Inconel Alloy 713C Seamless Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel alloy 713c seamless pipe in China. If you're going to wholesale high quality inconel alloy 713c seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Inconel 713C Capillary Tube is generally referred to as a narrow tube that has a constant diameter.
Capillary tubes are used in various applications where precise control of fluid flow is required. Capillary Tubes are available in exact cut-to lengths and are also extremely operational in a wide range of high temperatures. These Capillary Tubes can be made in personalized thicknesses and sizes as per the specific requirements of our clients.
Inconel 713C is a γ' phase precipitation-strengthened nickel-based casting superalloy. It has good creep strength, thermal fatigue performance, and oxidation resistance below 900℃. The alloy composition is relatively simple, does not contain cobalt, has a low density, and is usually used in the cast state. The use of hot isostatic pressing (HIP) treatment and subsequent heat treatment can improve the plasticity and fatigue properties, and can also restore the structure and performance of parts that have experienced structural degradation and reduced performance after long-term use. A small amount of σ phase will precipitate during long-term aging at 800℃, but it will have no significant impact on performance.
Inconel 713C Capillary Tube Specification
|
Grade |
Inconel 713C |
|
Shape |
Capillary Tube |
|
Density (g/cm3) |
7.913 |
|
Tensile Strength |
110 psi |
|
Size |
Seamless pipe: OD:6-630, WT:0.3-100mm Capillary tube: OD:0.2-6, WT:0.02-2mm |
Chemical Composition (%)
|
C |
Cr |
Ni |
Mo |
Al |
Ti |
Fe |
Nb |
|
0. 08~0. 16 |
11.5~13.5 |
Bal. |
3.8~4.8 |
5. 5~6. 4 |
0.5~l.0 |
≤1.0 |
1.8~2.5 |
|
B |
Zr |
Mn |
Si |
P |
S |
Pb |
Bi |
|
0. 008~0. 020 |
0.6~0. 15 |
≤0.5 |
≤0.5 |
≤0.015 |
≤0.01 |
≤0. 001 |
≤0.0001 |