AMS 5662 / AMS 5663 GH4169 Brightening and Polishing Rods

AMS 5662 / AMS 5663 GH4169 Brightening and Polishing Rods
AMS 5662 and AMS 5663 represent different heat treatment states of GH4169 (a Chinese-made alloy, equivalent to Inconel 718 or UNS N07718), a precipitation-hardening nickel-chromium superalloy. These bars are typically finished with a "bright" (bright machining or grinding) surface treatment and are generally used in high-strength aerospace fasteners and turbine components.
What is AMS 5662 material?
Inconel 718 nickel alloy
Inconel 718 nickel alloy - AMS 5662 - UNS N07718. Nickel alloy 718, commonly known as Inconel 718, is a precipitation-hardening, corrosion-resistant, and heat-resistant nickel alloy, available in various forms including bars, forgings, plates, and sheets.

1.AMS 5662 and ASM 5663 GH4169 Rod Specifications Overview
| Parameter | AMS 5662 | AMS 5663 |
|---|---|---|
| Material | GH4169 (UNS N07718 / Inconel 718) | GH4169 (UNS N07718 / Inconel 718) |
| Specification Title | Nickel Alloy Bars, Forgings, and Rings | Nickel Alloy Bars, Forgings, and Rings (Alternative Heat Treatment) |
| Material Type | Wrought Nickel-based Superalloy | Wrought Nickel-based Superalloy |
| Strengthening Mechanism | γ″ + γ′ precipitation hardening | γ″ + γ′ precipitation hardening |
| Product Forms | Bar, forging, ring | Bar, forging, ring |
| Typical Applications | High-strength fasteners, turbine discs, shafts | High-temperature fasteners, turbine discs, springs, seals |
2. Chemical composition (weight percentage) of AMS 5662 and ASM 5663 GH4169
| Element | Content (%) | AMS Requirement | Function |
|---|---|---|---|
| Nickel (Ni) | 50.0 – 55.0 | 50.0 – 55.0 | Matrix element; high-temperature stability |
| Chromium (Cr) | 17.0 – 21.0 | 17.0 – 21.0 | Oxidation and corrosion resistance |
| Iron (Fe) | Balance (~18-20) | Balance | Fe-Ni-Cr base alloy |
| Niobium (Nb) | 4.75 – 5.50 | 4.75 – 5.50 | Core strengthening element – forms γ″ phase |
| Molybdenum (Mo) | 2.80 – 3.30 | 2.80 – 3.30 | Solid-solution strengthening; creep resistance |
| Titanium (Ti) | 0.65 – 1.15 | 0.65 – 1.15 | Forms γ′ strengthening phase |
| Aluminum (Al) | 0.20 – 0.80 | 0.20 – 0.80 | Forms γ′ strengthening phase; improves oxidation resistance |
| Carbon (C) | ≤ 0.08 | ≤ 0.08 | Low carbon for toughness |
| Manganese (Mn) | ≤ 0.35 | ≤ 0.35 | Deoxidizer |
| Silicon (Si) | ≤ 0.35 | ≤ 0.35 | Deoxidizer |
| Phosphorus (P) | ≤ 0.015 | ≤ 0.015 | Ensures toughness |
| Sulfur (S) | ≤ 0.015 | ≤ 0.015 | Ensures hot workability |
| Boron (B) | 0.002 – 0.006 | 0.002 – 0.006 | Grain boundary strengthener |
| Cobalt (Co) | ≤ 1.00 | ≤ 1.00 | Residual element |
| Copper (Cu) | ≤ 0.30 | ≤ 0.30 | Residual element |
3. Physical properties of AMS 5662 and ASM 5663 GH4169
| Property | Value | Significance |
|---|---|---|
| Density | 8.19 g/cm³ (0.296 lb/in³) | Weight calculation |
| Melting Range | 1260 – 1336°C (2300-2440°F) | Fire resistance margin |
| Thermal Conductivity (20°C) | 11.4 W/m·K | Heat dissipation |
| CTE (20-100°C) | 13.0 × 10⁻⁶/°C | Fitting compatibility |
| Specific Heat (20°C) | 435 J/kg·K | Thermal capacity |
| Modulus of Elasticity (20°C) | ~200 GPa | Stiffness |
| Electrical Resistivity | 1.25 µΩ·m | – |
| Magnetic Properties | Slightly magnetic | – |
Click to download the GH4169 alloy PDF file now
4. Material Specifications (GH4169 / Alloy 718)
AMS 5662 (Solution Annealed): This is the softest state, commonly used for manufacturing parts requiring machining or forming. It has good ductility and can be further hardened.
AMS 5663 (Precipitation Hardened): This is the fully heat-treated state (solution + aging). It provides maximum tensile strength and creep rupture strength at high temperatures.
Bright/Finish Finish: These bars are typically produced in a "bright" finish to indicate their excellent surface finish (smooth, clean, usually achieved through centerless grinding), reducing the need for subsequent machining.
Properties: These alloys exhibit excellent fatigue resistance, oxidation resistance up to 1000°C, and excellent corrosion resistance.
5. Common applications of GH4169
Aerospace: Gas turbine engine components, housings, and fasteners;
Marine: Marine technology;
Energy: Nuclear reactors and components.



6. GH4169 Selection Recommendations
| Requirement | Recommended Specification |
|---|---|
| General high-strength aerospace components | AMS 5662 |
| High-temperature fasteners | AMS 5663 |
| Springs and seals | AMS 5663 |
| Turbine discs and shafts | Either (verify design requirements) |
| When higher temperature capability is needed | AMS 5663 |
| Default / most common specification | AMS 5662 |
Why Choose Gnee as Your Nickel-Based Alloy Supplier
As a Tier-1 Manufacturer, we provide more than just raw material; we provide total quality transparency:
✅️VIM + VAR melting: Ensures zero internal inclusions, preventing "hard spots" that break tools.
✅️MTC 3.1 Traceability: Full heat-analysis and mechanical property verification documented with every batch.
✅️Global Compliance: Materials are fully compliant with UNS N07718, ASTM B637, and international aviation codes.
✅️Fast Global Shipping: We maintain a large inventory of 5.0mm to 50.0mm bright rods for immediate dispatch.

Gnee Alloy GH4169(inconel 718) Certificate
📦 Packaging and Shipping
All Nickel Based Alloy products are packaged using the following methods:
Wooden pallets or crates
Moisture-proof packaging
Labels with furnace number, standard, and size labels
Shipped worldwide by sea, air, or express

Gnee Alloy GH4169 Product Packing
Contact us for the latest export price quote for GH4169 Alloy
FAQ
Q1: Will your h9 tolerance rods work in a Citizen or Star Swiss lathe?
A: Yes. Our rods are specifically centerless ground to meet the exacting requirements of Swiss-type automatic lathes. The extreme straightness and tight tolerances ensure zero bar-feeder interference and zero vibration at high RPM.
Q2: Why is AMS 5662 better for my machine shop than AMS 5663?
A: Starting with AMS 5662 (Solution Treated) means you are cutting a much softer material. This significantly extends your CNC tool life and reduces machining time. You then perform the final 16-hour aging cycle on the nearly finished parts to reach the required high strength.
Q3: Is your GH4169 interchangeable with Inconel 718 bright rods?
A: Absolutely. GH4169 is the technische designation used in international blueprints for UNS N07718. They share the same chemical DNA and respond identically to heat treatment.
Q4: Do you offer trial orders for small batch fasteners?
A: Yes. We support R&D and prototype production by offering Flexible MOQs for all in-stock bright ground rods.