Alloy201 seamless pipe N02201 2.4068 mechanical properties
Alloy201
Alloy 201
Similar brands
Alloy 201 Nickel 201 N02201 2.4068
Chemical composition of Alloy 201:
Alloy 201 alloy %
Nickel Ni: balance
Iron Fe: ≤0.4
Carbon C: ≤0.02
Manganese Mn: ≤0.35
Silicon Si: ≤0.2
Copper Cu: ≤0.25
Magnesium Mg:≤0.15


Titanium Ti:≤0.1
Sulfur S: ≤0.01
Alloy 201 physical properties:
Density 8.89 g/cm3
Melting point 1440 ℃
The alloy is a solid solution strengthened nickel-based deformed high-temperature alloy with molybdenum and niobium as the main strengthening elements. It has excellent corrosion resistance and oxidation resistance, good tensile properties and fatigue properties from low temperature to 980°C, and is resistant to Stress corrosion in salt spray atmosphere. Therefore, it can be widely used in manufacturing aerospace engine parts, aerospace structural components and chemical equipment.