W C-2000 Hastelloy Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of w c-2000 hastelloy pipe in China. If you're going to wholesale high quality w c-2000 hastelloy pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
W C-2000 Hastelloy Pipe
| ASTM B777-15 | Non-magnetic Class 1 |
Non-magnetic Class 2 |
Non-magnetic Class 3 |
Magnetic Class 1 |
Magnetic Class 2 |
Magnetic Class 3 |
Magnetic Class 4 |
| AMS 7725E | Type 1 Class 1 |
Type 1 Class 2 |
Type 1 Class 3 |
Type 2 Class 1 |
Type 2 Class 2 |
Type 2 Class 3 |
Type 2 Class 4 |
| MIL-T-21014 Rev D | Class 1 | Class 2 | Class 3 | Class 1 | Class 2 | Class 3 | Class 4 |
| SAE-AMS-T-21014 | Class 1 | Class 2 | Class 3 | Class 1 | Class 2 | Class 3 | Class 4 |
| Tungsten (wt%) | 90 | 93 | 95 | 90 | 92.5 | 95 | 97 |
| Binder | Ni/Cu | Ni/Cu | Ni/Cu | Ni/Fe | Ni/Fe | Ni/Fe | Ni/Fe |
| g/cm3 | 17.10 | 17.60 | 17.90 | 17.10 | 17.50 | 18.10 | 18.50 |
| lb/in3 | 0.62 | 0.64 | 0.65 | 0.62 | 0.63 | 0.65 | 0.67 |
| Hardness, HRC | 24 | 24 | 24 | 27 | 24 | 24 | 25 |
| Mpa | 675 | 650 | 680 | 645 | 645 | 660 | 660 |
| ksi | 100 | 95 | 100 | 95 | 95 | 95 | 95 |
| Mpa | 805 | 830 | 805 | 875 | 900 | 910 | 915 |
| ksi | 116 | 120 | 116 | 126 | 130 | 131 | 132 |
W c-2000 Hastelloy Metal Pipe


Hastelloy W alloy is a nickel-based alloy composed of nickel, molybdenum, chromium, cobalt and other elements. Hastelloy W alloy has a nickel content of approximately 60%. Hastelloy W is a solid solution strengthened alloy, mainly used for welding dissimilar alloys. It can be used for gas tungsten arc welding straight-cut filament, gas metal arc welding layer wound wire, and coated electrode. The performance of dissimilar welded joints made from alloy w depends on the alloy to which they are joined, but they are often used in various combinations. It is also produced in sheet and sheet form for structural applications up to 760 °C (1400 °f).
Hastelloy C-2000 Hastelloy C-2000 is an enhanced alloy developed to expand the application range of materials. It originated from a conceptual design idea and added copper to the already well-established Ni-Cr-Mo alloy. Since it entered the market in late 1996, it has continued to gain market popularity, thanks to its inherent versatility. Technical innovation not only gradually improves the alloy's resistance to water corrosion, but also expands the application scope of the Ni-Cr-Mo family alloy as a whole.
Hot Tags: w c-2000 hastelloy pipe, China w c-2000 hastelloy pipe suppliers, alloy for milling, G 35 C 22HS Hastelloy Pipe, nickel chromium molybdenum alloy, material seamless piping, alloy for heat treatment, alloy for finishing
Previous
UNS N06002 G30 Hastelloy PipeYou Might Also Like
Send Inquiry