Hastelloy Alloy C22 Buttweld Fittings
video

Hastelloy Alloy C22 Buttweld Fittings

Gnee Steel Group is the foremost option for the best quality Hastelloy C22 Buttweld Fittings. Our fittings can applicable for all types of industrial applications. We use high quality materials for manufacturing these fittings. We produce buttweld fittings in various lengths, diameters, and dimensions as per requirement. We use reliable machinery to produce an exclusive quality product. As per international standards, our company produces these fittings. Buttweld Fittings used to prevent metal from damage. Buttweld Fittings shows seamless flow inside the pipe.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy alloy c22 buttweld fittings in China. If you're going to wholesale high quality hastelloy alloy c22 buttweld fittings made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

 

Product Introduction

 

Hastelloy C22 is used in applications that required excellent resistance to intergranular corrosion and natural corrosion. Our Hastelloy C22 Buttweld Fittings shows resistance pitting and crevice corrosion and stress corrosion cracking. This alloy has high resistance to high temperatures. Our welding rod has great work capability in any condition. Hastelloy C22 shows resistance to all metal that is used in the marine industry. This Hastelloy C22 is resistant to reducing conditions and prevents aqueous corrosion. Our fittings are used in chlorination plants, incinerators, water treatment plants, and other implementations. This alloy contains carbon, chromium, cobalt, iron, and molybdenum. These contents provide enhanced functionality. Hastelloy C22 Buttweld Fittings show excellent resistance to several chemical processing conditions like ferric and cupric chloride hot solutions. Hastelloy C22 alloy also resists the production of grain precipitates in the welded areas. In welded form, it is suitable for use in chemical processing operations. Our products have physical properties like thermal conductivity, the mean coefficient of thermal expansion, and thermal diffusivity. Our Hastelloy C22 Buttweld Fittings are used in various manufacturing industries like power, chemical processing, paper processing, and waste disposal.

 

Hastelloy C22 Pipe Fittings can be welded using shielded metal arc, gas metal arc, or gas tungsten arc. For maximum corrosion resistance, ASTM B366 UNS N06022 cold worked parts can be re-annealed. Rapid work hardening of ASTM B366 UNS N06022 material produces heat while cutting. It also offers great resistance to metal removal due to its high shear strength.

The compound of various elements performs well to work in a highly acidic atmosphere. Additionally, it gives the ability to sustain in pitting and crevice corrosion resistance conditions. These abilities are due to the presence of nickel and molybdenum. Additionally, Hastelloy C22 Pipe Fittings give additional stability to work in metallurgical operations. Also, it does not receive the impact of heating and welding conditions. Hence, our designed pipe fittings of Hastelloy C22 can sustain well in higher temperature and atmospheric conditions.

 

product-891-251

 

product-1223-687

 

Specification Of Hastelloy C22 Buttweld Pipe Fittings

Specifications : ASTM B366 / ASME SB366

Dimensions : ASME/ANSI B16.9, ASME B16.28, MSS-SP-43

Size : Seamless Butt Weld Fittings: 1/2″ – 10″, Welded Butt Weld Fittings: 1/2″ – 48″

Type : Seamless / Welded / Fabricated

Schedule : Sch 5 TO Sch XXS.

Thickness : 20 Swg., 18 Swg., 16 Swg., 14 Swg., 12 Swg., 10 Swg., & Sch. 10, Sch. 40, Sch. 80, etc

 

Chemical Composition Of Hastelloy C22 Pipe Fittings

Grade

C

Mn

Si

Co

P>

Fe

Mo

Ni

Cr

S

W

V

Alloy C22

0.010 max

0.50 max

0.08 max

2.5 max

0.02 max

2 – 6

12.5 – 14.5

Bal

20 – 22.5

0.02 max

2.5 – 3.5

0.35 max

 

ASME SB 366 Hastelloy C22 Pipe Fittings Mechanical Properties

Density

Melting Point

Tensile Strength

Yield Strength (0.2%Offset)

Elongation

8.69 g/cm3

1399 °C (2550 °F)

Psi – 1,00,000 , MPa – 690

Psi – 45000 , MPa – 310

45%

 

Equivalent Grades Of Hastelloy C22 Pipe Fittings

STANDARD

WERKSTOFF NR.

UNS

JIS

EN

Hastelloy C22

2.4602

N06022

NW 6022