Inconel Alloy 718 Polishing Plate
GNEE Group offers Inconel Alloy 718 Polishing Plate in a variety of forms, including:
Bars
Wires
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel alloy 718 polishing plate in China. If you're going to wholesale high quality inconel alloy 718 polishing plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Inconel Alloy 718 Polishing Plate Introduction
Gnee Steel Group are known as the best manufacturer, supplier and stockiest of the high quality of Inconel 718 Sheet & Plate all across the globe. The product to the buyers is offered to the buyers at the comprehensive range so that it can be easily used. It can be acquired at different sizes, length, wall thickness, dimensions, and specifications. Also, the industry is offering the same to all their valuable buyers at customized specification as per their needs and prerequisites. With respect to several raw material quality standards, it is provided to the buyers at reasonable rates. The industry is also good at offering value-added and sales after services to buyers.
Inconel 718 Plate Specification
Alloy 718 Sheet, Plate, & Strip Related Specifications
AMS 5596
AMS 5597
UNS N07718
ASTM B670

UNS N07718 Sheet Thickness
| SIZES (INCH) | SIZES (mm) |
|---|---|
| .125" | 3.18mm |
| .134" | 3.40mm |
| .156" | 3.96mm |
| .187" | 4.75mm |
| .250" | 6.35mm |
| .312" | 7.92mm |
| .375" | 9.53mm |
| .500" | 12.7mm |
| .625" | 15.9mm |
| .750" | 19.1mm |
| .875" | 22.2mm |
| 1" | 25.4mm |
| 1.125" | 28.6mm |
| 1.250" | 31.8mm |
| 1.500" | 38.1mm |
| 1.750" | 44.5mm |
| 2" | 50.8mm |
| 2.500" | 63.5mm |
| 3" | 76.2mm |
Inconel 718 (Alloy 718, UNS N07718) Plate/Sheet Specifications:
Metal Type: UNS N07718
Standard: ASTM B670, AMS 5596, AMS 5597, PWA 1033, GE B50TF15, ASTM B670, ASTM B637
Chemical Composition, %
| Ni | Fe | Mo | Mn | Si | Cr | C | |
| Max | 55.0 | Bal | 3.30 | 0.35 | 0.35 | 21.0 | 0.08 |
| Min | 50.0 | 2.80 | 17.0 |
GNEE Group 718 Polishing PlateTesting
Material testing is done-
Prior to the shipping of the product, various effective tests are conducted over the Inconel 718 Sheet & Plate. The test performed is including flattening test, PMI test, macro test, hardness test, IGC test, micro test, flaring tests, chemical test, pitting resistance test and mechanical test. All these tests are assuring in bringing out error free quality of the product.

The mill test certifications-
Now the mill test certifications are provided to all the esteem patrons dealing with the industry as per EN 10204/3.1B. The test certifications are too provided to the buyers that include third-party test report, lab test certificate, radiography test report and buyers report.


GNEE Group Factory Environment
Inconel 718 Polishing Mirror Plate factory

FAQ
Q: How long is your delivery time?
A: Generally it is 2-5 days if the goods are in stock or it will need 7-20 days if the goods need to be customized.
Q: Do you provide samples Is it free or extra?
A: Yes, we could offer free samples.
Q: What is your terms of payment?
A: 20% Prepayment and balance see B/L copy or 100%LC at sight.
Hot Tags: Inconel Alloy 718 Polishing Plate, China Inconel Alloy 718 Polishing Plate suppliers, inconel alloy heating system parts, inconel alloy filter parts, inconel alloy timer parts, inconel alloy mixer parts, inconel alloy shaft parts, inconel alloy transfer molding process