Nickel Alloy 600 Stainless Steel Plate
GNEE Group offers Nickel Alloy Inconel 600 in a variety of forms, including:
Bars
Wires
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of nickel alloy 600 stainless steel plate in China. If you're going to wholesale high quality nickel alloy 600 stainless steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Nickel Alloy 600 Stainless Steel Plate introduce
Thickness: 0.3mm to 50mm
Width: 1000mm to 2000mm
Length: Custom lengths up to 6000mm
Surface Finish: 2B, BA, No. 4, HL, and more
Standards: ASTM B168, ASME SB168, AMS 5540
Nickel Alloy 600 Stainless Steel Plate


Inconel 600 Plates are a corrosion-resistant alloy known for its excellent resistance to oxidation and high-temperature strength. It is a nickel-chromium-based superalloy with good formability, weldability, and fabricability. Additionally, Inconel 600 exhibits superior resistance to chloride stress corrosion cracking, very low thermal expansion rate and outstanding thermal fatigue strength. It is often used in aircraft engine components and petrochemical equipment applications.
Specifications of Inconel 600 Sheet / Plate / Coil
| Product Type | Thickness (mm) | Width (mm) | Length (mm) | Surface Finish | Standards |
|---|---|---|---|---|---|
| Sheet | 0.3 – 6.0 | 1000 – 2000 | Up to 6000 | 2B, BA, No. 4, HL | ASTM B168, ASME SB168, AMS 5540 |
| Plate | 6.0 – 50 | 1000 – 2000 | Custom Lengths | No. 1, No. 2D | ASTM B168, ASME SB168, AMS 5540 |
| Coil | 0.3 – 6.0 | 1000 – 1500 | Coil Form | 2B, BA, No. 4 | ASTM B168, ASME SB168, AMS 5540 |
Specification of Inconel 600 Sheet
| Specification | Inconel 600 Plate And Sheet |
|---|---|
| Mechanical Properties Of Tensile | 40000 psi |
| Plate Length | Up to 240 Inches |
| Form | Blank (Circle)/ Ring (Flange)/ Plain Sheet/ Strip/ Flats/ Coils/ Foils/ Rolls |
| Most Selling Type Of | Rolling Sheet/ Rolling Plate/ Flat Shim/ Flat Sheet/ Shim Sheet/ descaled/ tread plate/ Checker Plate, Plate/ Sheet/ Coils/ Foils/ Strip/ Flats/ Clad Plate/ Plain Sheet/ Rolls/ Blank (Circle)/ sheared/ annealed/ soft annealed |
| Plate Width | 36 to 60 Inches |
| Thickness | 0.063 to 0.375 Inches |
| Standard Dimensions Of | EN ISO 18286/ ASME IID/ ASTM A 959/ ASTM A 480 |
| UNS Number Of Alloy 600 Plate | UNS N06600 |
| Chemical Composition | UNS N06600 Sheet : Copper (69.5%)/ Nickel (30.0%)/ Iron (0.5%) |
Mechanical Properties
| Typical Values at 68°F (20°C) | ||||
|---|---|---|---|---|
| Yield Strength 0.2% Offset |
Ultimate Tensile Strength (min) |
Elongation in 2" |
||
| psi | (MPa) | psi | (MPa) | % |
| 35,000 | (240) | 80,000 | (550) | 30 |
Chemical Analysis of Inconel Alloy 600
Weight % (all values are maximum unless a range is otherwise indicated)
| Nickel (plus Cobalt) | 72.0 min. | Manganese | 1.00 |
| Chromium | 14.0 min.-17.0 max. | Sulfur | 0.015 |
| Iron | 6.0 min.-10.0 max. | Silicon | 0.50 |
| Carbon | 0.15 | Copper | 0.50 |
GNEE Group Product Packaging
Nickel Alloy 600 Stainless Steel Plate

GNEE Group Factory Environment
Nickel Alloy 600 Stainless Steel Plate

FAQ
Q:Can we visit your factory ?
A:Warmly welcome once we have your schedule we will pick you up .
Q: Do you have quality control?
A: Yes, we have gained BV, SGS authentication.
Q: Can you arrange the shipment?
A: Sure, we have permanent freight forwarder who can gain the best price from most ship company and offer professional service.
Hot Tags: nickel alloy 600 stainless steel plate, China nickel alloy 600 stainless steel plate suppliers, inconel alloy combustion chamber parts, alloy inconel piping, inconel alloy plug fittings, inconel alloy demultiplexer parts, Inconel Alloy 625 693, Inconel Alloy 625 Pipe Fittings