Duplex Stainless Steel Welded Pipe, S32205, ASTM A789
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of duplex stainless steel welded pipe, s32205, astm a789 in China. If you're going to wholesale high quality duplex stainless steel welded pipe, s32205, astm a789 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Duplex Stainless Steel Welded Pipe, S32205, ASTM A789
Product Description
Duplex Stainless Steel welded Pipe, S32205, ASMTA789
ISO9001:2015 and PED 2014/68/EU certified manufacturer

Product Description
| Material | Stainless Steel 304/304L/316L |
| Shape | Round Tubes |
| Production Standards | ASTM A270, ASTM A269, ASTM A249, ASTM A778, ASTM A789, DIN 11850, EN 10357, EN 10217-7 and so on. |
| Outer Diameter | 16mm - 2000mm ; |
| Thickness | 0.8mm - 20 mm ; |
| Max Length | 3000 Meters; As per customers' request ; |
| Tolerance | According to the Standard, +/-10% Commonly ; |
| Surface Treatment | Bright Annealed (BA) |
| Application | Petrochemical Industry; Chemical Fertilizer Industry; Oil Refining Industry; Oil And Gas Industry; Light Industry And Food Industry; Pulp And Paper Industry; Energy And Environmental Industries. |
| Test | Flaring test; Flattening test; Bending Test; Hydraulic Test; Eddy Current test |
| Design | OEM / ODM / Customized |
| Certificate | ISO9001; ISO14001; PED. |
Stainless Steel Tube Tolerances
| Stainless Steel Heat Exchanger Tube Tolerances | ||||
| Standard | OD(mm) | WT(mm) | Length(meters) | Grade |
| ASTM A249, ASTM A269, EN 10217-7 |
15.88 to 114.3 | 0.3 to 4.0 | Up to 18.3 meter | 1.4301, 1.4306, 1.4404, AISI 304/304L/316L, S31803/S32205, etc |
| Standard | Outside Diameter | Thickness | Length | |
| ASTM A249 (A1016) |
<25.4 | ±0.10 | ±10%S | OD<50.8+3-0 OD≥50.8+5-0 |
| ≥25.4~<38.1 | ±0.15 | |||
| ≥38.1~<50.8 | ±0.20 | |||
| ≥50.8~<63.5 | ±0.25 | |||
| ≥63.5~<76.2 | ±0.31 | |||
| ASTM A269 (A1016) |
<38.1 | ±0.13 | OD<12.7±15% OD≥12.7±10% |
OD<38.1+3.2-0 OD≥38.1+4.8-0 |
Hot Tags: duplex stainless steel welded pipe, s32205, astm a789, China duplex stainless steel welded pipe, s32205, astm a789 suppliers, duplex stainless steel customization, duplex stainless steel importer, duplex stainless steel reliability, duplex stainless steel weight, duplex stainless steel operator, duplex stainless steel estimate