Inconel 601 Round Grind Bars
video

Inconel 601 Round Grind Bars

Inconel 601 Bar Specifications
Specifications: ASTM B166 / ASME SB166
Standards: ASTM, ASME and API
Range: 5mm to 500mm diameter
Length: 100mm to 6010mm
Surface treatment: bright, polished and blackened
Shapes: round, square, hexagonal (A/F), rectangular, wire (coil), wire mesh, billet, ingot, forging, etc.
601 Grade UNS (N06601), DIN (2.4851)

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 601 round grind bars in China. If you're going to wholesale high quality inconel 601 round grind bars made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel 601 Round Grind Bars introduce

alloy 601 Round Grind Bars

Inconel 601 Round Grind BarsInconel 601 Round Grind Bars

Gnee Steel alloy 601 rods are Manufactured in compliance with industry standards, specifically AMS 5715 and ASTM B166, they are available in various diameters and lengths, featuring shapes like circles, squares, and hexagons. The range spans from small 1/16″ diameter bars to larger 12″ diameter bars, ensuring a comprehensive selection to meet varied needs.

Inconel 601 is a standard engineering material that has excellent heat and corrosion resistance. It also has excellent machinability and metallurgical stability, making it ideal for critical applications. The company focuses on the production and supply of Inconel 601 round bars.

Made of nickel and chromium, Inconel 601 round bars have excellent heat and corrosion resistance. They can withstand temperatures up to 1250 degrees Celsius and are not easily deformed under pressure. Inconel 601 round bars are mainly available in two forms: hot rolled and cold rolled. Hot rolled Inconel 601 round bars have excellent dimensional accuracy and smooth surface.

Inconel 601 round bars are available in a variety of shapes, including hexagonal bars, flat bars, and threaded bars. It is also known as Inconel 601 triangular bars and is an important component for manufacturing products.

meatl 601 Round Grind Bars

Inconel 601 Round Grind Bars

The applications of Inconel N06601 round bars are diverse and occur in many industries. The alloy is suitable and useful for heat exchanger, combustion chambers, furnace components gas turbines chemical processing equipment. Inconel 601 rods are popular in the petrochemical and chemical processing industries for their high heat and corrosion resistance.

AMS 5715 round bars have many advantages and benefits, such as:

The alloy's great heat protection makes it perfect for uses where hot situations are common.

The ASTM B166 rod is strong and does not change or get damaged easily. This works well in rough conditions, too.

It can handle hot gases and liquids well because it has great corrosion resistance.

UNS N06601 round bars also don't expand much when it gets hot. This makes them good for high-temp jobs where keeping the same size is important.

AMS 5715 Round Bar

Length: 0.5 - 6.0 meter

Diameter: 3 - 600 mm

Surface: Black, Pickled, Bright, Polished,

INCONEL 601 ROUND BAR EQUIVALENT GRADES

STANDARD WERKSTOFF NR. UNS GOST AFNOR JIS BS EN OR
Inconel 601 2.4851 N06601 XH60BT NC23FeA NCF 601 NA 49 NiCr23Fe ЭИ868

INCONEL 601 ROUND BAR CHEMICAL COMPOSITION

Grade Ni Cr Fe C Mn S Si Cu
Inconel 601 58.0 – 63.0 21.0 -25.0 Balance 0.10 max 1.0 max 0.015 max 0.5 max 1.0 max

GNEE Group Factory Environment

601 Grind Bars

Inconel 601 Round Grind Bars

GNEE Group Product Packaging

601 Round Grind Bars

Inconel 601 Round Grind Bars

FAQ

Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.
Q: Will the Test Certificate meet EN10204 3.1/3.2?
A: We will provide Original Mill Test Certificate certified to EN10204 3.1/3.2 for products in stock or further processing needed.
Q: How long is your delivery time?
A: Generally it is 2-5 days if the goods are in stock or it will need 7-20 days if the goods need to be customized.

Hot Tags: Inconel 601 Round Grind Bars, China Inconel 601 Round Grind Bars suppliers, inconel alloy camshaft parts, inconel alloy detector parts, Inconel 625 Stainless Steel Coil, nickel-based, inconel alloy integrated circuit parts, Inconel X 750

Send Inquiry

whatsapp

Phone

E-mail

Inquiry