Alloy 600 Nickel Steel Plate
GNEE Group offers Nickel Alloy Inconel 600 in a variety of forms, including:
Bars
Wires
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of alloy 600 nickel steel plate in China. If you're going to wholesale high quality alloy 600 nickel steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Alloy 600 Nickel Steel Plate introduce
Inconel 600 Plate is manufactured using high quality material, the substantial which is used to produce this industrialized product is patterned under a huge procedure to satisfy the consumers and retailer demands, and with respect to standard quality of material we also manufacture this industrial products which is Inconel 600 Plate as according to the need of respectable consumer in different dimensions, outlines and strategies. Inconel 600 plates can be recycled at a very high heats up to 2000 degree F whereas if we talk about Alloy 600 Sheet so it can also be used at a very high temperature same as the heat of Inconel 600 plates which is 2000 F but just a one minor difference between both of them is Alloy 600 sheets are non-magnetic and enthusiastically weld able in its features.
Alloy 600 Nickel Steel Plate


Inconel 600 plate Specification
Alloy 600 Plate Thickness 0.3 to 1200 mm or as required
UNS N06600 Plate Process Hot/ Cold Rolled
Inconel 600 Plate Length 0-12mm or as required
ASTM B168 Alloy 600 Plate Width 0-2500mm or as required
ASTM B168 Inconel 600 Plate surface No.1, No. 2D, No. 2B, BA, No.3, No.4, No.6, No.7, 2B, 2D, BA NO(8), Cold rolled sheet (CR), Hot rolled plate (HR), SATIN (Met with Plastic Coated), No.1 finish hot rolled Inconel 600 Plate, 1D, 2B, No.4, BA, 8K, satin, hairline, brush, mirror etc.
Inconel 600 Plate Dimensions
| Inconel 600 Plate Metric Dimensions | ||
|---|---|---|
| Surface finish | Thickness (mm) | Width (mm) |
| 2B – Cold rolled, heat treated, pickled, skin passed | 0.25–8.0 | max. 2032 |
| 2D – Cold rolled, heat treated, pickled | 0.4–6.35 | max. 1524 |
| 2E – Cold rolled, heat treated, mechanically descaled | 0.4–8.0 | max. 2032 |
| 2R – Cold rolled, bright annealed | 0.25–3.5 | max. 1524 |
| 2H – Work hardened | 0.4–6.35 | max. 1524 |
| Polished, brushed | 0.5–4.0 | max. 1524 |
Nickel Alloy 600 Plate Mechanical Properties
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Inconel 600 | 8.47 g/cm3 | 1413 °C (2580 °F) | Psi – 95,000 , MPa – 655 | Psi – 45,000 , MPa – 310 | 40 % |
GNEE Group Factory Environment
Alloy 600 Nickel Steel Plate

GNEE Group Product Packaging
Alloy 600 Nickel Steel Plate

FAQ
Q:Can we visit your factory ?
A:Warmly welcome once we have your schedule we will pick you up .
Q: Do you have quality control?
A: Yes, we have gained BV, SGS authentication.
Q: Can you arrange the shipment?
A: Sure, we have permanent freight forwarder who can gain the best price from most ship company and offer professional service.
Hot Tags: alloy 600 nickel steel plate, China alloy 600 nickel steel plate suppliers, seamless piping, inconel alloy printed circuit board parts, Inconel alloy material, nickel based alloy, inconel alloy mechanical parts, inconel alloy capacitor parts