ASTM B335 Hastelloy Alloy B2 Round Bar
video

ASTM B335 Hastelloy Alloy B2 Round Bar

Hastelloy B2 round bar specifications
Standards: ASTM, ASME
Grade: B335, SB335
Thickness: 50mm to 6000mm
Length: 1 to 6 meters, customized cutting lengths
Round bar size: 3mm to 800mm
Square bar size: 4mm*4mm to 100mm*100mm
Flat bar size: 2mm to 100mm
Hexagonal bar size: 2mm to 100mm
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm b335 hastelloy alloy b2 round bar in China. If you're going to wholesale high quality astm b335 hastelloy alloy b2 round bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

ASTM B335 Hastelloy B2 Round Bar introduce

ASTM B335 Hastelloy Alloy B2 Round Bar

ASTM B335 Hastelloy Alloy B2 Round BarASTM B335 Hastelloy Alloy B2 Round Bar

ASTM B335 rods are made from a nickel-molybdenum alloy. ASTM B335 rods and round bars exhibit excellent resistance in reducing environments such as phosphoric acid, acetic acid, sulfuric acid and hydrogen chloride gas. Nickel-molybdenum alloy rods are extremely resistant to hydrochloric acid at all temperatures and concentrations. Nickel-molybdenum alloy rods also exhibit excellent resistance to stress corrosion cracking, pitting corrosion, and heat-affected zone and knife-line corrosion.

The equivalent designations for Hastelloy B2 round bars are UNS N10665 and WERKSTOFF NR. 2.4617. Hastelloy B2 round bars are made from a nickel-chromium alloy with small additions of aluminum, niobium, molybdenum, titanium and iron. Hastelloy B2 round bars have excellent corrosion resistance, excellent weldability, heat treatability, excellent formability and very high strength. Hastelloy B2 round bars also have excellent resistance to heat and cryogenic temperatures. Hastelloy B2 round bar is widely used in gas turbines, fasteners, auxiliary safety valves, pipes, reverse thrust devices, spindles, industrial fasteners, aircraft engines, etc. due to its many excellent properties.

Hastelloy Alloy B2 Rods Specification :

Designation : ASTM B335 / ASME SB335
Size : 5 mm To 500 mm
Diameter : 0.1 mm to 100 mm
Length : 100 mm To 3000 mm Long & Above
Grades : Hastelloy B2 (UNS N10665) Round Bars 2.4617
Length :

100 mm To 3000 mm Long & Above

Form :

Round, Square, Hex (A/F), Bush, Rectangle, Flat, Wire Mesh

Hastelloy B2 Round Bars Chemical Composition

Hastelloy B2 Ni C Mo Mn Si Fe P S Co Cr
Balance .02 max 26.0-30.0 1.0 max .10 max 2.0 max .040 max .030 max 1.0 max 1.0 max

Mechanical Properties of B335 Hastelloy B2 Bar

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
9.2 g/cm3 1370 °C (2550 °F) Psi – 1,15,000 , MPa –760 Psi – 52,000 , MPa – 350 40 %

Hastelloy B2 Bars have exceptional chemical resistance. They can be used in high temperatures. They have a nickel base. They are highly resistant to all temperatures. It is used for chemical progression application applications. It is an alloy of tungsten, molybdenum, chromium, and nickel.An alloy B2 is an alloy made of nickel and molybdenum. A B2 Alloy Flat Bar has a significant resistance to reducing environments. It can resist hydrogen chloride gas. It can also resist sulphuric, acetic, and phosphoric acids. It also has elongation properties and stiffness.

GNEE Group Factory Environment

ASTM B335 Alloy B2 Round Bar

ASTM B335 Hastelloy Alloy B2 Round Bar

GNEE Group Product Packaging

ASTM B335 Hastelloy Metal Alloy B2 Round Bar

ASTM B335 Hastelloy Alloy B2 Round Bar

FAQ

Q: Can I get samples before order ?

A: Yes, of course.We can produce by your samples or technical drawings ;

Q: Can I go to your factory to visit?

A: Of course, we welcome customers from all over the world to visit our factory ;

Q: What are the advantages of your company ?

A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.

Hot Tags: ASTM B335 Hastelloy Alloy B2 Round Bar, China ASTM B335 Hastelloy Alloy B2 Round Bar suppliers, alloy for drawing, material seamless piping, G 35 C 22HS Hastelloy Pipe, Hastelloy B2, Hastelloy Alloy S Seamless Pipe, alloy for petrochemical applications