Hastelloy C-22 Alloy Steel Rod
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy c-22 alloy steel rod in China. If you're going to wholesale high quality hastelloy c-22 alloy steel rod made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Hastelloy C-22 Alloy Steel Rod is a versatile nickel-chromium-molybdenum alloy with excellent resistance to corrosion in both oxidizing and reducing environments. It is perfect for use in severe environment applications, including chemical processing, pollution control, and pulp and paper production.

The alloy conforms to ASTM B574 standards and is available in diameters ranging from 3.0mm to 300.0mm, with a length of either random or custom. Hastelloy C-22 Alloy Steel Rod has excellent resistance to pitting, crevice corrosion, and stress corrosion cracking.
| Grade | Hastelloy C-22 |
|---|---|
| ASTM Standards | ASTM B574 |
| Diameter (mm) | 3.0 - 300.0 |
| Length (m) | Random or Custom |

Moreover, it has superior resistance to a wide range of corrosive media, including oxidizing and reducing acids, molten sulfur, phosphate esters, and seawater. This makes it suitable for use in highly corrosive environments found in the chemical, petrochemical, and pharmaceutical industries.
In conclusion, Hastelloy C-22 Alloy Steel Rod is a high-performance alloy that offers excellent corrosion resistance and superior mechanical properties. Its impressive capabilities make it an ideal choice for applications that require resistance to corrosive media.
Hot Tags: hastelloy c-22 alloy steel rod, China hastelloy c-22 alloy steel rod suppliers, Hastelloy B2, alloy for scrubbers, alloy for plating, alloy for nuclear power plants, material seamless piping, alloy for turning