Incoloy Alloy 825 Round Bar
video

Incoloy Alloy 825 Round Bar

Incoloy 825 is a nickel-iron-chromium alloy with additions of molybdenum, copper and titanium. This nickel steel alloy's chemical composition is designed to provide exceptional resistance to many corrosive environments. It is similar to alloy 800 but has improved resistance to aqueous corrosion.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy alloy 825 round bar in China. If you're going to wholesale high quality incoloy alloy 825 round bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Incoloy Alloy 825 Round Bar introduce

Incoloy Alloy 825 Round Bar

Incoloy Alloy 825 Round BarIncoloy Alloy 825 Round Bar

Gnee Steel Group is a prominent Incoloy 825 Round Bar fabricator, supplier, stockiest, and exporter. We are well-known for delivering high-quality round bars in a variety of diameters, lengths, standards, and thicknesses to meet our customers' needs. With the addition of titanium, copper, and molybdenum, Incoloy 825 is a chromium, nickel, and iron stabilized alloy. It is resistant to corrosion in a variety of acidic and corrosive conditions. Its resistance to crevice corrosion, pitting, and stress corrosion cracking is exceptional. In order to manufacture Incoloy 825 Round Bars, we make sure to use only the highest quality raw materials.

Incoloy 825 Round Bars are corrosion-resistant alloys based on nickel, chromium, and iron. Because of their corrosion resistance, these alloys can be used at extremely high or increased temperatures. It's also noted for its resistance to stress corrosion. Universal Metal Corporation is the most well-known and well-respected distributor and producer of Incoloy bars. The inclusion of titanium stabilizes the alloy. After fabrication, stabilizing the Incoloy 825 Bar has been shown to resist pitting and intergranular assault. This comprises welding, in which the Alloy 825 Round Bar is heated to a crucial sensitization temperature range of 650°C – 760°C. The use of Inconel 825 Round Bar in pressure vessels operating at temperatures up to 525°C has been allowed. At temperatures higher than 540°C, brittle phases can develop in Incoloy 825. As a result, it is rarely employed in applications where creep rupture qualities of the alloy are design concerns, both at these temperatures and at higher temperatures.

At 980°C, Inconel 825 Round Bar has the softest structure. Working temperatures should be in the range of 870 – 1180°C, with a finish temperature of 870 – 980°C. Incoloy 825 Round Bar can be welded using standard methods (GMAW (MIG), GTAW (TIG), SMAW (manual), and SAW). 940°C annealed Incoloy 825 Bar (UNS N08825) and other bars. The examinations are carried out by a professional who employs all of the most advanced technologies available. PMI/IGC testing, pitting resistance testing, hardness testing, macro/micro testing, chemical analysis, mechanical testing, flattening/flaring testing, and so on are all done.

Incoloy Alloy Round Bar

Incoloy Alloy 825 Round Bar

 

Specifications : ASTM B425 / ASME SB425

Dimensions : ASTM, ASME and API

Size : 10 mm To 100 mm Dia in 100 mm TO 6000 mm Length.

Length : 3 to 6 meter, Custom Cut Lengths

Finish : Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish

Form : Round, Square, Hex (A/F), Rectangle, Wire (Coil Form), Wiremesh, Billet, Ingot, Forging Etc.,

Condition : Cold Drawn & Polished Cold Drawn, Centreless Ground & Polished

Incoloy Alloy Bar

Incoloy Alloy 825 Round Bar

IS NCF 825 Incoloy Alloy Round Bar Equivalent Indian Standard

STANDARD UNS WNR. AFNOR EN JIS BS GOST OR
Alloy 825 N08825 2.4858 NC22DNB4M NiCr22Mo9Nb NCF 825 NA 21 ЭП703 ЭИ602

ASTM B425 Incoloy 825 Cold Drawn Round Bar Chemical Composition

Grade C Mn Si S Al Ti Fe Ni Cr
Incoloy 825 0.10 max 0.50 max 0.50 max 0.015 max 0.40 max 0.40 max 5.0 max 58.0 min 20.0 - 23.0

GNEE Group Factory Environment

Incoloy Alloy 825 Round Bar

Incoloy Alloy 825 Round Bar

GNEE Group Product Packaging

Incoloy 825 Round Bar

Incoloy Alloy 825 Round Bar

FAQ 

Q:Can we visit your factory ?
A:Warmly welcome once we have your schedule we will pick you up .
Q: Do you have quality control?
A: Yes, we have gained BV, SGS authentication.
Q: Can you arrange the shipment?
A: Sure, we have permanent freight forwarder who can gain the best price from most ship company and offer professional service.

Hot Tags: incoloy alloy 825 round bar, China incoloy alloy 825 round bar suppliers, Incoloy Alloy 800, alloy for flanges, alloy for drying baths, alloy for environmental protection baths, Lncoloy 800H, incoloy pipe steel

Send Inquiry

whatsapp

Phone

E-mail

Inquiry