Inconel 713C Nickel-Based Alloy Round Bar
Process Method: VIM (Vacuum Induction Melting) / VIM+ESR
Diameter Range: Φ4mm – Φ600mm / Custom Sizes
Key Certification: ISO 9001, EN 10204 3.1 MTC, SGS/TÜV Third-Party Test Available
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 713c nickel-based alloy round bar in China. If you're going to wholesale high quality inconel 713c nickel-based alloy round bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
What Is Inconel 713C Round Bar?

Inconel 713C (UNS N07713) is a precipitation-hardening nickel-based casting superalloy.
Renowned for its exceptional high-temperature strength, oxidation resistance, and superior thermal fatigue performance, it is widely utilized in extreme high-temperature and high-pressure applications ranging from 1000°F to 1700°F (approx. 538°C to 927°C).
Inconel 713C Major Equivalent Grades & Standards
| Standard / System | Designation / Grade |
| UNS Number | UNS N07713 |
| DIN / EN Standard | W.Nr. 2.4671 |
| Chinese Standard (GB) | K418 / K418B / GH413 |
| Common Trade Names | IN-713C, Alloy 713C, Cast Inconel 713C |
Inconel 713C Quick Reference Table
- Form / Condition: As-Cast Master Alloy Bars (Remelt Stock) / Investment Casting Raw Material / Machined Bars
- Process Method: VIM (Vacuum Induction Melting) / VIM+ESR
- Diameter Range: Φ4mm – Φ600mm / Custom Sizes
- Key Certification: ISO 9001, EN 10204 3.1 MTC, SGS/TÜV Third-Party Test Available
Inconel 713C Round Bar Chemical Compositons:
|
Alloy |
% |
Ni |
Cr |
Fe |
Mn |
Si |
Mo |
Zr |
Ti |
Cu |
Co |
Al |
C |
S |
|
713C |
Min. |
Bal |
12.0 |
- |
- |
- |
3.8 |
0.05 |
0.5 |
- |
1.8 |
5.5 |
- |
- |
|
Max. |
14.0 |
2.5 |
0.25 |
0.5 |
5.2 |
0.15 |
1.0 |
0.5 |
2.8 |
6.5 |
0.20 |
0.015 |
Inconl 713C Round Bar Physical properties
|
Density |
7.913 g/cm³ |
|
Melting point |
1260℃-1288℃ |
Inconel 713C Heat Treatment & Delivery Condition
Inconel 713C is a precipitation-hardening nickel superalloy. Its standard heat treatment includes solution treatment followed by ageing precipitation to boost high-temperature rupture strength. Round bars are commonly supplied in hot-forged, rough-machined or solution-treated states. Ageing is usually performed by end users after component machining.
| Treatment / State | Temperature | Purpose |
|---|---|---|
| Solution Treatment | 1175–1205 °C, air cool | Dissolve alloy phases, prepare for ageing |
| Ageing Hardening | 645–665 °C, hold 16 h | Precipitate γ' phase for high-temperature strength |
| Delivery Condition | Hot forged / Solution treated | Supply for customer follow-up machining & ageing |
How Do Heat Treatment and Delivery Condition Affect Corrosion Resistance of Inconel 713C:
Inconel 713C's corrosion resistance is mainly governed by alloy composition, while heat treatment exerts secondary influence. Solution treatment produces a uniform matrix and stable passive film. Ageing forms γ′ precipitates; prolonged high-temperature ageing may create grain-boundary phases that slightly reduce local corrosion resistance. Hot-forged delivery without full solution treatment carries uneven microstructure and higher corrosion risk.

Inconel 713C Production Process
Inconel 713C is a precipitation-hardening nickel superalloy requiring vacuum melting to control gas content and impurity levels. The standard route uses VIM followed by VAR remelting to refine ingot microstructure. Subsequent homogenisation heating reduces segregation before hot working. Controlled forging or rolling shapes the ingot into round bar, with intermediate heat treatment to manage work hardening.
| Process Step | Core Operation | Process Purpose |
|---|---|---|
| VIM Vacuum Induction Melting | Melt raw alloy materials under vacuum | Reduce oxygen, nitrogen and volatile impurities |
| VAR Vacuum Arc Remelting | Re-melt VIM ingot in vacuum arc furnace | Improve microstructure uniformity, minimise segregation |
| Homogenization Heat Treatment | High-temperature long-duration soaking | Dissolve segregated phases from solidification |
| Hot Forging / Hot Rolling | Plastic forming within controlled temperature window | Convert ingot to semi-finished round bar |
| Finishing & Straightening | Centerless grinding, straightening | Achieve required diameter tolerance and straightness |
| Inspection & NDT | PMI, UT, hardness, tensile and metallurgy testing | Verify composition, mechanical properties and internal integrity |
Inconel 713C Machinability & Physical Machining Guidance
Inconel 713C exhibits high work-hardening tendency during machining, requiring rigid setups and sharp tooling. High-speed tungsten‑cobalt HSS or molybdenum‑tungsten‑vanadium cutting tools are recommended. Suitable cutting fluids include chlorinated/sulfurized fatty mineral oil, and soluble oil emulsion mixed at a 1:10 oil‑to‑water ratio.
For grinding, select medium‑soft vitrified‑bond alumina abrasives with an open structure. Clean grinding wheels using 1 lb sal soda diluted in 25 gal water, or chemically active grinding coolant. Maintain low cutting speeds and light depths of cut to avoid surface cold work.
| Machining Operation | Recommended Consumables & Parameters |
|---|---|
| Turning / Milling Tools | Tungsten‑cobalt HSS, Mo‑W‑V high-speed steel |
| Cutting Lubricant | Chlorinated sulfurized fatty oil; 1:10 soluble oil emulsion |
| Grinding Wheel | Al₂O₃, vitrified bond, medium-soft grade, open structure |
| Wheel Cleaning Coolant | 1 lb sal soda / 25 gal water or active grinding coolant |
Inconel 713C Weldability
Inconel 713C has limited weldability and is only suitable for low-restraint assemblies. Inco-Weld A electrode is the matching filler. Flash-butt welding is an acceptable joining method. It performs well in hydrogen-atmosphere brazing; electroplated contact surfaces paired with conventional high-temperature brazing alloys help produce sound joints. Avoid high-constraint welding to prevent cracking.
| Item | Guidance |
|---|---|
| Welding Restriction | Only low-restraint service conditions |
| Filler Metal | Inco-Weld A electrode |
| Welding Method | Flash-butt welding |
| Brazing Option | Hydrogen-atmosphere brazing, electroplated mating surfaces |
Inconel 713C Key Industrial Applications

