253MA heat-resistant alloy properties
253MA austenitic chromium nickel silicon alloy has excellent strength and unparalleled heat resistance. 253MA was developed over 30 years ago when the industry required heat-resistant stainless steel with high strength and good oxidation resistance.
Despite containing only 10 nickels, the 253MA alloy has excellent creep strength and high resistance to oxidation, sulfidation and corrosion/wear resistance. This makes 253MA alloy more economical than most heat-resistant alloys.
The high heat resistance of 253MA is obtained through strict control of micro-alloy additives. While the creep rupture strength benefit lies in the combination of nitrogen, carbon and cerium, its superior oxidation resistance is the result of the combination of cerium and silicon.
1. Chemical composition of 253MA: Carbon C: 0.05-0.10, Sulfur S: ≤0.030, Silicon Si: 1.40-2.00, Chromium Cr: 20.00-22.00, Nickel Ni: 10.00-12.00,


Nitrogen N: 0.14-0.20, Ce: 0.03-0.08.
fabrication and welding
Stainless steel 253 MA is easy to manufacture by standard commercial procedures. Stainless steel is tougher and easier to machine quickly than carbon steel. However, the work hardening tendency of this alloy can be minimized under conditions of positive feed and low speed combined with large amounts of cutting fluid.
Stainless steel 253 MA can be welded using conventional welding processes. Filler metal should be of similar composition for maximum weld integrity and performance.
2. Performance characteristics of 253MA: 1. Compared with 310S and 1Cr20Ni14Si2, it has superior performance, saves Ni and is cheap. 2. It has high strength at 900℃. In the air, it can be used up to 1150℃ under non-pressure conditions, and has excellent high temperature oxidation resistance. 3. The short-term tensile strength at each temperature is more than 20% higher than that of ordinary stainless steel (such as 304, 310S). 4. It has high temperature and long-term performance (creep performance, durability performance).
3. Corresponding grades of 253MA: German standard: 1.4835, X9CRNISINCE21-11-2, American standard: S30815, F45, 253MA.
Scope of use of 253MA: Widely used in sintering equipment, blast furnace equipment, steel melting, furnaces and continuous casting equipment, rolling mills (heating furnaces), heat treatment furnaces and accessories, mineral equipment and cement production equipment, etc. 253MA steel can be used in pressure-bearing situations up to 900°C and non-pressure-bearing high-temperature parts with working temperatures up to 1150°C.
253MA can be used in a variety of applications, here are just a few examples:
Pyrolysis vessel
boiler nozzle
corrugated carton
cyclone
radiant tube
combustion chamber
253MA heat-resistant alloy properties
Density: 8g/cm³
Melting range: 1371-1432⁰C
Poisson's ratio: 0.31
253MA can be used in a variety of applications, here are just a few examples:
Pyrolysis vessel
boiler nozzle
corrugated carton
cyclone
radiant tube
combustion chamber
253MA heat-resistant alloy properties
Density: 8g/cm³
Melting range: 1371-1432⁰C
Poisson's ratio: 0.31
253MA heat-resistant alloy specifications
UNS Company Number: S30815
W.Nr. Number: 1.4835
Standard: ASTM A182, A240, A276, A312, A479