Super Duplex UNS S32750 Alloy Stainless Steel Plates
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of super duplex uns s32750 alloy stainless steel plates in China. If you're going to wholesale high quality super duplex uns s32750 alloy stainless steel plates made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
We manufacture these sheets and plates in all dimensions and specifications, primarily focusing on super duplex plate production. Super Duplex UNS S32750 alloy, which is an excellent choice for producing these products, contains iron, chromium, and the addition of molybdenum. This alloy offers exceptional qualities such as good pitting resistance, high tensile strength, and remarkable overall strength. It also resists stress corrosion cracking at moderate temperatures, surpassing conventional austenitic stainless steel.

Super Duplex UNS S32750 Plates' speciality lies in their exceptional ability to withstand corrosive media effectively. Super Duplex UNS S32750 plates exhibit extraordinary strength thanks to their composition of metals such as nickel, chromium, cobalt, sulfur, and carbon. These plates find extensive utility in applications requiring the creation of intricate hardware tools. The alloy is produced using techniques that ensure robustness and durability.
| Property | Details |
|---|---|
| Specifications | ASTM A240 / ASME SA240 |
| Dimension Standard | MSRR, AMS, BS, JIS, AISI, ASTM, GB, DIN, EN, etc |
| Thickness | 0.3 mm to 120 mm |
| Width | 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc |
| Length | 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc |
| Finish | 2B, 2D, BA NO (8), Cold rolled sheet (CR), Hot rolled plate (HR), SATIN (Met wistrong Plastic Coated), No.1 finish hot rolled, 1D, 2B, No.4, BA, 8K, satin, hairline, brush, mirror etc. |

Super Duplex UNS S32750 sheets are generously sized, allowing various welding processes. Their thickness is sufficient for exposure to rigorous hardening procedures. These products are well-suited for heavy workloads and high-pressure conditions, showcasing remarkable adaptability. Notably, our plates have low thermal expansion and high strength, and they exhibit higher thermal conductivity compared to other types of steel. This grade performs exceptionally well even in high-temperature environments, withstanding temperatures of up to 300 degrees Celsius.
Hot Tags: super duplex uns s32750 alloy stainless steel plates, China super duplex uns s32750 alloy stainless steel plates suppliers, duplex stainless steel construction, duplex stainless steel valve, duplex stainless steel user, duplex stainless steel transportation, duplex stainless steel maintainer, duplex stainless steel structure