AMS 5589 GH4169 Nickel Alloy Seamless Tube
video

AMS 5589 GH4169 Nickel Alloy Seamless Tube

Looking for a reliable supplier of high-temperature alloys for aerospace applications?
We offer high-performance GH4169 (Inconel 718) seamless tubing that meets AMS 5589 standards.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ams 5589 gh4169 nickel alloy seamless tube in China. If you're going to wholesale high quality ams 5589 gh4169 nickel alloy seamless tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Gnee Steel, a leading manufacturer of GH4169 seamless steel tubing, specializes in producing high-precision nickel-based alloy steel tubing designed for the most demanding aerospace and defense applications. Our AMS 5589 GH4169 / Inconel 718 steel tubing, processed with solution annealing, achieves an optimal balance between high-temperature strength (up to 700°C), excellent weldability, and superior oxidation resistance.

 

Whether you are designing advanced aero-engine fuel lines or high-stress structural components, our tubing ensures unparalleled reliability and long-term performance in extreme environments.

Get a quote for GH4169 seamless steel pipe now

GNEE GH4169 seamless Pipe introduce

 

AMS 5589 And AMS 5590 Aerospace Standard GH4169 Inconel 718 Seamless Tubing

 

GH4169 Superalloy Pipe

AMS 5589 specifies the requirements for seamless GH4169 (Inconel 718) nickel alloy tubing, designed for high-strength, corrosion-resistant aerospace applications, with a maximum operating temperature of 1300°F (704°C). As an age-hardening superalloy, it is commonly used in jet engine components, fasteners, and high-temperature hydraulic lines. Its key properties include high tensile strength and creep rupture strength.

Request a GH4169 pipe quote

 

AMS 5589 GH4169 Tube Description

 

Property Value / Details
Material Grade GH4169 (Equivalent to Inconel 718, UNS N07718, 2.4668)
Standard Compliance AMS 5589, ASTM B670, GJB 2296A
Outer Diameter (OD) 3mm – 219mm (Customizable)
Wall Thickness (WT) 0.5mm – 20mm
Condition Solution Annealed & Precipitation Hardened (Optional)
Mechanical Properties High Tensile Strength (>1035 MPa), Excellent Fatigue Life
Testing 100% Eddy Current / Ultrasonic / Hydrostatic Test

Note: AMS 5589 standard covers Inconel 718 seamless tubing for aerospace applications. This material must be produced using a vacuum induction melting (VIM) process, followed by vacuum arc remelting (VAR) or electroslag remelting (ESR).

 

GNEE GH4169 Tube Specification Sheet 

 

Chemical Composition (wt%) – per AMS 5589 (UNS N07718)

Element Content (%) Standard Requirement Notes
Nickel (Ni) 50.0 – 55.0 50.0 – 55.0 Matrix element
Chromium (Cr) 17.0 – 21.0 17.0 – 21.0 Oxidation and corrosion resistance
Iron (Fe) Balance (~18-20) Balance Fe-Ni-Cr base alloy
Niobium (Nb) 4.75 – 5.50 4.75 – 5.50 Primary γ″ strengthening element
Molybdenum (Mo) 2.80 – 3.30 2.80 – 3.30 Solid-solution strengthening
Titanium (Ti) 0.65 – 1.15 0.65 – 1.15 Forms γ′ strengthening phase
Aluminum (Al) 0.20 – 0.80 0.20 – 0.80 Forms γ′ strengthening phase
Carbon (C) ≤ 0.08 ≤ 0.08 Low carbon for weldability
Manganese (Mn) ≤ 0.35 ≤ 0.35 Deoxidizer
Silicon (Si) ≤ 0.35 ≤ 0.35 Deoxidizer
Phosphorus (P) ≤ 0.015 ≤ 0.015 Low for toughness
Sulfur (S) ≤ 0.015 ≤ 0.015 Low for hot workability
Boron (B) 0.002 – 0.006 0.002 – 0.006 Grain boundary strengthener
Cobalt (Co) ≤ 1.00 ≤ 1.00 Residual element
Copper (Cu) ≤ 0.30 ≤ 0.30 Residual element
Tantalum (Ta) ≤ 0.05 ≤ 0.05 Residual element
Lead (Pb) ≤ 0.0005 ≤ 0.0005 Trace element control
Bismuth (Bi) ≤ 0.00003 ≤ 0.00003 Trace element control

 

Physical properties of GH4169 tube

Property Value Notes
Density 8.19 g/cm³ –
Melting Range 1260 – 1336°C –
Thermal Conductivity (20°C) 11.4 W/m·K –
Thermal Conductivity (500°C) ~16.0 W/m·K –
Coefficient of Thermal Expansion (20-100°C) 13.0 × 10⁻⁶/°C –
Coefficient of Thermal Expansion (20-600°C) ~14.5 × 10⁻⁶/°C –
Specific Heat (20°C) 435 J/kg·K –
Modulus of Elasticity (20°C) ~200 GPa (29.0 × 10⁶ psi) –
Modulus of Elasticity (600°C) ~175 GPa –
Poisson's Ratio 0.29 – 0.30 –
Electrical Resistivity 1.25 µΩ·m –
Magnetic Permeability 1.005 (slightly magnetic) –

 

High-temperature mechanical properties of GH4169 alloy tubes (solution treatment + aging treatment)

