UNS S31803 Duplex Stainless Steel Welded Pipe
video

UNS S31803 Duplex Stainless Steel Welded Pipe

Duplex Steel S31803 Welded Tube is highly regarded for its superior corrosion resistance, mechanical strength, and versatility in diverse industries such as oil and gas, chemical processing, and desalination plants.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of uns s31803 duplex stainless steel welded pipe in China. If you're going to wholesale high quality uns s31803 duplex stainless steel welded pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

UNS S31803 Duplex Stainless Steel Welded Pipe

Product Introduction

S31803 duplex stainless steel is a kind of steel with good corrosion resistance and high strength (yield strength is 2-3 times that of other austenitic steels). The steel contains high chromium and molybdenum, so it has excellent The ability to resist pitting and uniform corrosion. The dual-phase microstructure ensures that the steel has a high resistance to stress corrosion cracking, and the mechanical strength is also high. S31803 duplex stainless steel pipe is a medium-alloy duplex stainless steel with good chloride stress resistance. Medium alloy type-representative grade is UNS S31803 (22Cr-5Ni-3Mo-0.15N); S31803 duplex steel pipe is used in three types of duplex steel (2205 duplex stainless steel pipe, 2507 duplex stainless steel pipe, S31803 duplex stainless steel pipe, and S31803 duplex stainless steel pipe. Seam tube).

Duplex Steel S31803 Welded Tube is a type of tubing made from Duplex Steel Grade S31803. This material combines austenite and ferrite microstructures, offering a unique set of properties. The key features of Duplex Steel S31803 Welded Tube include excellent corrosion resistance, particularly in environments containing chlorides and acidic solutions. It also exhibits high strength, allowing it to withstand demanding conditions.

ASTM A790 S31803 Duplex Steel Welded Pipes Equivalent Grades

STANDARD UNS WERKSTOFF NR.
Duplex 31803 S31803 1.4462

 

UNS S31803 Duplex Steel Welded Pipe Chemical Composition

C Mn Si P S Cr Mo Ni N Fe
0.030 max 2.00 max 1.00 max 0.030 max 0.020 max 22.0 – 23.0 3.0 – 3.5 4.50 – 6.50 0.14 – 0.20 63.72 min

 

Duplex Steel WERKSTOFF NR. 1.4462 Welded Pipe Mechanical Properties

Grades Density (g/cm 3) Density (lb/in 3) Melting Point (°C) Melting Point (°F)
S31803 7.805 0.285 1420 – 1465 2588 – 2669

Hot Tags: uns s31803 duplex stainless steel welded pipe, China uns s31803 duplex stainless steel welded pipe suppliers, duplex stainless steel user, duplex stainless steel sell, duplex stainless steel purpose, duplex stainless steel upgrade, duplex stainless steel machining, duplex stainless steel importer