Inconel X-750 Brushed Finish Plate
video

Inconel X-750 Brushed Finish Plate

Name:Nickel Alloy X-750 Plate
Length:1-6m or as Customer's Requirement
Size:6mm~150mm
Thickness:0.8~8.0mm
Certificate:ISO9001 RoHS
Service:OEM /ODM
Processing Service:Bending, Welding, Decoiling, Punching, Cutting
Inconel:600/601/625/718/750/X-750/800
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel x-750 brushed finish plate in China. If you're going to wholesale high quality inconel x-750 brushed finish plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

‌Inconel X-750 brushed veneer is a high-performance decorative material made of Inconel X-750 alloy with a brushed surface. ‌

 

The brushed treatment of Inconel X-750 alloy plate gives the panel surface a delicate texture, which is not only beautiful but also enhances the panel's wear resistance and scratch resistance. ‌

 

Inconel X-750 2b Finish Plate is widely used in aerospace, energy and chemical, marine engineering and other fields, especially in situations where it needs to withstand high temperature, high pressure and corrosive environment.

Specifications of Inconel X-750 Plasma Cutting Plate
Outer Diameter 6-2500mm, (3/8"-100")
Thickness 0.3-150mm,(SCH10-XXS)
Length 2000mm, 2500mm, 3000mm, 5800mm, 6000mm,12000mm,etc
Standard ASTM,JIS, AISI, GB, DIN, EN
Application It is widely used in high-temperature and electric industry, medical devices, construction, chemistry, food industry, agriculture, and ship components.
It also applies to food and beverage packaging, kitchen supplies, trains, aircraft, conveyor belts, vehicles, bolts, nuts, springs, and screen mesh etc.
Certification ISO, SGS
Technique Cold Rolled Hot Rolled Cold Drawn
Inconel X-750  Thick Nickel Alloy Sheet

Inconel X-750  Thick Nickel Alloy Sheet

 

Why choosing GNEE

GNEE has several advanced production lines, including a 3300mm wide hot rolling production line and a 1580mm cold rolling production line; it has also introduced a number of key equipment, including two new 12-ton American Consac vacuum induction furnaces, two 12-ton German ALD vacuum consumable furnaces, and 10 electroslag remelting equipment with capacities ranging from 5 to 25 tons.

please contact us for a quote! ss@gneesteel.com

Industry-leading inconel alloy production testing

Industry-Leading Inconel Alloy Production Testing

inconel X-750 suppliers

​​Inconel X-750 Suppliers

Nickel Alloy X-750 PACKAGING AND SHIPPING

Nickel Alloy X-750 PACKAGING AND SHIPPING

FAQ

1.Q.How can I trust you?
A. We think honesty is the core of our company, you can come to know it personally so that you can check our credit.

2.Q.Can your products be customized?
A.Yes, we can produce and process according to your requirements.

3.Q. Do you have a quality control system?
A.Yes, we have our own quality control laboratory.

Hot Tags: inconel x-750 brushed finish plate, China inconel x-750 brushed finish plate suppliers, 706 602ca Inconel Alloy Pipe, inconel alloy integrated circuit parts, Inconel UNS N06625 Welded Pipe, inconel alloy resonator parts, inconel alloy exhaust system parts, inconel alloy extrusion molding process

Send Inquiry

whatsapp

Phone

E-mail

Inquiry