2.4618 2.4619 Hastelloy Pipe And Tube
video

2.4618 2.4619 Hastelloy Pipe And Tube

N10629 N10629 alloy is a NI-MO corrosion alloy, which is a low-carbon alloy. It is an alloy developed to solve the medium-temperature brittleness and welding cracks caused by the precipitation of B2 alloy B phase.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 2.4618 2.4619 hastelloy pipe and tube in China. If you're going to wholesale high quality 2.4618 2.4619 hastelloy pipe and tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

2.4618 2.4619 Hastelloy Pipe and tube

Product Introduction

1. Chemical composition analysis

The main chemical components of 2.4619 (NiCr22Mo7Cu) and 2.4618 (NiCr22Mo6Cu) include carbon (C), silicon (Si), manganese (Mn), chromium (Cr), molybdenum (Mo), nickel (Ni), niobium (Nb), cobalt (Co) and iron (Fe). Among them, nickel is the main matrix element of these two alloys, giving them good toughness and corrosion resistance. The addition of chromium, molybdenum and niobium further improves the alloy's resistance to oxidation and corrosion, especially in high-temperature environments.

Specifically, the carbon content in 2.4619 is lower (≤0.015%), which helps reduce the brittleness of the alloy. At the same time, its molybdenum content range is wide (6.0~8.0%), which helps to improve the corrosion resistance of the alloy. The niobium content in 2.4618 is relatively high (1.75~2.5%), which enhances the high temperature stability and oxidation resistance of the alloy.

2. Performance characteristics

1. Corrosion resistance: Due to high chromium, high molybdenum and the addition of an appropriate amount of niobium, these two alloys show good corrosion resistance in a variety of media, especially in oxidizing media.
2. High temperature stability: The high niobium content in 2.4618 gives it better stability at high temperatures and is suitable for high temperature working environments.
3. Mechanical properties: These two alloys have high strength and hardness while maintaining good toughness and ductility, giving them excellent mechanical properties in a variety of applications.

3. Application fields

1. Aerospace: Due to the high temperature stability and corrosion resistance of nickel-based alloys, they are widely used in the aerospace field, such as engine parts, combustion chambers, turbine blades, etc.
2. Petrochemical industry: These two alloys are commonly used in the petrochemical industry to manufacture corrosion-resistant pipes, valves, pumps, heat exchangers and other equipment.
3. Nuclear energy: The radiation resistance of nickel-based alloys gives them certain application prospects in the field of nuclear energy, such as heat exchangers and pumps in nuclear reactors.

 