UNS S32760 Duplex Stainless Steel Sheet
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of uns s32760 duplex stainless steel sheet in China. If you're going to wholesale high quality uns s32760 duplex stainless steel sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
UNS S32760 Duplex Stainless Steel Sheet
Product Introduction
UNS S32760 is a grade of duplex stainless steel plate that is highly resistant to corrosion and erosion. With its excellent properties, S32760 is becoming increasingly popular in industries such as oil and gas, chemical processing, and seawater applications.
UNS S32760 is a stainless steel containing 18% to 20% chromium, 11% to 15% nickel, and 3% to 4% molybdenum. It has excellent corrosion resistance, especially to the corrosion of sulfuric acid, acidic solutions and salt water, and is often used in the manufacture of chemical equipment, marine equipment, pharmaceutical equipment, etc.
When the chromium content in UNS S32760 is high, its oxidation resistance and weld strength can be improved, thereby improving the welding performance of UNS S32760.
The chemical composition of UNS S32760 is: Chromium (Cr):
23.0-26.0%, Nickel (Ni): 19.0-22.0%, Silicon (Si): ≤1.50%, Phosphorus (P): ≤0.045%, Sulfur (S): ≤0.030%. If the phase distribution is uniform, the strength and plasticity of UNS S32760 will be uniformly improved; on the contrary, if the phase distribution is uneven, it will easily lead to uneven fracture and deformation of the material, reducing the strength and plasticity of UNS S32760.

Hot Tags: uns s32760 duplex stainless steel sheet, China uns s32760 duplex stainless steel sheet suppliers, duplex stainless steel modification, duplex stainless steel toughness, duplex stainless steel research, duplex stainless steel manufacturing, duplex stainless steel coil, duplex stainless steel recyclability