625 690 Inconel Alloy Pipe
video

625 690 Inconel Alloy Pipe

Available Formats
GNEE Group offers Nickel Alloy Inconel 625 690 in a variety of forms, including:
Bars
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 625 690 inconel alloy pipe in China. If you're going to wholesale high quality 625 690 inconel alloy pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

inconel Products Application

625 690 Inconel Alloy Pipe video

625 alloy Stock Size Range:

OD: 1/2" through 4"

Wall: Schedule 10 through Schedule 80

Specifications: ASTM B444, ASME SB444

Inconel 690 Tube & Pipe N06690 Nickel Alloy Seamless Pipe
Outside Diameter 10.3-426mm
Wall Thickness 1.24-40.49mm
Length Up to 25m
inconel Material Specification

UNS N06625 Tube Chemical Composition

 

Nickel 58.0 min
Molybdenum 8.0-10.0
Nb 3.15-4.15
Iron 5.0 max
Silicon 0.50max
Sulfur 0.015 max
Carbon 0.10 max
Manganese 0.50 max
Al 0.40 max
Cr 20.0-23.0
Ti 0.40 max
P 0.015 max
Cobalt 1.0 max

Alloy 690 Pipes Chemical Composition

Element Inconel Alloy 690
Ni 58.0 min
Cr 27.0 - 31.0
Fe -
C 0.05 max.
Mn 0.50 max
S 0.015 max
Si 0.50max
Co 0.50max

 

625 690 Inconel Alloy Pipe

625 690 Inconel Alloy Pipe625 690 Inconel Alloy Pipe

Inconel625 is an alloy grade with a density of 8.4 g/cm3 and a melting point of 1290-1350°C. It has excellent resistance to inorganic acid corrosion and has excellent corrosion resistance to various corrosive media in oxidizing and reducing environments. Alloy 625 shows excellent corrosion resistance in many media. Excellent resistance to pitting, crevice corrosion, intergranular corrosion and erosion in chloride media.
INCONEL 690 (UNS N06690/W. Nr. 2.4642) is a high-chromium nickel-based alloy. It is a new third-generation alloy with better stress corrosion resistance and other properties under the working conditions of pressurized water reactor heat transfer tubes. This alloy was publicly announced in 1972. It is actually an improved alloy based on Inconel 600 with increased chromium content.

GNEE Group Factory Environment

625 690 Inconel Alloy Pipe

625 690 Inconel Alloy Pipe

Customer Case

customer visit

625 690 Inconel Alloy Pipe

625 690 Inconel Alloy Pipe

FAQ

 

 

 

 

Q: What are the advantages of your company?
A: We have many professionals, technicians, more competitive prices and the best after-sales service than other stainless steel companies.

Q: Can you send samples?
A: Of course, we can send samples to all over the world, our samples are free, but customers need to bear the express cost.

Q: What product information do I need to provide?
A: You need to provide the grade, width, thickness, coating and tonnage you need to purchase.

Q: About the product price of 625 690 Inconel Alloy Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Hot Tags: 625 690 inconel alloy pipe, China 625 690 inconel alloy pipe suppliers, inconel alloy transformer parts, inconel alloy thermoforming process, inconel alloy shaft parts, inconel alloy lubrication system parts, inconel alloy relay parts, inconel alloy steel piping

Send Inquiry

whatsapp

Phone

E-mail

Inquiry