Welding Hastelloy C22 Uns N06022 En 2.4602 Tube
Outer diameter: 6-200 mm
Wall thickness: 0.35-6.00 mm
Length: 0.5-12 m
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of welding hastelloy c22 uns n06022 en 2.4602 tube in China. If you're going to wholesale high quality welding hastelloy c22 uns n06022 en 2.4602 tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Welding Hastelloy C22 Uns N06022 Tube introduce
Welding alloy C22 Uns N06022 En 2.4602 Tube


Hastelloy WNR 2.4602 welded pipe has improved creep and stress rupture properties, which should be considered under sensitization and intergranular corrosion exposure conditions. It is a low carbon steel. It is often used at low temperatures due to its high toughness and low magnetic permeability. This high alloy steel has excellent strength at high temperatures, as well as strong resistance to creep deformation and environmental erosion. It is used in fluidized bed coal burners, flare heads, tube hangers and radiant tubes in oil refining and steam boilers. It is also used to make burner heads, clamps, brick brackets, brick racks and tube hangers.
C22 Hastelloy Alloy Welded Pipes Specification :
| Specifications | : | ASTM, ASME and API |
| Dimensions | : | ASTM, ASME B619 |
| Size | : | 15NB TO 150 NB IN |
| Welded B619 Pipes | : | 1 1/2" NB - 16" NB |
| Schedule | : | SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
| Grade | : | , Hastelloy C22 (UNS No. N06022) |
| Type | : | ERW / Welded / Fabricated / CDW |
| Specialized in | : | Large Diameter Size |
| Length | : | Single Random, Double Random & Required Length |
| Form | : | Round Pipes/Tubes, Square Pipes/Tubes, Rectangular Pipe/Tubes, Coiled Tubes, "U" Shape, Pan Cake Coils, Hydraulic Tubes |
| End | : | Plain End, Beveled End, Treaded |
Hastelloy UNS N06022 Welded Pipes Chemical Composition
| Hastelloy C22 | Ni | C | Mo | Mn | Si | Fe | P | S | Co | Cr | W | V |
| Balance | 0.010 max | 12.5 – 14.5 | 0.50 max | 0.08 max | 2 – 6 | 0.02 max | 0.02 max | 2.5 max | 20 – 22.5 | 2.5 – 3.5 | 0.35 max |
GNEE Group Product Packaging
Welding Hastelloy C22 Uns N06022 Tube

GNEE Group Factory Environment
Hastelloy C22 Uns N06022 En 2.4602 Tube

FAQ
Q: How do you control quality ?
A: Mill test certification is supplied with shipment, third party inspection is available. And we also get ISO, SGS, Alibaba Verified.
Q: How many coutries you already exported ?
A: We have become trade partners with more than 50 countries around the world, mainly exporting to the United States, Britain, Kuwait, Egypt, Türkiye, Jordan, India, etc.
Q: Can you provide sample ?
A: Of course! As long as you contact us, we can provide free inventory samples. Customized samples take approximately 5-10 days.