UNS N06625 N06600 Inconel Pipe
video

UNS N06625 N06600 Inconel Pipe

Available Formats
GNEE Group offers Nickel Alloy Inconel UNS N06625 N06600 in a variety of forms, including:
Bars
Wires
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of uns n06625 n06600 inconel pipe in China. If you're going to wholesale high quality uns n06625 n06600 inconel pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

inconel Pipe Products

UNS n06625 n06600 inconel metal Pipe video

 

inconel Material Specification

Equivalent Grades

STANDARD WERKSTOFF NR. UNS AFNOR GOST JIS BS EN OR
Inconel / Incoloy 2.4816 N06600 NC15FE11M МНЖМц 28-2,5-1,5 NCF 600 NA 13 NiCr15Fe ЭИ868

Chemical Composition

Grade Cr Fe Ni C Mn Cu Si S
Inconel 600 14.0 – 17.0 6.0 – 10.0 72.0 min 0.15 max 1.0 max 0.5 max 0.5 max 0.015 max

Inconel Alloy 600 Seamless Pipe Specification

Trade name Inconel Alloy 600 Seamless Pipe
Alloy 600 Pipes Standard AISI, DIN, EN, GB, JIS, ASTM, ASME
Inconel 600 Seamless Pipe Dimensions ANSI/ASME B36.19, B36.10
ASTM B167 Inconel 600 Seamless Pipe OD 6.00 mm OD up to 250 mm OD, Sizes up to 12" NB
Wall Thickness 0.3mm – 50 mm
Inconel 600 Seamless Pipe Available Sizes

3/8″ NB to 12″ NB Schedule 10s

1/8″ NB to 12″ NB Schedule 40s

1/8″ NB to 12″ NB Schedule 80s

4″ NB to 8″ NB Schedule 120

1/2″ NB to 10″ NB Schedule 160

1/2″ NB to 6″ NB Schedule XXS

Pipe Schedule SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS

Inconel 625 Pipes and Tubes Specification

Alloy UNS N06625 Seamless Pipe and Tube : ASTM B444 / ASME SB444

Alloy UNS N06625 Welded Pipe : ASTM B705 / ASME SB705

Alloy UNS N06625 Welded Tube : ASTM B704 / ASME SB704

Standard : ASTM, ASME and API

Pipe Size : 15 NB UP TO 625 NB IN SCH 5S, 10S,10, 20, 40S, 40, STD, 60, 80S, 80, XS, 100, 120, 140, 160 & XXS

Tube Size : 1 mm OD upto 254 mm OD in 0.2 TO 20 mm thickness.

Type : Seamless / ERW / Welded / Fabricated

Length: Single Random, Double Random & Required Length, Cut Length

End : Plain End, Beveled End, Treaded

Inconel 625 Pipes & Tubes Equivalent Grades

STANDARD UNS WERKSTOFF NR. JIS AFNOR BS GOST EN
Inconel Alloy 625 N06625 2.4856 NCF 625 NC22DNB4M NA 21 ХН75МБТЮ NiCr22Mo9Nb

Inconel Alloy 625 Pipes & Tubes Chemical Composition

Grade C Mn Si S Cu Fe Ni Cr
Inconel 625 0.10 max 0.50 max 0.50 max 0.015 max - 5.0 max 58.0 min 20.0 - 23.0

UNS n06625 n06600 inconel Pipe

UNS n06625 n06600 inconel Pipe alloy suppliersUNS n06625 n06600 inconel seamless Pipe dealer

Inconel 625 Pipes and Tubes is the most versatile of Inconel products. It is known for its excellent fabricability, excellent corrosion resistance, high strength, etc. This all features are comes by his balance chemical composition. Inconel 625 includes chromium, nickel, molybdenum, and many more materials. This combination makes it unique from different Inconel products. The Inconel 625 Pipes and Tubes can withstand in a highly corrosive environment, and its structure gives it excellent strength. Welded Inconel 625 pipes and tubes can be utilized for the thermal process, aerospace, pollution control, power generation, and many more. Inconel 625 Pipes and Tubes are suitable to prefer for sour gas pipelines, power plants, superheating tubing systems, seawater heat exchangers, etc.
N06600 alloy is a Ni-Cr alloy that was developed and applied very early. It is widely used in various industries because of its corrosion resistance, heat resistance, curing resistance and good workmanship. It has good corrosion resistance in fresh water and fluctuating sea water. Corrosion spots may occur in still sea water. It has high corrosion resistance to various alkaline solutions and most organic acids and compounds, and is not prone to stress corrosion cracks. , but stress corrosion cracking is prone to occur under high concentration caustic alkali or high temperature Hg conditions.

GNEE Group Factory Environment

inconel Mirror polished tube factory

inconel polished tube

GNEE Group Product Delivery

inconel polished tube

inconel polished tube

Customer Case

customer visit

UNS n06625 n06600 inconel ss Pipe price

UNS n06625 n06600 alloy Pipe for sale

FAQ

 

 

 

Q: What is your delivery time?
A: Our delivery time is about one week, based on the number of customers.

Q: Can you send samples?
A: Of course, we can send samples to all over the world, our samples are free, but customers need to bear the express cost.

Q: What shipping ports are there?
A: Generally, we ship from Tianjin Port, you can choose other ports according to your needs.

Q: Can I get a sample before ordering?
A: Yes, of course. Usually our samples are free. We can produce according to your samples or technical drawings.

Q: About the product price of UNS n06625 n06600 inconel Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Contact Us

 

Address

No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China

 

Phone

+86-15824687445

 

Email

ss@gneesteel.com

 

Skype

mmkelly1314

 

Whatsapp/Wechat

+86 15824687445

 

Hot Tags: uns n06625 n06600 inconel pipe, China uns n06625 n06600 inconel pipe suppliers, inconel alloy structural parts, inconel alloy capacitor parts, inconel alloy reaction injection molding process, inconel alloy seamless piping, inconel alloy instrumentation parts, inconel alloy crankshaft parts

Send Inquiry

whatsapp

Phone

E-mail

Inquiry