Inconel 617
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 617 in China. If you're going to wholesale high quality inconel 617 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Overview
As a leading supplier & manufacturer in China, AEETHER supply cost-effective Inconel 617 Products.
INCONEL® alloy 617 (UNS N06617 / W.Nr. 2.4663a) is a solid-solution, strengthened, nickel-chromium-cobalt-molybdenum alloy with an exceptional combination of high-temperature strength and oxidation resistance. The alloy also has excellent resistance to a wide range of corrosive environments, and it is readily formed and welded by conventional techniques.
The high nickel and chromium contents make the alloy resistant to a variety of both reducing and oxidizing media. The aluminum, in conjunction with the chromium, provides oxidation resistance at high temperatures. Solid-solution strengthening is imparted by the cobalt and molybdenum.
The combination of high strength and oxidation resistance at temperatures over 1800°F (980°C) makes INCONEL alloy 617 an attractive material for such components as ducting, combustion cans, and transition liners in both aircraft and land-based gas turbines. Because of its resistance to high-temperature corrosion, the alloy is used for catalyst-grid supports in the production of nitric acid, for heat-treating baskets, and for reduction boats in the refining of molybdenum. INCONEL alloy 617 also offers attractive properties for components of power-generating plants, both fossilfueled and nuclear.
Property values are given in both United States customary units and the International System of Units (SI). The SI unit of stress is the pascal (Pa), which is equivalent to newton per square metre. The approximate relationship between the pascal and the pound per square inch (psi) is 1 Pa = 0.0001450 psi, or 1 psi = 6895 Pa.
Mechanical Properties
INCONEL alloy 617 has high mechanical properties over a broad range of temperatures. One of the alloy's outstanding characteristics is the strength level it maintains at elevated temperatures. The resistance of the alloy to high-temperature corrosion enhances the usefulness of its strength.
Corrosion Resistance
The composition of INCONEL alloy 617 includes substantial amounts of nickel, chromium, and aluminum for a high degree of resistance to oxidation and carburization at high temperatures. Those elements, along with the molybdenum content, also enable the alloy to withstand many wet corrosive environments.
More +
Main Standards
ASTM B167
Seamless Pipe & Tube
ASTM B829
Seamless Pipe & Tube
ASTM B546
Electric Fusion-Welded Pipe
ASTM B366
Welded Fittings
ASTM B166
Rod, Bar and Wire
ASTM B564
Forgings
ASTM B168
Plate, Sheet and Strip
SAE AMS 5887
Rod, Bar and Wire
SAE AMS 5888
Plate, Sheet & Strip
SAE AMS 5889
Plate, Sheet & Strip
AWS A5.14 ERNiCrCoMo-1
Filler Metal
AWS A5.11 ENiCrCoMo-1
Welding Electrode
Chemical Composition
Data Sheet
Physical Properties
| Density | g/cm3 | 8.36 | |
|---|---|---|---|
| lb/in.3 | 0.302 | ||
| Melting Range | °F | 2430 - 2510 | |
| °C | 1332 - 1380 | ||
| Specific Heat at 78°F (26°C) | Btu/lb-°F | 0.100 | |
| J/kg-°C | 419 | ||
| Electrical Resistivity at 78°F (26°C) | ohm-circ mil/ft | 736 | |
| μΩ-m | 1.22 | ||
Mechanical Properties
| Product Form | Product Method | Yield Strength (0.2% Offset) |
Tensile Strength | Elongation, % |
Reduction Of Area, % |
Hardness, BHN |
||
|---|---|---|---|---|---|---|---|---|
| ksi | MPa | ksi | MPa | |||||
| Plate | Hot Rolling | 46.7 | 322 | 106.5 | 734 | 62 | 56 | 172 |
| Bar | Hot Rolling | 46.1 | 318 | 111.5 | 769 | 56 | 50 | 181 |
| Tubing | Cold Drawing | 55.6 | 383 | 110 | 758 | 56 | - | 193 |
| Sheet or Strip | Cold Rolling | 50.9 | 351 | 109.5 | 755 | 58 | - | 173 |
More +
FAQ
Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, Kazakhstan, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.




Hot Tags: inconel 617, China inconel 617 suppliers, nickel-based, inconel alloy crankshaft parts, inconel alloy inductor parts, inconel alloy reducer fittings, inconel alloy ss tubing, inconel alloy connecting rod parts
Previous
Inconel 625 alloy plateNext
Inconel 603XLYou Might Also Like
Send Inquiry