ASTM B163 Incoloy 825 Alloy Round Pipe
video

ASTM B163 Incoloy 825 Alloy Round Pipe

Name:ASTM B163 Incoloy 825 Alloy Round Pipe
Approximate grades: UNS N08825, NCF825
Certification: ISO9001:2015
Alloy category: Corrosion-resistant alloy
Substrate shape: Axis wire/strip/straight bar
Alloy series: Nickel-chromium-iron alloy
Application areas: Marine ships, petrochemicals, energy fields
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm b163 incoloy 825 alloy round pipe in China. If you're going to wholesale high quality astm b163 incoloy 825 alloy round pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

ASTM B163 Incoloy 825 Alloy Round Pipe is a nickel-iron-chromium alloy with added molybdenum, copper and titanium. Provides excellent corrosion resistance in many corrosive environments. Similar to Alloy 800, but with improved resistance to aqueous corrosion.

UNS N08825 Seamless Steel Pipe Implementation Standard: ASTM B163, ASTM SB163,
Production Method: Hot Rolling, Cold Rolling, Cold Drawing. Delivery Status: Heat Treatment and Pickling.
Product Specifications Outer Diameter: 21.3mm~762mm

Incoloy 825 Specification

Chemical Composition of ASTM B163 Incoloy 825(UNS N08825)pipe

Composition,%  
Grade N08825
Nicke 38.0–46.0
Copper 1.5–3.0
Molybdenum 2.5–3.5
Iron 22.0 min B
Manganese 1.0
Carbon 0.05
Silicon 0.5
Sulfur 0.03
Chromium 19.5–23.5
Aluminum 0.2
Titanium 0.6–1.2

 Mechanical Properties of  Nickel Alloy 825 Seamless pipes

Material and Condition Tensile Strength,
min, ksi (MPa)
Yield Strength
(0.2 % Offset),
min, ksi (MPa)
Elongation in 2in.or 50 mm (or 4 D)min, % Rockwell Hardness
(or equivalent) for
annealed ends A
Nickel-iron-chromium-molybdenum-copper alloys:Annealed UNS N08825 85 (586) 35 (241) 30 ...
Nickel Alloy 825 Products Display

ASTM B163 UNS N08825 Nickel Alloy Tube

ASTM B163 UNS N08825 Nickel Alloy Tube

Why choosing GNEE

GNEE is equipped with advanced manufacturing technologies, including: Dutch DELEM CNC bending machines that can handle thicknesses from 2mm to 100mm; Austrian Fronius welders, Japanese FANUC welding robots, and laser weld seam guidance and tracking systems. This powerful automated pipe welding production line guarantees excellent product consistency and reliability.

please contact us in time to get a quote!ss@gneesteel.com

PRODUCTS TESTING

PRODUCTS TESTING

 

Incoloy 825  pipe Supplier

Alloy 800 Plate Supplier

Incoloy 2.4858 ERW Pipe Stockists 

Incoloy 2.4858 ERW Pipe Stockists 

FAQ

Q:Can we visit your factory ?
A:Warmly welcome once we have your schedule we will pick you up .
Q: Do you have quality control?
A: Yes, we have gained BV, SGS authentication.
Q: Can you arrange the shipment?
A: Sure, we have permanent freight forwarder who can gain the best price from most ship company and offer professional service.

Hot Tags: astm b163 incoloy 825 alloy round pipe, China astm b163 incoloy 825 alloy round pipe suppliers, Incoloy Metal Tubing, alloy for springs, corrosion resistant material, alloy for motors, alloy for power plants, alloy for pharmaceutical industry

Send Inquiry

whatsapp

Phone

E-mail

Inquiry