Inconel Alloy 600 Flanges
GNEE Group offers Nickel Alloy Inconel 600 in a variety of forms, including:
Bars
Wires
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel alloy 600 flanges in China. If you're going to wholesale high quality inconel alloy 600 flanges made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Inconel Alloy 600 Flanges Introduction
Inconel Alloy 600 Flanges


Inconel 600 flanges Corrosion Resistance
ANSI B16.5 Alloy 600 flanges, also known as weld neck flanges, are highly corrosion resistant due to their ability to form a strong oxide layer. This oxide layer helps protect them from oxidation and other corrosive chemicals. Inconel 600 is ideal for applications with high temperatures, such as in chemical process industries, nuclear power plants, and petrochemical refineries. Additionally, the weld neck design of these flanges allows for easy connection of pipes, making it a popular choice among industrial users.
Alloy 600 flanges Heat Treatment
Inconel 600 Flanges are typically heat treated in four steps. First, the parts are normalized for grain and microstructural refinement. Second, alloy 6000 flanges are solution annealed to improve formability and remove cold work from forming operations. Third, the components are aged to obtain desired mechanical properties. Finally, all components must undergo a stress relief process to ensure dimensional stability during application or service. By following these steps, optimal performance can be achieved from Inconel 600 flanges in demanding applications.
600 inconel flanges Chemical Features
ASTM B564 Inconel 600 Alloy flanges are made from an alloy of nickel and chromium, which offers good corrosion resistance, high strength, and excellent heat resistance. This material has various weld neck flange types, including lap joint, spectacle blind, orifice plate, gasket rings, reducer/increaser, etc., for pipe connection purposes in various industries. It is also non-magnetic and offers superior mechanical properties at temperatures up to 1200°F (649°C). Connections made with Inconel 600 Weldneck flanges have exceptional leak tightness that can withstand severe thermal cycling applications due to their low coefficient of thermal expansion and oxidation-resistant properties.
UNS N06600 flanges Uses
Inconel 600 flange is a weld neck flange used in various piping applications. It is made from an alloy of nickel and chromium and is known for its ability to withstand extremely high temperatures, corrosion resistance, and strength. The weld neck flange design allows the connection points to rotate easily to be aligned with other components without experiencing any deformation or damage.
Types of Inconel 600 Flange:
High-quality flange made from Inconel 600, a nickel-chromium alloy. Offers excellent resistance to high temperatures, corrosion, and oxidation. Suitable for various industrial applications. The Inconel 600 Flange comes in various types, including the Weldneck Flange. It provides a strong and leak-resistant connection for welding applications.
Inconel Alloy 600 Socket Weld Flanges Specification
Specifications ASTM B564 / ASME SB564
Dimensions ANSI/ASME B16.5, B 16.47 Series A & B, B16.48, BS4504, BS 10, EN-1092, DIN, etc.
Standard ANSI Flanges, ASME Flanges, BS Flanges, DIN Flanges, EN Flanges, etc.
Size 1/2″NB TO 60″NB
Class / Pressure 150#, 300#, 600#, 900#, 1500#, 2500#, PN6, PN10, PN16, PN25, PN40, PN64 etc.
Flange Face Type Flate Face (FF), Raised Face (RF), Ring Type Joint (RTJ)
Grade 600 UNS (N06600), DIN (2.4816)

Inconel 600 Flanges Equivalent Indian Standard
| STANDARD | UNS | WNR. | AFNOR | EN | JIS | BS | GOST | OR |
| Alloy 600 | N06600 | 2.4816 | NC15FE11M | NiCr15Fe | NCF 600 | NA 13 | МНЖМц 28-2,5-1,5 | ЭИ868 |
ASTM B564 Inconel Alloy 600 Forged Flanges Chemical Composition
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr |
| Inconel 600 | 0.15 max | 1.00 max | 0.50 max | 0.015 max | 0.50 max | 6.00 – 10.00 | 72.00 min | 14.00 – 17.00 |
600 Inconel ASME SB564 Threaded / Screwed Flanges Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.47 g/cm3 | 1413 °C (2580 °F) | 655 MPa, 95000 psi | 310 MPa, 45000 psi | 45 % |
GNEE Group Factory Environment
Inconel Alloy 600 Flanges

GNEE Group Product Delivery
600 metal alloy delivery

FAQ
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: What is your terms of payment?
A: 20% Prepayment and balance see B/L copy or 100%LC at sight.
Hot Tags: inconel alloy 600 flanges, China inconel alloy 600 flanges suppliers, inconel alloy gear parts, inconel alloy reaction injection molding process, inconel seamless Piping, inconel alloy extrusion molding process, inconel alloy antenna parts, inconel alloy steel piping
Previous
Inconel 600 Metal PlatesYou Might Also Like
Send Inquiry