High Strength Structural Steel Plate EN10149 S700MC
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of high strength structural steel plate en10149 s700mc in China. If you're going to wholesale high quality high strength structural steel plate en10149 s700mc made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Hot Rolled BS700MCK2 High Strength Structural Steel Plate EN10149 S700MC 4*1500*10000mm
Description
| Application: | Container Plate | Technique: | S355J2+N |
|---|---|---|---|
| Standard: | ASTM,AISI,JIS,DIN | Length: | 1000-12000mm |
| Type: | Steel Plate | Width: | 600mm-1250mm,2000-2300mm |
| Special Use: | High-strength Steel Plate | Thickness: | 6-100mm |
| Shape: | High Quality S355J2+N Hot Rolled Carbon Steel Plate | Price Term: | CIF CFR FOB EX-WORK |
| High Light: |
DIN High Strength Carbon Steel Plate,4mm Hot Rolled Carbon Steel Plate,4mm Hot Rolled Carbon Steel Sheet |
||
Hot-Rolled BS700MCK2 High Strength Structural Steel Plate 4*1500*10000mm
BS700MCK2 is one of a series of high-strength steel, China special steel limited, engineering machinery series of high-strength, ultra high strength structural steel. China special steel limited in 2000, first in China to the successful development of a new class of hot-rolled products, grades are mostly used at the beginning of BS, as the first generation of high-strength steel and BS700MC have been widely used in engineering machinery, container and other industries.
BS700MCK2 steel Chemical Composition :
|
Grade |
C | Si | Mn | P | S | Alt | B |
| BS700MCK2 | ≤0.12 | ≤0.60 | ≤2.10 | ≤0.025 | ≤0.010 | ≥0.015 | ≤0.005 |
BS700MCK2 steel Mechanical Properties :
|
|
Thickness (mm) |
Yield Strength Re(MPa) | tensile strength Rm(MPa) | Elongation A5(%) | Shock Value IE (J) |
| BS700MCK2 | 3-8 | 700-860 | 780-920 | 15-21 | 40-100 |
| (8)-12 | 685-820 | 790-900 | 15-21 | 60-150 |
BS700MCK2 Delivery status: BS series adopt high-strength steel-rolled (TMCP) delivery.
Good Weldability --- carbon equivalent(Ceq) and weld crack sensitivity index(Pcm)
|
Grade |
Performance carbon content C(%) | Performance carbon content Ceq | Welding sensitivity index performance Pcm |
| BS700MCK2 | ≤0.08 | ≤0.47 | ≤0.21 |
Ceq = C + Mn/6 (Cu + Ni)/15 + (Cr + Mo + V)/5
Pcm =C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B
The number of samples required for each batch of steel sheet and strip the test items, sampling methods, test methods shall be in accordance with Table 1
|
No. |
Pilot projects | Number of tests,A | Sampling methods | Test method |
| 1 | Chemical analysis | Each furnace | GB/T20066 | GB/T223 or GB/T4335 |
| 2 | Stretching test | 1 | GB/T2975 | GB/T228 |
| 3 | Bending test | 1 | GB/T2975 | GB/T232 |
BS700MCK2 steels plate/sheet are featured :
1 . Good formability. All grades of BS steel can be cold formed.
2 . Excellent welding performance. The steels have low welding crack sensitivity and the properties of welding joint are good.
3 . Good toughness at low temperature.



FAQ
Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, Russia, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.
Hot Tags: high strength structural steel plate en10149 s700mc, China high strength structural steel plate en10149 s700mc suppliers, 686 718 Inconel Pipe, inconel alloy heating system parts, inconel alloy reaction injection molding process, 601GC Alloy Pipe, alloy inconel piping, Inconel 625 Stainless Steel Coil
You Might Also Like
Send Inquiry