Incoloy 800H Grind Round Bar UNS N08810
video

Incoloy 800H Grind Round Bar UNS N08810

Incoloy 800H Grind Round Bar Testing and Certifications:
Annealed and Pickled
100% PMI Testing
EN10204.3.1B Mill Test Certificate
Third-Party Inspection Accepted
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy 800h grind round bar uns n08810 in China. If you're going to wholesale high quality incoloy 800h grind round bar uns n08810 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

 

Incoloy 800H Grind Round Bar UNS N08810 Description

Incoloy 800H Grind Round Bar

 

Gnee Steel Incoloy 800H Grind Round Bar UNS N08810

Incoloy 800H ground round bar is a nickel-iron-chromium alloy known for its high-temperature strength and excellent resistance to oxidation, carburization, and high-temperature corrosion. It is a variant of Incoloy 800 with improved chemical composition and heat treatment to enhance creep and stress-rupture resistance. "Ground bar" refers to a manufacturing process in which the bar is ground to precise dimensions, surface finish, and straightness.

Size Chart Of Alloy Incoloy 800h Round Bar

Description Diameter Shape
1.250 DIA 1.2500 Rod/Bar round
1.500 DIA 1.5000 Rod/Bar round
1.00 DIA 1.0000 Rod/Bar round
4.00 DIA 4.0000 Rod/Bar round
2.00 DIA 2.0000 Rod/Bar round
.500 DIA 0.5000 Rod/Bar round
2.0000 DIA 2.0000 Rod/Bar round
3.00 DIA 3.0000 Rod/Bar round
2.500 DIA 2.5000 Rod/Bar round

Incoloy 800H Round Bars specifications

Incoloy 800H Round Bars Specification

Specifications : EN, DIN, JIS, ASTM, BS, ASME, AISI

Standard Specification :ASTM B408 / ASME SB408

Size : 5 mm To 500 mm

Diameter : 0.1 mm to 100 mm

Length : 100 mm To 3000 mm Long & Abov

Tolerance : H8, H9, H10, H11, H12, H13K9, K10, K11, K12 or as per clients' requirements

Grade : Incoloy 800H (UNS No. N08810) Round Bars 1.4958 / 1.4876

Finish : Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish

Form : Round, Square, Hex (A/F), Rectangle, Billet, Ingot, Forging Etc.

Surface : Hot Rolled Pickled or Sand Blasting Finished, Cold Drawn, Bright, Polished, Hairline

Application : Chemical process, Food processing, Petrochemical, Pollution control, Pulp and Paper, Refining, Waste treatment facilities

Condition : Cold Drawnd Pulished Cold Drawn Centreless Ground & Polished.

Incoloy 800H Chemical Composition of Grind Round Bar

Grade Ni Cr Fe Mb Ti Cu Mn C S Al Al + Ti
Incoloy 800 30.0 – 35.0 19.0 – 23.0 39.5 min – 0.15 – 0.60 – – 0.10 max – 0.15 -0.60 3.15 – 4.15

Mechanical Properties of Incoloy 800H Material Bar

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
7.94 g/cm3 1385 °C (2525 °F) Psi – 75,000 , MPa – 520 Psi – 30,000 , MPa – 205 30 %

800 Incoloy Round Bar finishes

 

800 Incoloy Round Bar finishes


Inconel 800 Round Bar Surface finish

CD Cold drawn P Polished
BD Bright drawn SRE Slit rolled edge
CG Centreless ground HF Hot finished
CF Cold finished HRAP Hot rolled annealed and pickled
P&T Peeled and turned RT Rough turned/peeled
ST Smooth turned PR Peeled and reeled

Difference Between Inconel 800 Precision Ground Bar and Inconel 800 Round Bar


Inconel 800 Round bar: is precisely as it sounds; a long, round and hollow metal bar. Inconel 800 Round bar is accessible in numerous diverse diameters extending from 1/4" up to 24".

Inconel 800 Precision Ground Bar: too known as 'Turned Ground and Polished' shafting, refers to round bars made with fine precision and high-quality steel. They are polished to ensure flawless and perfectly straight surfaces. .

 

alloy 800H Grind Round Bar UNS N08810 testing & Qualification Certificate

 

alloy 800H Grind Round Bar UNS N08810 testing & Qualification Certificate

alloy 800H Grind Round Bar UNS N08810 testing
alloy 800H Grind Round Bar UNS N08810 testing
alloy 800H Grind Round Bar UNS N08810 Qualification Certificate
alloy 800H Grind Round Bar UNS N08810 Qualification Certificate

About Gnee Steel

Gnee Steel

 

About Gnee Steel

Gnee Steel is a supplier of Incoloy 800H Grind Round Bar. Our product offerings include seamless pipes (sizes from 4 to 219 mm, thicknesses from 0.5 to 20 mm), welded pipes (sizes from 5.0 to 1219.2 mm, thicknesses from 0.5 to 20 mm), plates (thicknesses from 0.1 to 100 mm, widths from 10 to 2500 mm), strip, alloy round bar (sizes from 3 to 800 mm in diameter), flat bar (sizes from 2 to 100 mm, thicknesses from 10 to 500 mm), hexagonal bar (sizes from 2 to 100 mm), wire rod, and extruded sections. We partner with steel mills to provide our customers with Alloy 625 that meets or exceeds numerous leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN, and BS. Gnee Steel stocks and sells Incoloy 800H Grind Round Bar, pipe, tube, plate, strip, sheet, round bar, flat bar, forging billet, hexagon, wire and extruded sections. Please feel free to contact us for a quote at ss@gneesteel.com

Hot Tags: Incoloy 800H Grind Round Bar UNS N08810, China Incoloy 800H Grind Round Bar UNS N08810 suppliers, incoloy stainless pipe, alloy for magnetic materials, alloy for precipitation baths, alloy for alkali resistance, alloy for heating baths, alloy for neurology baths

Send Inquiry

whatsapp

Phone

E-mail

Inquiry