It has the characteristics of high strength, high toughness, high heat resistance and high corrosion resistance, and is widely used in aviation, aerospace, energy , chemical industry and other fields.

Closer to home, let's talk about──────Nickel270 pure nickel alloy

Nickel 270 is a high-purity nickel alloy with a nickel content of more than 99.97% and good ductility and plasticity. It has a high melting point, corrosion resistance and thermal stability. Nickel 270 also has good electrical conductivity and permeability and is an important component of many electronic devices and magnetic materials.

Nickel270 chemical composition:

C(%): ≤0.02

Si(%): ≤0.001

Mn(%): ≤0.001

Cr(%): 0.001

Ni(%): ≥99.97

Mo(%):-

Co(%): ≤0.001

W(%):-

Al(%):-

Cu(%): ≤0.001

Ti(%): ≤0.001

Fe(%): ≤0.005

Others (%): Mg≤0.001,S≤0.001

Physical functions:

Density: 0.322 lb/in3, 8.91 g/cm3

Resistivity: ohm-cir-mil/ft, (μohmm): 45.0 (0.075)

Specific Heat: BTU/lb-°F (J/g-°K): 0.110 (460)

Thermal Conductivity: BTU-in/hr-ft2-°F (W/m - °C): 595 (86)

Average coefficient of thermal expansion: μin/in-°F (μm/m-°C) 70 - 200°F (20 - 95°C): 7.4 (13.3)

Modulus of elasticity: KSI (MPa) 30 x 103 (207 x 103)

Tension Permeability: Ferromagnetic Melting Scale: 2650°F (1454°C)

Nickel270 mechanical function at room temperature

Characteristics: Typical limits of annealing

Tensile strength: 50 KSI min (345MPa min)

Yield strength: 16 KSI min (110 MPa min)

Elongation: 50%min

Hardness: Rb 66 max

Gauge ≥0.010 inches Nickel270

Features: Quenched Nickel 270 can be cold worked into various conditions.

Analysis of performance parameters of Nickel270 pure nickel alloy

Analysis of performance parameters of Nickel270 pure nickel alloy

Form coils - sheets, strips, foil wires - profiles, round, flat, square

Processing and heat treatment: It is a difficult-to-process material in the field of mechanical processing.

Preheating: The surface of the workpiece must be cleaned before heating and during the heating process to keep the surface clean. If the heating environment contains sulfur, phosphorus, lead, or other low melting point metals, the alloy will become brittle. Impurities come from marking paint, chalk, lubricants, water, fuel, etc. The sulfur content of fuel should be low. For example, the impurity content of liquefied petroleum gas and natural gas should be less than 0.1%, the sulfur content of city gas should be less than 0.25g/m3, and the sulfur content of liquefied petroleum gas should be less than 0.5%.

The electric heating furnace should have precise temperature control capabilities, the furnace gas must be neutral or weakly alkaline, and fluctuations in the cationic chemistry and reducing properties of the furnace gas components should be avoided.

Hot processing: The suitable hot processing temperature of the alloy is 1120-900℃, and the cooling method can be water quenching or other rapid cooling methods. Annealing should be carried out in time after thermal processing to ensure optimal performance. During thermal processing, the material should be heated to the upper limit of the processing temperature. In order to ensure plasticity during processing, the final processing temperature when the deformation reaches 20% should not be lower than 960°C.

Cold working: Cold working should be carried out after solid solution treatment. The work hardening rate is higher than that of austenitic stainless steel, so the processing equipment must be adjusted accordingly, and there must be an intermediate annealing process during cold working.

Nickel270 is a very important material. Although the price is relatively high, its strong performance and wide range of applications make it a leader in the high-end alloy material market. Due to its purity and quality, Nickel 270 is used in medical, food processing and petroleum applications. In medical devices, it is used to manufacture high-quality products such as artificial joints, dental and surgical instruments. In the field of food processing, nickel 270 is used to make high-temperature baking equipment and high-temperature baking racks. In the petroleum industry, Nickel 270 is used in the production of protective equipment in corrosive and high-temperature environments.

In short, with the development of science and technology and the advancement of industry, high-temperature alloys are also constantly being developed and upgraded. Currently, researchers are developing a series of new high-temperature alloys to improve their mechanical properties and processing properties, and to explore their application in a wider range of fields. In the future, high-temperature alloys will continue to exert their unique advantages and become one of the important representatives in the field of high-performance materials.

 