Hastelloy G-33
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy g-33 in China. If you're going to wholesale high quality hastelloy g-33 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
HASTELLOY alloy G-3 (UNS N06985 / W. Nr. 2.4619) is a nickel-chromium-iron alloy with additions of molybdenum and copper. Some of the minor elements are controlled to yield increased resistance to heataffected-zone (HAZ) corrosion and improved weldability. Alloy G-3 has excellent corrosion resistance to oxidizing chemicals and atmospheres. It is also resistant to reducing chemicals because of its nickel and copper contents. Nickel also provides the alloy with exceptional stress-corrosion-cracking resistance in chloride-containing environments. The high molybdenum provides very good resistance to pitting and crevice corrosion. The low carbon helps prevent sensitization, giving the alloy resistance to intergranular corrosion.
HASTELLOY alloy G-3 is particularly suitable for handling reducing acids such as phosphoric and sulfuric. It is used in flue gas desulfurization systems (scrubbers), especially in quencher, damper, and outlet ducting areas. It can be used in other air pollution control systems in the chemical and pulp and paper industries. It is a good candidate for evaporators, heatexchangers, tank liners, and other equipment in phosphoric acid manufacturing plants.
Today's exploration for oil and gas leads to a range of highly corrosive environments that, in turn, require a range of corrosion-resistant high nickel content alloys. HASTELLOY® alloy G-3 is one of these alloys, providing an excellent combination of mechanical properties and strength. This alloy has been used extensively as OCTG (Oil Country Tubular Goods) in hot, sour environments.
Corrosion Resistance
The combination of alloying elements in HASTELLOY alloy G-3 is designed to provide broad resistance to general and localized corrosion, as well as to stress corrosion cracking. The range of corrosive conditions withstood by HASTELLOY alloy G-3 is indicated by the alloy's ability to resist both acids and alkalies and both oxidizing and reducing media.
HASTELLOY alloy G-3 exhibited better corrosion resistance than Alloy G in the 10% HCl; 50% H2SO4; 85% H3PO4; 7% H2SO4 + 3% HCl + 1% FeCl3 + 1% CuCl2; 65% HNO3, and Streicher test environments. Alloy G showed slightly better resistance in the 10% H2SO4 test. Both alloys showed similar corrosion resistance in the 30% H3PO4 test.
More +
Main Standards




Chemical Composition
Data Sheet
Mechanical Properties
| Product | Tensile Strength | Yield Strength (0.2% Offset) |
Elongation | ||
|---|---|---|---|---|---|
| ksi | MPa | ksi | MPa | % | |
| Sheet & Plate (Annealed) | 90 | 621 | 35 | 241 | 45 |
| OCTG (Cold worked) | 130 | 896 | 125 | 862 | 13 |
FAQ
Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.