C22 C276 Hastelloy Alloy mirror polishing Tubing
Length: 0.5 to 12 m
Wall thickness: 0.5 to 30 mm
Outer diameter: 3 to 600 mm
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of c22 c276 hastelloy alloy mirror polishing tubing in China. If you're going to wholesale high quality c22 c276 hastelloy alloy mirror polishing tubing made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
C22 C276 Hastelloy mirror polishing Tubing introduce
C22 C276 Hastelloy Alloy mirror Tubing


Hastelloy C-22 has the UNS designation N06022. The alloy is primarily nickel, accounting for about 56% of its total weight. The additions of chromium and molybdenum in the Hastelloy C22 seamless pipe alloy are 22% and 13%, respectively. The alloy has excellent oxidation resistance. C22 Hastelloy hexagonal pipes are particularly resistant to corrosive aqueous media, such as chemicals containing wet chlorine, and oxidizing acid solutions containing nitric acid or chloride ions.
Hastelloy C22 pipe suppliers recommend this alloy when super austenitic or duplex stainless steel alloys are overwhelmed in extremely corrosive media. Another important addition to the ASTM B622 Hastelloy C22 seamless pipe chemistry is tungsten, which gives the alloy superior resistance to uniform corrosion compared to other alloys such as 625 alloy or C276 alloy. Tungsten also improves the localized corrosion resistance of ASTM B619 UNS N06022 welded pipe.
Hastelloy C276 pipes are made of nickel-molybdenum-chromium alloy, which has excellent corrosion resistance. The material is resistant to pitting and crevice corrosion. Tungsten is added to Hastelloy C276 pipes, making it one of the most versatile corrosion-resistant alloys in the world.
Gnee Steel is a leading manufacturer and supplier of this type of pipes, covering a wide range of sizes and types. Pipe types include seamless, electric resistance welded (ERW), fabricated, and welded. Hastelloy C276 pipes meet ASTM B622 and B619 specifications. Its sizes vary according to ASTM, ASME, and API standards. Pipe lengths range from single-layer random, double-layer random to cut-to-length.
Alloy C276 seamless pipes are available in sizes ranging from 15 inches to 150 inches. Pipe gauges vary from sch5 to sch160, and pressure ratings vary from gauge to gauge. In addition, hydraulic pipes and round pipes are also available. UNS N10276 pipes can be plain end, threaded end, or bevel end. The material also contains carbon, manganese, silicon, iron, phosphorus, sulfur, and cobalt. This composition gives the material a high melting point of 1370 degrees Celsius. Hastelloy C276 seamless pipes have a minimum yield strength of 355MPa and a minimum tensile strength of 790MPa. The material has a high density, weighing 8.89 grams per cubic centimeter. With these mechanical and physical properties, these pipes can be used in some of the most demanding applications such as pollution control, exhaust pipes, heat exchangers, and offshore engineering applications. Contact us to learn more about ASTM B619 Hastelloy C276 welded pipes and their prices.
Hastelloy C22 Seamless Pipes Specification:
| Specifications | : | ASTM B 622 ASME SB 622 / ASTM B 619 ASME SB 619 |
| Dimensions | : | ASTM, ASME, and API |
| Size | : | 15″NB TO 150″NB IN |
| Specialized in | : | Large Diameter Size |
| Schedule | : | SCH5, SCH10, SCH40, STD, SCH80, SCH160 |
| Type | : | Seamless / ERW / Welded / Fabricated |
| Form | : | Round, Hydraulic Etc |
| Length | : | Single Random, Double Random & Cut Length. |
| End | : | Plain End, Beveled End, Treaded |
C22 Hastelloy Alloy Pipes and Tubes Chemical Composition:
| Hastelloy C22 | Ni | C | Mo | Mn | Si | Fe | P | S | Co | Cr |
| Balance | 0.010 max | 12.5 – 14.5 | 0.50 max | 0.08 max | 2 – 6 | 0.02 max | 0.02 max | 2.5 max | 20 – 22.5 |
Hastelloy C276 Pipes & Tubes Specification
Specifications : ASTM B622, B619, B626 / ASME SB622, SB619, SB626
Standard : ASTM, ASME and API
Size Range : 15"NB – 150"NB
Outer Diameter : 1.250″ – 6.000″ (30-150mm)
Wall Range : 0.095″ – 1.000″ (.2.5-25mm)
Schedule : SCH 10, SCH20, SCH30, SCH40, STD, SCH60, XS, SCH80, SCH120, SCH140, SCH160, XXS
Type : Seamless / ERW / Welded / Fabricated / LSAW Pipes
Length : Single Random, Double Random & Cut Length
Form : Round Pipes/Tubes, Square Pipes/Tubes, Rectangular Pipe/Tubes, Coiled Tubes, "U" Shape, Pan Cake Coils, Hydraulic Tube
Grade Hastelloy C276 Pipes & Tubes UNS (N10276), DIN (2.4819)
UNS N10276 Pipe Chemical Composition
| Hastelloy C276 | Ni | C | Mo | Mn | Si | Fe | P | S | Co | Cr |
| Balance | 0.010 max | 15.00 – 17.00 | 1.00 max | 0.08 max | 4.00 – 7.00 | 0.04 max | 0.03 max | 2.5 max | 14.50 – 16.50 |
GNEE Group Factory Environment
C276 Hastelloy Alloy mirror polishing Tubing

GNEE Group Product Packaging
C22 Hastelloy Alloy mirror polishing Tubing

FAQ
Q: What is your terms of payment?
A: 20% Prepayment and balance see B/L copy or 100%LC at sight.
Q: Are you a factory or a trading company?
A: We are a professional manufacturer, and our company is also a very professional steel products trading company. We can offer a wide range of steel as well as super stainless steel products.
Q: What does your factory do in terms of quality control?
A: We have obtained ISO, CE and other certifications. From materials to products, we check every process to maintain good quality.