S32760 Duplex Stainless Steel Sheet
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of s32760 duplex stainless steel sheet in China. If you're going to wholesale high quality s32760 duplex stainless steel sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
S32760 Duplex Stainless Steel Sheet
Product Introduction
The chemical composition of UNS S32760 is: Chromium (Cr):
23.0-26.0%, Nickel (Ni): 19.0-22.0%, Silicon (Si): ≤1.50%, Phosphorus (P): ≤0.045%, Sulfur (S): ≤0.030%. If the phase distribution is uniform, the strength and plasticity of UNS S32760 will be uniformly improved; on the contrary, if the phase distribution is uneven, it will easily lead to uneven fracture and deformation of the material, reducing the strength and plasticity of UNS S32760.
S32760 (F55), X2CrNiMoCuWN 25.7.4, German standard 1.4501, with strong strength and corrosion resistance, mainly used in chemical processing, petrochemical industry and submarine equipment. It has strong resistance to chloride corrosion, high thermal conductivity and low thermal expansion coefficient. The higher chromium, molybdenum and nitrogen content makes it highly resistant to pitting, crevice corrosion and general corrosion. Application areas: Oil and gas industry equipment Offshore platforms, heat exchangers, underwater equipment, fire-fighting equipment Chemical processing industry, vessel and pipeline industry Desalination plants, high-pressure RO plants and subsea pipelines Mechanical components (high-strength, corrosion-resistant components).
S32760 chemical composition
C:0.030
Mn:1.00
P:0.030
S: 0.010
Si: 1.00
Ni: 6.0~8.0
Cr: 24~26
Mo: 3.0~4.0
N:0.20~0.30
Cu:0.50~1.00
W:0.50~1.00
S32760 mechanical properties:
Tensile strength: 750~895
Yield: >550
Elongation: >25
Shrinkage: >45
Hot Tags: s32760 duplex stainless steel sheet, China s32760 duplex stainless steel sheet suppliers, duplex stainless steel manufacturing, duplex stainless steel use, duplex stainless steel thickness, duplex stainless steel repair, duplex stainless steel alloy, duplex stainless steel tank