Temperature (°C) Tensile Strength (MPa) Yield Strength (MPa) Elongation (%) Test Standard
20 (Room Temp) ≥ 1275 ≥ 1035 ≥ 12 ASTM E8
300 ~1200 ~1000 ~15 ASTM E21
400 ~1180 ~980 ~15 ASTM E21
500 ~1150 ~950 ~16 ASTM E21
600 ~1100 ~900 ~18 ASTM E21
650 ~1000 ~850 ~20 ASTM E21
700 ~850 ~750 ~22 ASTM E21
760 ~600 ~550 ~25 ASTM E21

Click to download the GH4169 alloy PDF file now

 

AMS 5589 GH4169 seamless tube dimensions and specifications

 

Parameter Range Tolerance (AMS 5589)
Outside Diameter (OD) 1.0 mm – 50.8 mm (0.040″ – 2.000″) ±0.025 – ±0.050 mm
Wall Thickness 0.15 mm – 3.0 mm (0.006″ – 0.120″) ±5% – ±10%
Length Up to 15,000 mm ±3 mm
OD Ovality – ≤ 0.75% of OD
Wall Concentricity – ≤ 10% of wall thickness
Straightness – ≤ 0.5 mm/m

 

Common AMS 5589 Tube Sizes

OD (in) OD (mm) Wall Thickness (in) Wall Thickness (mm) Typical Application
0.125 3.18 0.020 0.51 Instrumentation
0.188 4.78 0.028 0.71 Hydraulic lines
0.250 6.35 0.035 0.89 Fuel systems
0.375 9.53 0.042 1.07 Bleed air
0.500 12.70 0.049 1.24 High-pressure hydraulic
0.625 15.88 0.065 1.65 Structural lines

Contact us to customize GH4169 products to fit your project dimensions

 

Main Applications of GH4169 Seamless Steel Tubes in the Aerospace Industry

 

Aircraft Engine Components: Fuel manifolds, nozzles, and hydraulic lines.

Gas Turbines: High-pressure structural shells and internal piping.

Spacecraft Engineering: Rocket engine thrust chambers and cooling systems.

Nuclear Energy: Heat exchanger piping in high-radiation environments.

Aviation Fuel Manifold
Aviation fuel manifold
Gas Turbine
Gas turbine
Rocket Engine Thrust Chamber
Rocket engine thrust chamber
Nuclear Heat Exchanger Piping
Nuclear heat exchanger piping

 

GH4169 seamless pipe quality inspection specifications

 

As a trusted supplier, Gnee Steel adheres to a "zero-defect" principle. Every GH4169 seamless pipe undergoes a rigorous inspection process before shipment.

Eddy Current Testing (ET): Used to detect minute cracks and defects on and near the surface of pipes.

Ultrasonic Testing (UT): For thick-walled or pressure-critical pipes, it detects deep defects such as internal inclusions and porosity, conforming to AMS 2630 requirements.

Hydrostatic Testing: Each pipe must undergo high-pressure hydrostatic testing to ensure no leakage or deformation under rated operating pressure.

 

UT
UT test
PMI
PMI
Eddy Current Testing (ET)
Eddy Current Testing (ET)
Hydrostatic Testing
Hydrostatic Testing

 

GNEE Group GH4169 superalloy Packaging 

GNEE Group GH4169 superalloy Packaging

about us

Contact us to choose your preferred packaging and shipping method

 

Why do global aerospace engineering companies choose Gnee Steel's Inconel 718 tubing?

 

✅️Factory Direct: Eliminate intermediaries. We offer the most competitive wholesale prices for bulk orders, ensuring your project budget remains within reasonable limits.

✅️Quality Certification: Every shipment comes with a Factory Test Certificate (MTC) conforming to EN 10204 3.1, providing full traceability from raw materials to finished tubing.

✅️Custom Processing and OEM Services: We offer precision cutting, professional deburring, and custom length services to meet your specific assembly requirements.

✅️Experience Exporting to Global Markets: We have extensive experience handling customs clearance and logistics for aerospace projects and can provide all necessary compliance documentation.

 GH4169 certificate

 GH4169 certificate

Click to view our professional certificates for GH4169 alloy

 

FAQ

 

Q: Is your AMS 5589 GH4169 tube suitable for aero-engine casings?
A: Yes, our tubes meet the strict metallurgical and grain-size requirements mandated by AMS 5589, making them ideal for aero-engine structural components and fluid delivery systems.

 

Q: What is the lead time for bulk orders?
A: Standard sizes are typically in stock for immediate shipment (7-day delivery). For custom production runs, our lead time ranges from 4 to 6 weeks depending on quantity and specification.

 

Q: Can you provide GH4169 tubes with specific tolerances for hydraulic systems?
A: Absolutely. We use advanced cold-drawing and cold-rolling processes to achieve ultra-tight tolerances that exceed standard industry requirements.

 

Q: Do you support third-party inspections?
A: Yes, we welcome third-party inspections (SGS, BV, TUV) at our factory to verify chemical composition and mechanical properties before shipment.

Hot Tags: ams 5589 gh4169 nickel alloy seamless tube, China ams 5589 gh4169 nickel alloy seamless tube suppliers, engine alloy, engineering alloy, industrial alloy, product alloy, turbine alloy, machinery alloy

Send Inquiry

whatsapp

Phone

E-mail

Inquiry