INCONEL alloy 686 (UNS N06686/WNr. 2.4606) is a single-phase, austenitic Ni-Cr-Mo-W alloy offering outstanding corrosion-resistance in a range of severe environments. Its high Ni and Mo provide good resistance in reducing condi- tions, and high Cr offers resistance to oxidizing media.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel alloy 686 pipe in China. If you're going to wholesale high quality inconel alloy 686 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel Alloy 686 pipe refers to a high-performance nickel-chromium alloy pipe, which is widely used in many industrial fields for its excellent high temperature resistance and corrosion resistance. The following will delve into the characteristics, applications and advantages of choosing Inconel Alloy 686 pipe:

basic introduction
Chemical composition and improvement: Inconel 686 is based on the C276 alloy. By increasing the chromium content and reducing the proportion of iron, this alloy not only inherits the resistance of the 276 alloy to reducing media, but also enhances the resistance of the C22 alloy. Resistance to oxidizing media.
Low impurity design: The alloy adopts low carbon, low silicon, and low iron design. This treatment significantly improves the material's structure and performance stability.
Physical and mechanical properties
High temperature performance: Inconel Alloy 686 can be used at temperatures up to 982°C, maintaining its excellent mechanical strength and oxidation resistance, making it very suitable for use in high temperature environments.
Machining: Although Inconel Alloy 686 is a difficult-to-machine material, it can be machined and formed efficiently by optimizing processing parameters and selecting appropriate tools.
Corrosion resistance
Broad corrosion resistance: Due to its unique chemical composition, Inconel Alloy 686 shows excellent resistance to a variety of acid and alkali environments, including sulfuric acid, phosphoric acid and hydrofluoric acid.
Specific Environmental Applications: This alloy is particularly suitable for applications where chloride stress corrosion cracking and pitting corrosion are issues, such as in marine and offshore environments.

Chemical composition

Item

Ni

C

Si

Mn

Cr

Mo

W

Ti

Fe

S

P

Min

Balance

     

19.0

15.0

3.0

0.02

     
Max

0.010

0.08

0.75

23.0

17.0

4.4

0.25

2.0

0.02

0.02

 

Specifications

Inconel 686 UNS NO6686 2.4606 Similar Grade
UNS W.Nr ASME EN
N06686 2.4606 B564 Inconel 686

 

Inconel Alloy 686 pipeInconel Alloy 686 pipeInconel Alloy 686 pipe

Hot Tags: inconel alloy 686 pipe, China inconel alloy 686 pipe suppliers, Inconel 617 Super Stainless Pipe, inconel alloy cap fittings, 706 602ca Inconel Alloy Pipe, inconel alloy gear parts, inconel alloy modulator parts, Inconel Seamless Pipe

Send Inquiry

whatsapp

Phone

E-mail

Inquiry