UNS N07750 Plate
Product Introduction
UNS N07750 plate is a corrosion-resistant, high strength precipitation-hardenable nickel-chromium super-alloy plate. It provides high corrosion and oxidation resistance and maintains its strength at temperatures from cryogenic to 1300°F. When heat-treated, X-750 plate exhibits good strength up to 1800°F. It is easy to form and weld, making it an ideal alloy plate material for structural and high wear applications.
Chemical Properties:
| Chromium (%) | 14.0 to 17.0 |
| Nickel + Cobalt (%) | 70.00 Minimum |
| Iron (%) | 5.0 to 9.0 |
| Aluminum (%) | 0.40 to 1.00 |
| Titanium (%) | 2.25 to 2.75 |
| Manganese (%) | 1.00 Maximum |
| Niobium + Tantalum (%) | 0.70 to 1.20 |
| Silicon (%) | 0.50 Maximum |
| Copper (%) | 0.50 Maximum |
| Sulfur (%) | 0.01 Maximum |
| Cobalt (%) | 1.00 Maximum |
| Carbon (%) | 0.08 Maximum |
Mechanical Properties:
| Tensile Strength | MPa | 1250 |
| Ksi | 181000 | |
| Yield Strength | MPa | 850 |
| Ksi | 123000 | |
| Elongation | % | 30 |

UNS N07750 Inconel X-750 Plate Process Performance And Requirements:
Inconel X-750 alloy has good process performance, but the following factors need to be considered during processing and forming:
Heat treatment:
Inconel X-750 requires heat treatment to obtain the best mechanical properties and corrosion resistance. The heat treatment conditions can be adjusted according to the required performance.
Work hardening:
Inconel X-750 can be cold-processed to obtain higher strength, but attention should be paid to the brittleness of the material and excessive cold processing should be avoided.
Cutting:
When cutting Inconel X-750, tools with sufficient hardness and toughness should be used, and proper cooling and lubrication should be maintained.
Welding:
Inconel X-750 has good welding performance, but appropriate welding materials and processes need to be selected to avoid problems such as weld cracking.
Surface treatment:
The surface of Inconel X-750 usually needs pickling and descaling to ensure its excellent corrosion resistance.