Inconel 693
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 693 in China. If you're going to wholesale high quality inconel 693 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Overview
As a leading supplier & manufacturer in China, AEETHER supply cost-effective Inconel 693 Products.
INCONEL alloy 693 (UNS N06693) is a new alloy from Special Metals which offers resistance to high temperature corrosion mechanisms not previously available from a nickel-based alloy. Of particular interest to the designer is the alloy's resistance to metal dusting. INCONEL® alloy 693 offers the best resistance to metal dusting in chemical and petrochemical processing environments of any conventional alloy currently manufactured. Alloy 693 typically contains 60.5% nickel, 29% chromium, and 3.1% aluminum. Like its predecessor, INCONEL alloy 690, the alloy's high chromium content gives it excellent resistance to oxidation and sulfidation. However, the addition of 3.1% aluminum to alloy 693 vastly improves resistance to other forms of high temperature corrosion as well. Alloy 693 is protected by U.S. Patent Number 4,882,125.
Corrosion Resistance
Alloy 693 offers superior resistance to metal dusting, a particularly aggressive form of carburization that can cause failure after very short exposures. Atmospheres containing reducing media (e.g. carbon monoxide and hydrogen) are known to induce metal dusting at elevated temperatures. Alloy 693 offers good resistance to sulfidation in both oxidizing and reducing environments containing sulfur. Also, the alloy performed well when exposed to oxide-rich media such as glass frit and fluxing compounds at temperatures up to 1100°C (2012°F).
Main Standards
ASTM B167
Seamless Pipe & Tube
ASTM B366
Welded Fittings
ASTM B166
Rod, Bar and Wire
ASTM B168
Plate, Sheet and Strip
ASTM B906
Plate, Sheet and Strip
AWS A5.14 ERNiCrFeAl-1
Filler Metal
Chemical Composition
Data Sheet
Physical Properties
| Density | g/cm3 | 7.77 | |
|---|---|---|---|
| lb/in.3 | 0.280 | ||
| Melting Range | °F | 2403 - 2493 | |
| °C | 1317 - 1367 | ||
| Electrical Resistivity | ohm-circ mil/ft | 702.7 | |
| μΩ-m | 1.168 | ||
Mechanical Properties
| Tensile strength, ksi (MPa) | 108.3 (746) |
|---|---|
| 0.2% Yield Strength, ksi (MPa) | 70.1 (483) |
| Elongation, % | 48.1 |
| Reduction of area, % | 58.7 |
| 2T side bend tests | No fissures |
FAQ
Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, Kazakhstan, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.