Inconel 713C for Automotive & Marine Turbochargers
Serves as premium remelt stock for precision casting of turbocharger turbine wheels and nozzle vanes. Delivers exceptional creep resistance and thermal fatigue strength under extreme high-temperature exhaust environments.
Inconel 713C for Aerospace & Defense Engines
Engineered for turbine blades, vanes, and integral wheels in small gas turbine engines and APUs. Provides superior oxidation and corrosion resistance under operating temperatures up to 927°C (1700°F).


Inconel 713C for Industrial Gas Turbines & Energy
Applied in gas path components, high-temperature nozzles, and structural liners for industrial gas turbines. Resists high-temperature gas erosion and stress relaxation, ensuring long-term operational stability for energy equipment.
Inconel 713C for Hot-Working Tools & Fixtures
Ideal for manufacturing high-temperature heat treating fixtures, die inserts, and specialized heat-resistant components. Retains superior hot hardness and spallation resistance, significantly extending tooling service life under harsh cycles.

Real Project Case of Inconel 713C Round Bar
Project Background
This batch of Inconel 713LC round bar order totals approximately 18 tons. The client required two custom sizes: Φ100 mm × 700 mm and Φ555 mm × 80 mm. The material was intended for high-temperature hot-section components of industrial gas turbines, with full material traceability and third-party test certificates.
Order Challenges
The large-diameter short billet (Φ555 mm) demanded strict microstructure uniformity. Inconel 713LC is sensitive to segregation during melting and forming. We adopted VIM+VAR double melting and controlled forging parameters to avoid internal defects, and conducted UT and PMI inspection on every piece.
Our Solutions
We arranged dedicated melting and forging schedules, implemented full NDT inspection. Each bar was marked with heat number and dimension data, and delivered with EN 10204 3.1 certification to satisfy the client's quality audit for turbine component machining.
| Material | Specification |
|---|---|
| Inconel 713LC Round Bar | DIA 100 mm, L=700 mm |
| Inconel 713LC Round Bar | DIA 555 mm, L=80 mm |
Why Choose Gnee as Your Nickel-Based Alloy Supplier?
✅ Since 2008, we have exported alloy materials to clients across Asia, Europe and other regions globally
✅ Qualified with ISO, SGS and BV third-party certifications
✅ Complete inspection services: PMI, UT, eddy current testing and other quality checks
✅ Global stock of Inconel, Hastelloy, Incoloy and Monel tubes, plates & bars
✅ Custom machining: cutting, polishing, CNC processing and tailored packaging
✅ Stock items ship in 7–15 working days; custom orders 15–25 working days, with priority MRO scheduling
📦 Packaging and Shipping
Our nickel-based alloy products adopt industrial anti-corrosion packaging for overseas shipment:
- Heat-treated wooden pallets or solid export crates
- Multi-layer moisture-proof & rust-resistant wrapping
- Marked labels with heat number, material grade, standard and dimensions
- Global delivery options: sea freight, air freight and courier express


About Gnee Steel

Gnee Steel is a company specializing in the production of various nickel-based alloys, nickel 201, nickel202, hastelloy c-276, hastelloy c-22, hastelloy b, hastelloy c-4, Inconel alloy 600, Inconel 625, Inconel 718, Inconel x-750, incoloy alloy 800, incoloy 800H/HT, incoloy 825, monel alloy 400, monel k500 and high temperature alloy materials. It specializes in the production and sales of alloy materials. Gnee Steel's products are widely used in aerospace, chemical, electric power, automobile, nuclear energy and other fields, and can provide customized alloy material solutions according to customer needs. If you need to know the alloy material price consultation or provide customized alloy material solutions, you are welcome to contact us at any time to get a quote at ss@gneesteel.com
Hot Tags: inconel 713c nickel-based alloy round bar, China inconel 713c nickel-based alloy round bar suppliers, Inconel 602CA Capillary Tube, Inconel Alloy 706 Pipe, inconel alloy decoder parts, inconel alloy demodulator parts, inconel alloy flange fittings, inconel alloy structural parts
Previous