Inconel Alloy X750 Round Bars
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel alloy x750 round bars in China. If you're going to wholesale high quality inconel alloy x750 round bars made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Product Introduction
GNEE STEEL GROUP stands out in the metal industry as a trusted inconel x750 round bar supplier and stockist. we offer them in various sizes, ranging from the smallest 0.5mm to as big as 500mm, with lengths up to 6 meters. For those seeking alloy x750 rods, we pride ourselves on providing top-notch round bar products at affordable rates.
We maintain Inconel X750 Round Bars stock in different diameters, lengths, and finishes. Our products are made with the highest quality standards and are tested for durability, strength, and flawless finish.
We are an ISO 14001: 2015 and 9001:2015 certified company that ensures the ASTM B637 bar we offer are manufactured through precise technology. We offer clear and competitive pricing that provides the best value for your investment without sacrificing quality. For an exact price, do not be afraid to call us directly.
We are a leading Inconel X750 Round Bars stockist worldwide because our reputation for providing the best in class products. For any metal requirements, contact us today and we shall be pleased to help.

What are Inconel X750 Round Bars?
Inconel X750 Round Bars are high-performance metal bars made from a nickel-chromium alloy. Known for their exceptional strength, heat resistance, and corrosion resilience, these UNS N07750 bars find applications in demanding environments like aerospace and high-temperature settings.
Packaging of ASTM B637 UNS N07750 Round Bars
Securely packaged to prevent damage during transit
Quality-tested packaging materials to ensure product integrity.
Each bar is individually wrapped for added protection
Clearly labeled for easy identification
INCONEL X750 ROUND BAR STOCK AND SUPPLY RANGE

INCONEL X750 ROUND BAR SPECIFICATION
| Standards | ASTM B637, ASME SB 637, AMS 5669, AMS 5667, AMS 5668 |
|---|---|
| Specifications | DIN, EN, ASTM, JIS, ASME, BS, AISI |
| X750 Round Bars size | Diameter: 3-~800mm |
| Inconel X750 Flat Bars size | Thickness: 2 -100mm |
| Width: 10 to 500mm | |
| Inconel X750 Angle Bars size | 3mm*20mm*20mm~12mm*100mm*100mm |
| Inconel X750 Channel Bars | 80 x 40mm to 150 x 75mm section; 5.0 to 6.0mm thickness |
| Alloy X750 Rectangular Bars Section | 3.0 to 12.0mm thickness |
| Inconel X750 Billet Size | 1/2 to 495mm Diameter |
| Inconel X750 Rectangle Bar Size | 33 x 30mm to 295 x 1066mm |