Hastelloy B3 Plate
video

Hastelloy B3 Plate

Hastelloy B3 is a nickel-molybdenum alloy with excellent resistance to pitting, corrosion, and stress-corrosion cracking plus, thermal stability superior to that of alloy B2.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy b3 plate in China. If you're going to wholesale high quality hastelloy b3 plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Hastelloy B3 is a nickel-molybdenum alloy with excellent resistance to pitting, corrosion, and stress-corrosion cracking plus, thermal stability superior to that of alloy B2.

 

This nickel steel alloy has great resistance to knife-line and heat–affected zone attack. Alloy B-3 also withstands sulfuric, acetic, formic and phosphoric acids, and other non-oxidizing media. Furthermore, this nickel alloy has excellent resistance to hydrochloric acid at all concentrations and temperatures. Hastelloy B-3's distinguishing feature is its ability to maintain excellent ductility during transient exposures to intermediate temperatures. Such exposures are routinely experienced during heat treatments associated with fabrication.

Alloy B-3 has poor corrosion resistance to oxidizing environments, therefore, it is not recommended for use in oxidizing media or in the presence of ferric or cupric salts because they may cause rapid premature corrosion failure. These salts may develop when hydrochloric acid comes in contact with iron and copper. Therefore, if this nickel steel alloy is used in conjunction with iron or copper piping in a system containing hydrochloric acid, the presence of these salts could cause the alloy to fail prematurely.

Common Trade Names:

Hastelloy B3 , UNS N10675 , W.Nr:2.4600

Specifications:

DIN: 17744, 17750, 17751, 17752, 17753

ASTM :B 333, B 335, B 564, B 619, B 622, B 626

ASME: SB 333, SB 335, SB 619, SB 622, SB 626

Hastelloy B3 Characteristic

Maintains excellent ductility during transient exposures to intermediate temperatures

Excellent resistance to pitting, corrosion and stress-corrosion cracking

Excellent resistance to knife-line and heat-affected zone attack

Excellent resistance to acetic, formic and phosphoric acids and other non-oxidizing media

Thermal stability superior to alloy B-2

Resistance to hydrochloric acid at all concentrations and temperatures

Hastelloy B3 Chemical Composition

% Ni Cr Mo Fe W C Si Co Mn V P S Ti Cu Al Zr Nb/Cb Ta Ni+Mo
Min 65 1 27 1 94
Max 3 32 3 3 0.01 0.1 3 3 0.2 0.03 0.01 0.2 0.2 0.5 0.1 0.2 0.2 98

Hastelloy B3 Physical Properties

Density Melting range
9.22 g/cm³ 1370-1418°C

Hastelloy B3 Alloy Minimum Mechanical Properties In The Room Temperature

Ultimate Tensile Strength Yield Strength (0.2% offset) Elongation
125 Ksi(860 MPa) 60 Ksi (420 MPa) 50%

Hastelloy B3 Available Shape

Hastelloy B3 Size Range

Bars & Rods & Foring Ring /Flanges

Sheet & Plate

Strip & Coil

Welding Wire &Spring wire

Seamless Tube & Welded Pipe

product-720-720product-720-720product-720-720product-720-720

Hastelloy B3 ApplicationsI

Acetic acid production, initial phase in presence of iodide catalyst

Methyl methacrylate production with hot 98 % H2SO4

Production of herbicides, insecticides, ethylene glycol, ethyl benzene

 

 

FAQ

 

Q: What are your company's main products ?
A: Our main products are stainless steel plate/sheet, coil, round/square pipe, bar, nickel alloys, etc.
Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, Russia, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.

Hot Tags: hastelloy b3 plate, China hastelloy b3 plate suppliers, alloy for machining, alloy for heat exchangers, alloy for welding, nickel chromium molybdenum tungsten alloy, material piping, UNS N06455 N10629 Hastelloy Pipe

Send Inquiry

whatsapp

Phone

E-mail

Inquiry